X-ray CT analysis of the influence of process on defect in Ti-6Al-4V parts produced with Selective Laser Melting technology

被引:28
作者
Zhou, Xin [1 ]
Dai, Ning [1 ]
Chu, Mingqiang [2 ]
Wang, Lei [3 ]
Li, Dawei [1 ]
Zhou, Lei [1 ]
Cheng, Xiaosheng [1 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mech & Elect Engn, Nanjing 210016, Jiangsu, Peoples R China
[2] Ctr Excellence Adv Mat, Dongguan 523808, Peoples R China
[3] Shanghai Aircraft Mfg Co Ltd, Inst Aeronaut Mfg Technol, Shanghai 201324, Peoples R China
基金
中国国家自然科学基金;
关键词
Selective Laser Melting; X-ray computed tomography; Defect; Process parameter; BEHAVIOR; POROSITY; DENSITY;
D O I
10.1007/s00170-019-04347-0
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
Selective Laser Melting (SLM) technology is a potential Additive Manufacturing (AM) process. It has the ability to manufacture metal parts with complex construction. However, there are always defects in SLM products due to the raw materials, manufacturing parameters, and post-treatment. To investigate the relationship between manufacturing process parameters and defects in SLM products, laser power and scan speed are selected as variable parameters to fabricate cube samples. The 3D information of each specimen are collected by X-ray computed tomography, including the size, morphology, and spatial distribution of defects. The mathematical model of laser power and scanning speed with defect volume fraction was established. The result shows that when the scanning speed is less than 1200 mm/s, the defect volume rate increases slowly, but when the scanning speed is faster than 1200 mm/s, the volume rate of defects increases rapidly. As the laser power increases, the volume rate of defect decreased initially and then followed by an increase. It can be concluded that there are many defects in the part manufactured by low laser power and high scanning speed parameter, and the same result by high laser power and high scanning speed parameter. Additionally, the defects are larger and some of them distribute along the scanning path in the latter. Besides, the process window for SLM Ti-6Al-4V is created for exposing the relationship between process parameters and defects, and volume-spherical scatters are used to characterize different process zones.
引用
收藏
页码:3 / 14
页数:12
相关论文
共 50 条
[21]   Optimization of selective laser melting process parameters for Ti-6Al-4V alloy manufacturing using deep learning [J].
Dinh Son Nguyen ;
Park, Hong Seok ;
Lee, Chang Myung .
JOURNAL OF MANUFACTURING PROCESSES, 2020, 55 :230-235
[22]   Short-Time Heat Treatment for Ti-6Al-4V Alloy Produced by Selective Laser Melting [J].
Morita, Tatsuro ;
Oka, Yohei ;
Tsutsumi, Seiichiro ;
Takesue, Shogo ;
Higuchi, Norio ;
Sakai, Hitoshi .
MATERIALS TRANSACTIONS, 2022, 63 (06) :854-863
[23]   Effect of high layer thickness on surface quality and defect behavior of Ti-6Al-4V fabricated by selective laser melting [J].
Shi, Xuezhi ;
Yan, Cheng ;
Feng, Wuwei ;
Zhang, Yulian ;
Leng, Zhe .
OPTICS AND LASER TECHNOLOGY, 2020, 132
[24]   Dimensional deviations in Ti-6Al-4V discs produced with different process parameters during selective laser melting [J].
Snehashis Pal ;
Marijana Milković ;
Riad Ramadani ;
Janez Gotlih ;
Nenad Gubeljak ;
Radovan Hudák ;
Igor Drstvenšek ;
Matjaž Finšgar ;
Tomaž Brajlih .
The International Journal of Advanced Manufacturing Technology, 2023, 129 :5655-5669
[25]   Dimensional deviations in Ti-6Al-4V discs produced with different process parameters during selective laser melting [J].
Pal, Snehashis ;
Milkovic, Marijana ;
Ramadani, Riad ;
Gotlih, Janez ;
Gubeljak, Nenad ;
Hudak, Radovan ;
Drstvensek, Igor ;
Finsgar, Matjaz ;
Brajlih, Tomaz .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 129 (11-12) :5643-5654
[26]   Microstructure-Properties Relationships of Ti-6Al-4V Parts Fabricated by Selective Laser Melting [J].
Justin Mezzetta ;
Joon-Phil Choi ;
Jason Milligan ;
Jason Danovitch ;
Nejib Chekir ;
Alexandre Bois-Brochu ;
Yaoyao Fiona Zhao ;
Mathieu Brochu .
International Journal of Precision Engineering and Manufacturing-Green Technology, 2018, 5 :605-612
[27]   Microstructure-Properties Relationships of Ti-6Al-4V Parts Fabricated by Selective Laser Melting [J].
Mezzetta, Justin ;
Choi, Joon-Phil ;
Milligan, Jason ;
Danovitch, Jason ;
Chekir, Nejib ;
Bois-Brochu, Alexandre ;
Zhao, Yaoyao Fiona ;
Brochu, Mathieu .
INTERNATIONAL JOURNAL OF PRECISION ENGINEERING AND MANUFACTURING-GREEN TECHNOLOGY, 2018, 5 (05) :605-612
[28]   The influence of porosity on Ti-6Al-4V parts fabricated by laser powder bed fusion in the pursuit of process efficiency [J].
Kan, Wen Hao ;
Gao, Mu ;
Zhang, Xi ;
Liang, Enquan ;
Chiu, Ngai Sum Louis ;
Lim, Chao Voon Samuel ;
Huang, Aijun .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 119 (7-8) :5417-5438
[29]   Study on the influence of process parameters on high performance Ti-6Al-4V parts in laser powder bed fusion [J].
Wang, Peng ;
Chen, Dongju ;
Fan, Jinwei ;
Sun, Kun ;
Wu, Shuiyuan ;
Li, Jia ;
Sun, Yueqiang .
RAPID PROTOTYPING JOURNAL, 2022, 28 (09) :1655-1676
[30]   Gaseous surface hardening of Ti-6Al-4V fabricated by selective laser melting [J].
Valente, Emilie H. ;
Jellesen, Morten S. ;
Somers, Marcel A. J. ;
Christiansen, Thomas L. .
SURFACE & COATINGS TECHNOLOGY, 2020, 383