Leaching of borosilicate glasses. I. Experiments

被引:105
作者
Ledieu, A
Devreux, F [1 ]
Barboux, P
Sicard, L
Spalla, O
机构
[1] CNRS, Phys Mat Condensee Lab, F-91128 Palaiseau, France
[2] Ecole Polytech, F-91128 Palaiseau, France
[3] CEA, Lab Etud Comportement Long Terme, DEN, DIEC,SESC,Ctr Valrho, F-30207 Bagnols Sur Ceze, France
[4] CEA, Lab Org Nanometr & Supramol, DSM, DRECAM,SCM, F-91191 Gif Sur Yvette, France
关键词
D O I
10.1016/j.jnoncrysol.2004.06.006
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The corrosion of sodium borosilicate glasses xNa(2)O-yB(2)O(3)-(1-x-y)SiO2 is studied at constant temperature and pH as a function of the glass composition for 0.10 < x approximate to y < 0.25. Two series of experiments are reported with different glass surface area to solution volume ratios (S/V = 100 and 2000 m(-1)). The dissolution kinetics are monitored by following the concentrations of the three cations (Si, B and Na) in solution as a function of time. The altered glasses are characterized by NMR and SAXS. For all glasses, the concentrations of released cations reach a stationary limit. The time required to reach the stationary state decreases from 40 days to a few hours when the content in boron and sodium oxides is increased from 10 to 25 mol.%. The final leached fraction of silicon, LF(Si), is controlled by an apparent silica saturation concentration, which is nearly independent of the initial glass composition. On the contrary, the final leached fraction of boron and sodium, LF(B) and LF(Na), which are always close to each other, show a strong compositional dependence. The LF(B) and LF(Na) are low and nearly equal the LF(Si) for the glasses with boron (and sodium) oxide content less than 15%. This is the mark of a nearly congruent dissolution for these glasses. When the boron (and sodium) oxide content increases from 15% to 20%, there is a sharp increase of LF(B) and LF(Na) in comparison to LF(Si). Above 20%, the LF(B) and LF(Na) saturate to unity, which means that all the soluble cations have been removed, whereas the dissolved fraction of silicon may be less than 10% (depending on the S/V ratio). Si-29 NMR shows a considerable reconstruction of the altered glasses. SAXS puts in evidence the formation of a porous network with a typical pore diameter of 5 nm. The results are qualitatively explained through the competition between (i) the extraction of the soluble boron and sodium, which initiates the formation of a porous network at the nanometer scale, and (ii) the recondensation of silica, which makes the surface layer more polymerized and more resistant than the original glass at the atomic scale. (C) 2004 Published by Elsevier B.V.
引用
收藏
页码:3 / 12
页数:10
相关论文
共 21 条
[1]  
ADAMS PB, 1978, MATER SCI RES, V12, P525
[2]   THE EFFECT OF MOLECULAR-STRUCTURE ON BOROSILICATE GLASS LEACHING [J].
BUNKER, BC ;
ARNOLD, GW ;
DAY, DE ;
BRAY, PJ .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1986, 87 (1-2) :226-253
[3]  
BUNKER BC, 1988, PHYS CHEM GLASSES, V29, P106
[4]  
CHICK LA, 1984, MATER RES SOC S P, V26, P635
[5]   Growth and ripening of porous layers in water altered glasses [J].
Deruelle, O ;
Spalla, O ;
Barboux, P ;
Lambard, J .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2000, 261 (1-3) :237-251
[6]  
ILER RK, 1979, CHEM SILICA, pCH1
[7]   Alteration kinetics of a simplified nuclear glass in an aqueous medium:: effects of solution chemistry and of protective gel properties on diminishing the alteration rate [J].
Jégou, C ;
Gin, S ;
Larché, F .
JOURNAL OF NUCLEAR MATERIALS, 2000, 280 (02) :216-229
[8]   PERCOLATION PHENOMENON FOR DISSOLUTION OF SODIUM BOROSILICATE GLASSES IN AQUEOUS-SOLUTIONS [J].
KINOSHITA, M ;
HARADA, M ;
SATO, Y ;
HARIGUCHI, Y .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (04) :783-787
[9]  
LAMBARD J, 1992, J PHYS I, V2, P1191, DOI 10.1051/jp1:1992204
[10]   Structural groups and their mixing in borosilicate glasses of various compositions -: an NMR study [J].
Martens, R ;
Müller-Warmuth, W .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2000, 265 (1-2) :167-175