Structure property relation of hybrid biocomposites based on jute, viscose and polypropylene: The effect of the fibre content and the length on the fracture toughness and the fatigue properties

被引:43
作者
Ranganathan, Nalini [1 ,3 ]
Oksman, Kristiina [1 ,2 ]
Nayak, Sanjay K. [3 ]
Sain, Mohini [1 ,2 ]
机构
[1] Univ Toronto, Fac Forestry, 33 Willcocks St, Toronto, ON M5S 3B3, Canada
[2] Lulea Univ Technol, Div Mat Sci, SE-97187 Lulea, Sweden
[3] CIPET, Madras 600032, Tamil Nadu, India
关键词
Fibres; Fatigue; Fracture toughness; Electron microscopy; MECHANICAL-PROPERTIES; REINFORCED POLYPROPYLENE; TENSILE PROPERTIES; MICROSTRUCTURE; ORIENTATION; MORPHOLOGY; DISPERSION; BEHAVIOR; IMPACT;
D O I
10.1016/j.compositesa.2015.10.037
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present study, the extent of jute and viscose fibre breakage during the extrusion process on the fracture toughness and the fatigue properties was investigated. The composite materials were manufactured using direct long fibre thermoplastic (D-LFT) extrusion, followed by compression moulding. The fracture toughness (K-IC) and the fracture energy (G(IC)) of the PP-J30 composites were significantly improved (133% and 514%, respectively) with the addition of 10 wt% viscose fibres, indicating hindered crack propagation. The addition of viscose fibres resulted in three times higher fatigue life compared with that of the unmodified jute composites. Further, with the addition of (2 wt%) MAPP, the PP-J30-V10 resulted in a higher average viscose fibre length of 8.1 mm, and the fracture toughness and fracture energy increased from 9.1 to 10.0 MPa m(1/2) and 28.9 to 31.2 kJ/m(2), respectively. Similarly, the fatigue life increased 51% compared with the PP-J30-V10, thus demonstrating the increased work energy due to hindrance of the propagation of cracks. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:169 / 175
页数:7
相关论文
共 37 条
[1]  
Adusumalli R-B, 2010, J COMPOS MATER, V46, P359
[2]   Impact damage on fibre-reinforced polymer matrix composite - A review [J].
Agrawal, Sandeep ;
Singh, Kalyan Kumar ;
Sarkar, P. K. .
JOURNAL OF COMPOSITE MATERIALS, 2014, 48 (03) :317-332
[3]   Fracture Toughness of Polypropylene-Based Particulate Composites [J].
Arencon, David ;
Ignacio Velasco, Jose .
MATERIALS, 2009, 2 (04) :2046-2094
[4]   A study on interfacial properties of jute-PP composites [J].
Bera, Moumita ;
Alagirusamy, R. ;
Das, Apurba .
JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2010, 29 (20) :3155-3161
[5]   SHORT JUTE FIBER REINFORCED CARBOXYLATED NITRILE RUBBER [J].
CHAKRABORTY, SK ;
SETUA, DK ;
DE, SK .
RUBBER CHEMISTRY AND TECHNOLOGY, 1982, 55 (05) :1286-1307
[6]   Dynamic fracture toughness of cellulose-fiber-reinforced polypropylene: Preliminary investigation of microstructural effects [J].
Clemons, CM ;
Caulfield, DF ;
Giacomin, AJ .
JOURNAL OF ELASTOMERS AND PLASTICS, 1999, 31 (04) :367-378
[7]  
Dieter GE., 1988, MECH METALLURGY, P348
[8]   The effect of short carbon fibre reinforcement on fatigue crack growth in PEEK [J].
Evans, WJ ;
Issac, DH ;
Saib, KS .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1996, 27 (07) :547-554
[9]   Tensile properties of short-glass-fiber- and short-carbon-fiber-reinforced polypropylene composites [J].
Fu, SY ;
Lauke, B ;
Mäder, E ;
Yue, CY ;
Hu, X .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2000, 31 (10) :1117-1125
[10]   Twin-screw extrusion impact on natural fibre morphology and material properties in poly(lactic acid) based biocomposites [J].
Gamon, G. ;
Evon, Ph ;
Rigal, L. .
INDUSTRIAL CROPS AND PRODUCTS, 2013, 46 :173-185