摘要
To understand the effect of environment on the fracture toughness of cubic titanium trialuminide (based on Al3Ti) intermetallics a wide program of fracture toughness testing using the single-edge-precracked-beam (SEPB) and chevron-notched-beam (CNB) in three-and four-point bending was carried out in air, vacuum (similar to 1.3x10(-5) Pa), oxygen, argon, water and liqiud nitrogen. The cubic titanium trialuminide (average composition 66at.% Al, 25at.% Ti and 9at.% Mn) modified with Mn, cast and HIP-ed at 1200 degrees C for 2h under 170 MPa was used for testing. Testing in air, vacuum and argon was carried out up to 1000 degrees C. It is shown that fracture toughness of cubic titanium trialuminides at ambient temperatures is not affected by the environments containing moisture (water vapour). It seems that at ambient temperatures these materials are completely immune to the water-vapour hydrogen embrittlement and their cause of brittleness is other than environment. At the intermediate temperature range of approx. 200-600 degrees C trialuminides tested in air and vacuum exhibit a mild but discernible peak of fracture toughness. However, testing in high-purity argon eliminates this peak and fracture toughness in argon is practically independent of temperature at the range from room temperature to 1000 degrees C.
引用
收藏
页码:787 / 793
页数:7
相关论文
共 50 条
  • [1] Fracture, ductility and fracture toughness behavior of the cubic (L12) titanium trialuminide intermetallics
    Varin, RA
    Zbroniec, L
    Witczak, Z
    DEFORMATION AND FRACTURE OF ORDERED INTERMETALLIC MATERIALS III, 1996, : 583 - 601
  • [2] Dynamic recrystallization, ductility and resulting fracture toughness of the cubic titanium trialuminide intermetallics
    Varin, RA
    Zbroniec, L
    THERMEC '97 - INTERNATIONAL CONFERENCE ON THERMOMECHANICAL PROCESSING OF STEELS AND OTHER MATERIALS, VOLS I-II, 1997, : 1535 - 1542
  • [3] Formation of nanocrystalline cubic (L12) titanium trialuminide by controlled ball milling
    Varin, RA
    Wexler, D
    Calka, A
    Zbroniec, L
    INTERMETALLICS, 1998, 6 (06) : 547 - 557
  • [4] Advances in cubic titanium trialuminide intermetallics
    Varin, RA
    Czujko, T
    Zbroniec, L
    PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 947 - 950
  • [5] Formation of nanocrystalline cubic (L12) titanium trialuminide by controlled ball milling
    Univ of Waterloo, Waterloo, Canada
    Intermet, 6 (547-557):
  • [6] Deformation and Dislocation Structure in L12 Titanium Trialuminide Alloys
    Gengxiang HU
    Shipu CHEN
    Xiaohua WU
    Yonghua RONG and Xiaofu CHEN(Dept. of Materials Science
    JournalofMaterialsScience&Technology, 1994, (06) : 435 - 440
  • [7] ORDERING, TERNARY ATOM LOCATION AND AGING IN L12 TRIALUMINIDE ALLOYS
    MORRIS, DG
    GUNTER, S
    ACTA METALLURGICA ET MATERIALIA, 1992, 40 (11): : 3065 - 3073
  • [8] Mechanically milled nanocrystalline cubic titanium trialuminide and iron aluminide intermetallics
    Varin, R.A.
    Bystrzycki, J.
    Calka, A.
    Wexler, D.
    Materials Science Forum, 1999, 312 : 103 - 108
  • [9] Observations of crack tip process zones in cubic titanium trialuminide intermetallics
    Varin, RA
    Zbroniec, L
    Chiu, C
    INTERMETALLICS, 2001, 9 (10-11) : 937 - 941