Stress Corrosion Behaviors of 316LN Stainless Steel in a Simulated PWR Primary Water Environment

被引:12
作者
Huang, Yong [1 ]
Wu, Weisong [1 ]
Cong, Shuo [1 ]
Ran, Guang [1 ]
Cen, Danxia [2 ]
Li, Ning [1 ]
机构
[1] Xiamen Univ, Coll Energy, Xiamen 361102, Peoples R China
[2] Xiamen Univ, Coll Chem & Chem Engn, Xiamen 361102, Peoples R China
基金
对外科技合作项目(国际科技项目); 中国国家自然科学基金;
关键词
316LN stainless steel; stress corrosion crack; tensile properties; nuclear materials; HIGH-TEMPERATURE WATER; OXIDE-FILMS; 288-DEGREES-C WATER; ZN INJECTION; GROWTH-RATE; CRACKING; ZINC; 304-STAINLESS-STEEL; ALLOY; HYDROGEN;
D O I
10.3390/ma11091509
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effect of the strain rate, experimental temperature, Zn content in the test solution, and prefilming time on the mechanical properties was investigated by a tensile test with a slow strain rate, at a chemical solution of 2.2 ppm Li and 1200 ppm B in a static autoclave with 8.2 MPa. The experimental parameters clearly affected the tensile properties. The surface morphology, fractograph, and cross-sectional microstructure were analyzed by scanning electron microscopy and transmission electron microscopy. The (elongation) and UTS (ultimate tensile strength) of the samples tested in chemical solution were obviously lower than those of the samples tested under a nitrogen atmosphere. However, in general, all samples showed a ductile fracture characteristic and an excellent tensile property in all experimental conditions. The and UTS were first increased with increasing Zn content, and then decreased at both conditions of 9.26 x 10(-7)/s and 4.63 x 10(-7)/s strain rates. The difference values of tensile properties at different strain rates showed fluctuations with increasing Zn content. The increased with both increasing experimental temperature and prefilming time. The UTS first decreased with increasing prefilming time and then increased. The I-scc (stress corrosion cracking susceptibility) decreased with an increasing strain rate, experiment temperature, and prefilming time. Many particles with polyhedrons were formed on the sample surfaces, which was attributed to corrosion in a periodical location at the sample surface. The average length of the particles decreased with increasing Zn content, but increased with both increasing experimental temperatures and prefilming time. The corresponding mechanism is also discussed in this work.
引用
收藏
页数:13
相关论文
共 41 条
[1]  
Andresen P.L., 2006, INT C WAT CHEM NUCL
[2]  
Angell MG, 1999, PROCEEDINGS OF THE NINTH INTERNATIONAL SYMPOSIUM ON ENVIRONMENTAL DEGRADATION OF MATERIALS IN NUCLEAR POWER SYSTEMS-WATER REACTORS, P97
[3]   The role of dynamic strain-ageing in the environment assisted cracking observed in pressure vessel steels [J].
Atkinson, JD ;
Yu, J .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1997, 20 (01) :1-12
[4]  
Betova I., 2011, VTTR0551111 TECHN RE
[5]   Influence of Zn on the oxide layer on AISI 316L(NG) stainless steel in simulated pressurised water reactor coolant [J].
Betova, Iva ;
Bojinov, Martin ;
Kinnunen, Petri ;
Lundgren, Klas ;
Saario, Tirno .
ELECTROCHIMICA ACTA, 2009, 54 (03) :1056-1069
[6]  
Brnic J, 2009, J MATER SCI TECHNOL, V25, P175
[7]   Modelling of stress-corrosion cracking by using peridynamics [J].
De Meo, Dennj ;
Diyaroglu, Cagan ;
Zhu, Ning ;
Oterkus, Erkan ;
Siddiq, M. Amir .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (15) :6593-6609
[8]  
Ehrnstén U, 2012, COMPREHENSIVE NUCLEAR MATERIALS, VOL 5: MATERIAL PERFORMANCE AND CORROSION/WASTE MATERIALS, P93
[9]   Stress corrosion cracking on irradiated 316 stainless steel [J].
Furutani, G ;
Nakajima, N ;
Konishi, T ;
Kodama, M .
JOURNAL OF NUCLEAR MATERIALS, 2001, 288 (2-3) :179-186
[10]   Solubility of zinc ferrite in high-temperature oxygenated water [J].
Hanzawa, Y ;
Hiroishi, D ;
Matsuura, C ;
Ishigure, K .
JOURNAL OF NUCLEAR MATERIALS, 1998, 252 (03) :209-215