Compressive Strength and Microstructure of Alkali-Activated Blast Furnace Slag/Sewage Sludge Ash (GGBS/SSA) Blends Cured at Room Temperature

被引:30
作者
Tashima, M. M. [1 ]
Reig, L. [2 ]
Santini, M. A., Jr. [1 ]
Moraes, J. C. B. [1 ]
Akasaki, J. L. [1 ]
Paya, J. [3 ]
Borrachero, M. V. [3 ]
Soriano, L. [3 ]
机构
[1] Univ Estadual Paulista, UNESP, MAC UNESP Grp Pesquisa Mat Alternat Construcao, Campus Ilha Solteira, Sao Paulo, Brazil
[2] Univ Jaume 1, EMC, Castellon de La Plana, Spain
[3] Univ Politecn Valencia, GIQUIMA Grp, ICITECH Inst Ciencia & Tecnol Hormigon, Valencia, Spain
基金
巴西圣保罗研究基金会;
关键词
Sewage sludge ash; Waste management; Alkali-activated cement; Compressive strength; INCINERATED SEWAGE-SLUDGE; FLY-ASH; LIGHTWEIGHT AGGREGATE; SLAG MORTARS; WASTE GLASS; CEMENT; CONCRETE; BEHAVIOR; SSA; WORKABILITY;
D O I
10.1007/s12649-016-9659-1
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
In the present work, ground granulated blast furnace slag (GGBS) and sewage sludge ash (SSA) blends were assessed for the production of alkali-activated pastes and mortars. Percentages of SSA to substitute GGBS ranged from 0 to 30 wt% and sodium concentrations of 6-10 mol kg(-1) were used for the activating solutions. Pastes and mortars were cured at 20 degrees C for up to 90 days. Raw materials were characterised by granulometric analysis, XRF, XRD, FTIR and SEM techniques. The replacement percentage of GGBS by SSA and the sodium hydroxide concentration of the alkaline activator were optimised to produce mortar with compressive strengths close to 30 MPa after 28 curing days at room temperature. Best results were obtained in samples blended with 20 wt% SSA activated with 6 mol kg(-1) NaOH solutions which, according to the XRD, FTIR and microscopic results, contained higher amounts of (N,C)-A-S-H gel. The potential use of SSA for the development of alternative cementitious materials at room temperature has been demonstrated.
引用
收藏
页码:1441 / 1451
页数:11
相关论文
共 50 条
[31]   Controllable setting time of alkali-activated materials incorporating sewage sludge ash and GGBS: The role of retarders [J].
Ma, Xiaobing ;
Shi, Daquan ;
Xia, Yan ;
Zhao, Yading ;
Liu, Minghao ;
Yang, Yingzi .
CONSTRUCTION AND BUILDING MATERIALS, 2024, 412
[32]   Influence of superplasticizers and retarders on the workability and strength of one-part alkali-activated fly ash/slag binders cured at room temperature [J].
Oderji, Sajjad Yousefi ;
Chen, Bing ;
Shakya, Chandan ;
Ahmad, Muhammad Riaz ;
Shah, Syed Farasat Ali .
CONSTRUCTION AND BUILDING MATERIALS, 2019, 229
[33]   Optimum Use of Sugar Cane Straw Ash in Alkali-Activated Binders Based on Blast Furnace Slag [J].
Bassan de Moraes, Joao Claudio ;
Tashima, Mauro Mitsuuchi ;
Pinheiro Melges, Jose Luiz ;
Akasaki, Jorge Luis ;
Monzo, Jose ;
Victoria Borrachero, Maria ;
Soriano, Lourdes ;
Paya, Jordi .
JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2018, 30 (06)
[34]   Reaction kinetics, gel character and strength of ambient temperature cured alkali activated slag-fly ash blends [J].
Gao, X. ;
Yu, Q. L. ;
Brouwers, H. J. H. .
CONSTRUCTION AND BUILDING MATERIALS, 2015, 80 :105-115
[35]   Thermal and chemical resistance of fly ash and blast furnace slag alkali-activated pastes after exposure to high temperature and NaOH [J].
Cao, Changshun ;
Lv, Xiaochen ;
Li, Hao ;
Wu, Shaowei ;
Lv, Jianfu .
CONSTRUCTION AND BUILDING MATERIALS, 2025, 490
[36]   Physical-mechanical and microstructural properties of alkali-activated fly ash-blast furnace slag blends [J].
Marjanovic, N. ;
Komljenovic, M. ;
Bascarevic, Z. ;
Nikolic, V. ;
Petrovic, R. .
CERAMICS INTERNATIONAL, 2015, 41 (01) :1421-1435
[37]   Mechanisms of autogenous shrinkage of alkali-activated fly ash-slag pastes cured at ambient temperature within 24 h [J].
Fang, Guohao ;
Bahrami, Hossein ;
Zhang, Mingzhong .
CONSTRUCTION AND BUILDING MATERIALS, 2018, 171 :377-387
[38]   Microstructure of Alkali-activated Granulated Blast Furnace Slag-based Geopolymer [J].
Zhang, Yao Jun ;
Li, Hai Hong ;
Zhao, Yong Lin ;
Wang, Ya Chao ;
Xu, De Long .
ADVANCED BUILDING MATERIALS, PTS 1-4, 2011, 250-253 (1-4) :528-+
[39]   Effect of Alkaline Solution and Supplementary Materials on Compressive Strength of Sewage Sludge Ash-Based Alkali-Activated Mortar [J].
Moussa, Amr ;
Fujiyama, Chikako .
4TH FIB INTERNATIONAL CONFERENCE ON CONCRETE SUSTAINABILITY, ICCS2024, VOL 1, 2025, 573 :296-304
[40]   Shrinkage of Alkali-Activated Combined Slag and Fly Ash Concrete Cured at Ambient Temperature [J].
Rodrigue, Alexandre ;
Bissonnette, Benoit ;
Duchesne, Josee ;
Fournier, Benoit .
ACI MATERIALS JOURNAL, 2022, 119 (03) :15-23