Surface Defects on Forged Nut of Stainless Steel

被引:0
作者
Sasa, Tomonori [1 ]
Wang, Zhigang [1 ]
Soga, Takashi [2 ]
机构
[1] Gifu Univ, Dept Mech Engn, 1-1 Yanagido, Gifu 5011193, Japan
[2] Ihara Sci Corp, Ihara Takanawa Bldg,3-11-3 Takanawa Minato Ku, Tokyo 1080074, Japan
来源
2016 7TH INTERNATIONAL CONFERENCE ON MECHATRONICS AND MANUFACTURING (ICMM 2016) | 2016年 / 45卷
关键词
DEFORMATION;
D O I
10.1051/matecconf/20164504002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Surface quality of nuts used in gas pipe joints is an important issue because the surface state affects the fatigue characteristics. Surface defects of nuts produced by warm forging from a stainless steel are observed and the cause of defect generation is discussed based on the numerical results of FEM simulation. It is revealed that there exists the lap defect on the drawn wire surface with an opened end and the surface defects on the forged nut are generated by the tensile stress during forging since there exists a moment at almost the whole area of the billet surface that a tensile stress over 200MPa is generated during nut forging.
引用
收藏
页数:4
相关论文
共 10 条
[1]  
HIRAI K, 1984, J JSTP, V25, P878
[2]   Deformation analysis of surface defect on plate rolling [J].
Ishikawa, T ;
Yukawa, N ;
Yoshida, Y ;
Tonohata, Y .
TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2003, 89 (11) :1142-1149
[3]  
Kumagai M., 2006, SURF TECHNOL, V57, P428
[4]  
MURAKAMI Y, 1988, J JPN SOC MECH ENG A, V54, P688
[5]  
Satoh H., 1995, WIRE J INT, V3, P120
[6]   Growth and disappearance of transversal cracks on stainless steel wire in wire drawing [J].
Shinohara, T ;
Yoshida, K .
TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2004, 90 (12) :1010-1015
[7]  
Sumami E., 1982, TETSU TO HAGANE, V68, P415
[8]   RECENT TREND OF WARM FORGING TECHNOLOGY [J].
YUASA, K ;
SUZUKI, Y .
TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (10) :1488-1497
[9]  
Yukawa N, 2005, TETSU TO HAGANE, V91, P861
[10]  
Yukawa N, 2006, TETSU TO HAGANE, V92, P19