Surface modifications and adhesion of SBS rubber containing calcium carbonate filler by treatment with UV radiation

被引:23
作者
Romero-Sanchez, Maria D.
Walzak, M. J.
Torregrosa-Macia, Rosa
Martin-Martinez, Jose Miguel [1 ]
机构
[1] Univ Alicante, Adhes & Adhes Lab, E-03080 Alicante, Spain
[2] Univ Western Ontario, London, ON N6A 5B7, Canada
关键词
rubbers; surface treatment; X-ray photoelectron spectroscopy; peel;
D O I
10.1016/j.ijadhadh.2006.08.002
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Two styrene-butadiene-styrene block rubbers, one with 10wt% calcium carbonate filler (S6C), and one without (S6) were surface treated with UV radiation. The resulting surface modifications and adhesion properties with polyurethane adhesive were studied. The surface modifications produced on these rubber surfaces were analyzed by contact angle measurements, ATR-IR spectroscopy, X-ray photoelectron spectroscopy, scanning electron microscopy and atomic force microscopy. The adhesion properties were evaluated using T-peel tests of treated SBS rubber/polyurethane adhesive/leather joints. Treatment with UV radiation produced improved wettability as well as chemical (surface oxidation) and morphological modifications (roughness, ablation) of the rubber surface. These modifications were more pronounced with increasing treatment time. Although the improvement in wettability was similar in the UV-treated SBS, without and with calcium carbonate filler, the presence of calcium carbonate inhibited the modifications produced at short treatment times, while surface oxidation of filled SBS rubbers was favored at longer treatment times. (C) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:434 / 445
页数:12
相关论文
共 30 条
[1]  
[Anonymous], TREATISE ADHES ADHES
[2]  
BHURKE AS, 2000, P 23 ANN M ADH SOC M, P285
[3]  
BUCHMAN A, 1997, 20 ANN ANN M ADH SOC, P509
[4]  
CARLSSON DJ, 1990, ENCY POLYMER SCI ENG, V4, P630
[5]   New pretreatment for elastomers to enhance adhesion [J].
Dahm, RH ;
Brewis, DM ;
Fletcher, IW ;
Mathieson, I .
JOURNAL OF ADHESION, 2005, 81 (01) :59-75
[6]  
Dodiuk H, 1998, FIRST INTERNATIONAL CONGRESS ON ADHESION SCIENCE AND TECHNOLOGY - INVITED PAPERS, P387
[7]  
FLETT CMS, 1963, CHARACTERISTIC FREQU, P29
[8]   INITIATION PROCESSES IN PHOTODEGRADATION OF HIGH IMPACT POLYSTYRENE .2. EFFECTS OF PRIOR EXPOSURE TO SENSITIZING ENVIRONMENTS [J].
GHAFFAR, A ;
SCOTT, A ;
SCOTT, G .
EUROPEAN POLYMER JOURNAL, 1977, 13 (02) :83-88
[9]  
Guven O., 1990, CROSSLINKING SCISSIO
[10]  
*IND RUBB I, 1998, RUBB ENG