Evolution of phases in P91 steel in various heat treatment conditions and their effect on microstructure stability and mechanical properties

被引:1
作者
Pandey, Chandan [1 ]
Giri, Anoj [1 ]
Mahapatra, M. M. [1 ]
机构
[1] Indian Inst Technol Roorkee, Dept Mech & Ind Engn, Roorkee 247667, Uttar Pradesh, India
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2016年 / 664卷
关键词
P91; steel; Tempering; M23C6; Microstructure; Mechanical properties; PAGBs; MODIFIED 9CR-1MO STEEL; FERRITIC STEELS; MINOR PHASES; CREEP; TEMPERATURE; ZONES; PLANT;
D O I
10.1016/j.msea.2016.03.132
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To achieve high thermal efficiency, modern day thermal power plants operate at higher operating temperature and pressure which necessitates use of steels with high creep rupture strength such as modified 9Cr-1Mo steels. In the present study, the evolution of phases in modified 9Cr-1Mo P91 steel and their effects on microstructural stability and mechanical properties have been studied for specimens that were subjected to different thermal heat treatment conditions. The main focus has been to study the effect of heat treatment temperature ranging from 623 K to 1033 K (350-760 degrees C) on P91 steel. Further, the effect of furnace cooling, water quenching, tempering at 1273 K (1000 degrees C) and austenitizing on the mechanical properties and microstructure has been studied. The techniques used for material characterization were scanning electron microscopy (SEM), optical microscopy (OM) and X-ray diffraction. For low tempering temperature, i.e. 623 K (350 degrees C), M23C6, M3C, M7C3, and MX precipitates have been observed with high yield strength (YS), tensile strength (UTS), hardness and low toughness. In the high temperature range, 923-1033 K (650-760 degrees C), fine MX, M7C3, M23C6, M2X, and M3C precipitates have been observed with low YS, UTS, hardness and high toughness. The steel tempered at 1033 K (760 degrees C) was observed to be having best combination of YS, UTS, hardness, toughness and ductility. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:58 / 74
页数:17
相关论文
共 27 条
  • [1] Alloy design of creep resistant 9Cr steel using a dispersion of nano-sized carbonitrides
    Abe, F.
    Taneike, M.
    Sawada, K.
    [J]. INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2007, 84 (1-2) : 3 - 12
  • [2] American Society of Testing Materials, ASTM A370: Standard test methods and definitions for mechanical testing of steel products
  • [3] Influence of Low Nickel (0.09 wt%) Content on Microstructure and Toughness of P91 Steel Welds
    Arivazhagan, B.
    Vasudevan, M.
    Kamaraj, M.
    [J]. METALS AND MATERIALS INTERNATIONAL, 2015, 21 (03) : 538 - 542
  • [4] A study on influence of shielding gas composition on toughness of flux-cored arc weld of modified 9Cr-1Mo (P91) steel
    Arivazhagan, B.
    Sundaresan, S.
    Kamaraj, M.
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (12-13) : 5245 - 5253
  • [5] Baltusnikas A, 2007, MATER SCI-MEDZG, V13, P286
  • [6] Effect of normalizing and tempering temperatures on microstructure and mechanical properties of P92 steel
    Barbadikar, Dipika R.
    Deshmukh, G. S.
    Maddi, L.
    Laha, K.
    Parameswaran, R.
    Ballal, A. R.
    Peshwe, D. R.
    Paretkar, R. K.
    Nandagopal, M.
    Mathew, M. D.
    [J]. INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2015, 132 : 97 - 105
  • [7] Fracture characteristics of thermally exposed 9Cr-1Mo steel after tensile and impact testing at room temperature
    Blach, Juraj
    Falat, Ladislav
    Sevc, Peter
    [J]. ENGINEERING FAILURE ANALYSIS, 2009, 16 (05) : 1397 - 1403
  • [8] Czyrska-Filemonowicz A., 2006, J ACHIEVEMENTS MAT M, V19, P43
  • [9] Modelling simultaneous alloy carbide sequence in power plant steels
    Fujita, N
    Bhadeshia, HKDH
    [J]. ISIJ INTERNATIONAL, 2002, 42 (07) : 760 - 769
  • [10] Microstructure and long-term creep properties of 9-12% Cr steels
    Hald, J.
    [J]. INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2008, 85 (1-2) : 30 - 37