Impact of graphene oxide and silver diamine fluoride in comparison to photodynamic therapy on bond integrity and microleakage scores of resin modified glass ionomer cement to demineralized dentin

被引:7
作者
Al-Qahtani, Yasser M. [1 ]
机构
[1] Minist Hlth, Consultant Restorat Dent Dept, Abha, Saudi Arabia
关键词
Graphene oxide; Silver diamine fluoride; Photodynamic therapy; Resin modified glass ionomer cement; RANDOMIZED CLINICAL-TRIAL; CARIES;
D O I
10.1016/j.pdpdt.2020.102163
中图分类号
R73 [肿瘤学];
学科分类号
100214 ;
摘要
Aim: To evaluate the impact of graphene oxide (GO) and silver diammine fluoride (SDF) in comparison to photodynamic therapy (PDT) on adhesive bond integrity and microleakage scores of resin-modified glass ionomer cement (RMGIC) to demineralized dentin. Methods: 80 non-carious and atraumatic third molars were mounted inside the segments of polyvinyl pipes. Exposure, homogenization, and polishing of dentinal tubules was performed. 20 specimens were left unconditioned and classified a group 4. Exposure of acetic acid was done to 60 specimens and randomly allocated into 3 groups. Group 1 specimens were treated with 0.25 % GO; group 2 specimens were treated with 3.8 % SDF; and group 3 specimens were exposed to PDT. The bonding of all samples to RMGIC was performed by light curing and universal testing machine was utilized for testing shear bond strength (SBS). For failure modes, an optical microscope at 40x magnification was used to observe the debonded interfaces. For microleakage, all the specimens were submerged in 2% methylene blue for 1 day and observed under a digital microscope. The post hoc Tukey and analysis of variance (ANOVA) were used to examine SBS. A p-value of ?0.05 was considered statistically significant. Results: Group 2 showed the highest bond strength (3.8 % SDF + RMGIC + DD ? 15.27 ? 2.19 MPa). Groups 1 (0.25 % GO + RMGIC + DD ? 14.11 ? 3.82) and 2 showed comparable results of SBS, which was significantly higher when compared with other research groups (p < 0.05). According to the post hoc Tukey test, the SBS scores of treatment groups exhibited statistically significant values as compared to the control group (p < 0.05). Group 2 samples showed the least microleakage mean score (0.8 ? 0.42), followed by group 1 specimens (1.02 ? 0.88). The comparable microleakage mean scores were demonstrated by the samples in group 1 and 2 (p < 0.01). According to one-way ANOVA, a significant difference was observed in microleakage scores among experimental groups (p < 0.01). Conclusion: Improved bond strength and marginal microleakage scores were demonstrated by the demineralized dentin treated with 0.25 % graphene oxide and 3.8 % silver diamine fluoride when bonded to resin-modified glass ionomer cement. The application of methylene blue photosensitizer for photodynamic therapy undermined the adhesive bond strength applied on demineralized dentin.
引用
收藏
页数:5
相关论文
共 48 条
  • [1] Influence of Curing Mode and Time on Degree of Conversion of One Conventional and Two Self-adhesive Resin Cements
    Aguiar, T. R.
    Francescantonio, M. D.
    Arrais, C. A. G.
    Ambrosano, G. M. B.
    Davanzo, C.
    Giannini, M.
    [J]. OPERATIVE DENTISTRY, 2010, 35 (03) : 295 - 299
  • [2] Clinical efficacy of photodynamic therapy and laser irradiation as an adjunct to open flap debridement in the treatment of chronic periodontitis: A systematic review and meta-analysis
    Akram, Zohaib
    Shafqat, Syed Saad
    Niaz, Muhammad Omar
    Raza, Anam
    Naseem, Mustafa
    [J]. PHOTODERMATOLOGY PHOTOIMMUNOLOGY & PHOTOMEDICINE, 2020, 36 (01) : 3 - 13
  • [3] Efficacy of chlorhexidine, Er Cr YSGG laser and photodynamic therapy on the adhesive bond integrity of caries affected dentin. An in-vitro study
    Al Deeb, Laila
    Bin-Shuwaish, Mohammed S.
    Abrar, Eisha
    Naseem, Mustafa
    Al-Hamdan, Rana S.
    Maawadh, Ahmed M.
    Al Deeb, Modhi
    Almohareb, Thamer
    Al Ahdal, Khold
    Vohra, Fahim
    Abduljabbar, Tariq
    [J]. PHOTODIAGNOSIS AND PHOTODYNAMIC THERAPY, 2020, 31
  • [4] Dentin bond strength of bioactive cement in comparison to conventional resin cement when photosensitized with Er,Cr:YSGG Laser
    Alkhudhairy, Fahad
    Al-Johany, Sulieman S.
    Naseem, Mustafa
    Bin-Shuwaish, Mohammed
    Vohra, Fahim
    [J]. PAKISTAN JOURNAL OF MEDICAL SCIENCES, 2020, 36 (02) : 85 - 90
  • [5] Influence of photobio-modulation with an Er,Cr: YSGG laser on dentin adhesion bonded with bioactive and resin-modified glass ionomer cement
    Alkhudhairy, Fahad
    Naseem, Mustafa
    Ahmad, Zeeshan H.
    Alnooh, Abrar N.
    Vohra, Fahim
    [J]. JOURNAL OF APPLIED BIOMATERIALS & FUNCTIONAL MATERIALS, 2019, 17 (04)
  • [6] Effect of Photodynamic Therapy, Er,Cr:YSGG, and Nd:YAG Laser on the Push-Out Bond Strength of Fiber Post to Root Dentin
    Alonaizan, Faisal Abdullah
    Alofi, Raneem S.
    AlFawaz, Yasser F.
    Alsahhaf, Abdulaziz
    Al-Aali, Khulud Abdulrahman
    Vohra, Fahim
    Abduljabbar, Tariq
    [J]. PHOTOBIOMODULATION PHOTOMEDICINE AND LASER SURGERY, 2020, 38 (01) : 24 - 29
  • [7] Treatment of caries affected dentin with different photosensitizers and its effect on adhesive bond integrity to resin composite
    Alrahlah, Ali
    Niaz, Muhammad Omar
    Abrar, Eisha
    Vohra, Fahim
    Rashid, Haroon
    [J]. PHOTODIAGNOSIS AND PHOTODYNAMIC THERAPY, 2020, 31
  • [8] Influence of silver diamine fluoride compared to photodynamic therapy on the bond integrity of resin modified glass ionomer cement to demineralized dentin
    Alshahrani, Abdullah
    [J]. PHOTODIAGNOSIS AND PHOTODYNAMIC THERAPY, 2020, 32
  • [9] Arias Vanessa Gallego, 2004, Braz. Dent. J., V15, P194
  • [10] Influence of graphene oxide filler content on the dentin bond integrity, degree of conversion and bond strength of experimental adhesive. A SEM, micro-Raman, FTIR and microtensile study
    Bin-Shuwaish, Mohammed S.
    Maawadh, Ahmed M.
    Al-Hamdan, Rana S.
    Alresayes, Saad
    Ali, Thamer
    Almutairi, Basil
    Vohra, Fahim
    Abduljabbar, Tariq
    [J]. MATERIALS RESEARCH EXPRESS, 2020, 7 (11)