Rotating-beam fatigue properties and effect of Ni element additive in bulk glassy Zr50CU40Al10 alloys

被引:0
|
作者
Yokoyama, Y [1 ]
Fukaura, K [1 ]
Inoue, A [1 ]
机构
[1] Himeji Inst Technol, Fac Engn, Himeji, Hyogo 6712201, Japan
来源
MATERIALS LIFETIME SCIENCE & ENGINEERING | 2003年
关键词
Zr50Cu40Al10 and Zr50Cu30Ni10Al10 bulk glassy alloy; rotating-beam fatigue testing; Wohler curve; fatigue limit; striation-like mark;
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
We examined Wohler curves of Zr50Cu40Al10 and Zr50Cu30Ni10Al10 bulk glassy alloys using a. rotating-beam fatigue test to evaluate the effect of adding a Ni element on fatigue strength. As a result, we found that the fatigue limit was increased from 250 Mpa to 500 MPa by adding 10 at% Ni instead of Cu to a Zr50Cu40Al10 bulk glassy alloy. A Zr50Cu40Al10 bulk glassy alloy exhibits a wide fatigue-fractured region With striation-like marks up to 80% in response to low applied stress (near the fatigue limit). However, adding Ni limits the fatigue-fractured region to half of the whole fractured surface. We also observed fatigue-fmcture surfaces OfZr(50)Cu(40)Al(10) and Zr50Cu30Ni10Al10 bulk glassy alloys to estimate the fatigue-fracture toughness. The fatigue fracture toughness decreases suddenly around N = 10(3) to 10(4), similar to Wohler curves.
引用
收藏
页码:77 / 90
页数:14
相关论文
共 50 条
  • [1] Effect of Ni addition on fatigue properties of bulk glassy Zr50Cu40Al10 alloys
    Yokoyama, Y
    Fukaura, K
    Inoue, A
    MATERIALS TRANSACTIONS, 2004, 45 (05) : 1672 - 1678
  • [2] Nanostructural control by additive Pd in cast Zr50CU40Al10 glassy alloys with good fatigue properties
    Yokoyama, Y
    Nishijima, M
    Hiraga, K
    Liaw, PK
    Inoue, A
    Metastable, Mechanically Alloyed and Nanocrystalline Materials, 2005, 24-25 : 677 - 680
  • [3] Volume change in Zr50Cu40Al10 glassy alloys
    Yokoyama, Y.
    Yamasaki, T.
    Liaw, P. K.
    Buchanan, R. A.
    Inoue, A.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 434 : 160 - 163
  • [4] Volume change in Zr50Cu40Al10 glassy alloys
    Yokoyama, Y.
    Yamasaki, T.
    Liaw, P.K.
    Buchanan, R.A.
    Inoue, A.
    Journal of Alloys and Compounds, 2007, 434-435 (SPEC. ISS.): : 160 - 163
  • [5] Fatigue-strength enhancement of cast Zr50Cu40Al10 glassy alloys
    Yokoyama, Yoshihiko
    Liaw, Peter K.
    Nishijima, Masahiko
    Hiraga, Kenji
    Buchanan, Raymond A.
    Inoue, Akihisa
    MATERIALS TRANSACTIONS, 2006, 47 (05) : 1286 - 1293
  • [6] Rotating-beam fatigue properties of Pd40Cu30Ni10P20 bulk glassy alloy
    Yokoyama, Y
    Nishiyama, N
    Fukaura, K
    Sunada, H
    Murakami, Y
    Inoue, A
    MATERIALS TRANSACTIONS, 2001, 42 (05) : 876 - 880
  • [7] Irradiation effect of swift heavy ion for Zr50Cu40Al10 bulk glassy alloy
    Onodera, Naoto
    Ishii, Akito
    Ishii, Kouji
    Iwase, Akihiro
    Yokoyama, Yoshihiko
    Saitoh, Yuichi
    Ishikawa, Norito
    Yabuuchi, Atsushi
    Hori, Fuminobu
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2013, 314 : 122 - 124
  • [8] Evolution of mechanical properties of cast Zr50Cu40Al10 glassy alloys by structural relaxation
    Yokoyama, Y
    Akeno, Y
    Yamasaki, T
    Liaw, PK
    Buchanan, RA
    Inoue, A
    MATERIALS TRANSACTIONS, 2005, 46 (12) : 2755 - 2761
  • [9] Surface properties of Zr50Cu40Al10 bulk metallic glass
    Nakayama, Koji S.
    Yokoyama, Y.
    Sakurai, T.
    Inoue, A.
    APPLIED PHYSICS LETTERS, 2007, 90 (18)
  • [10] Glassy Solidification Criterion of Zr50Cu40Al10 Alloy
    Yokoyama, Yoshihiko
    Fredriksson, Hasse
    Yasuda, Hideyuki
    Nishijima, Masahiko
    Inoue, Akihisa
    13TH INTERNATIONAL CONFERENCE ON RAPIDLY QUENCHED AND METASTABLE MATERIALS, 2009, 144