Corrosion Behaviour of AZ63 Magnesium Alloy in Natural Seawater and 3.5 wt.% NaCl Aqueous Solution

被引:24
作者
Yang, Lihui [1 ,2 ,3 ]
Lin, Cunguo [2 ]
Gao, Haiping [2 ]
Xu, Weichen [1 ,3 ]
Li, Yantao [1 ,3 ]
Hou, Baorong [1 ,3 ]
Huang, Yanliang [1 ,3 ]
机构
[1] Chinese Acad Sci, Inst Oceanol, Key Lab Marine Environm Corros & Biofouling, Qingdao 266071, Peoples R China
[2] LSMRI, State Key Lab Marine Corros & Protect, Qingdao 266101, Peoples R China
[3] Qingdao Natl Lab Marine Sci & Technol, Open Studio Marine Corros & Protect, Qingdao 266237, Peoples R China
来源
INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE | 2018年 / 13卷 / 08期
关键词
AZ63 magnesium alloy; corrosion behaviour; polarization curve; seawater; AL-ZN ALLOYS; CALCAREOUS DEPOSITS; ACTIVATED BATTERY; MG; MICROSTRUCTURE; STEEL; ANODE;
D O I
10.20964/2018.08.32
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
In this study, the corrosion behaviour of AZ63 magnesium alloy was investigated in natural seawater and neutral 3.5 wt.% NaCl aqueous solution. The electrochemical processes were studied using potentiodynamic polarization. The composition and morphology of the alloys and corrosion products formed were studied using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The experimental results highlighted the differences between the corrosion mechanisms of AZ63 magnesium alloy in natural seawater and that in 3.5 wt.% NaCl solution. The corrosion products formed in the seawater primarily consisted of CaCO3 and Mg(OH)(2), while the corrosion products formed in the 3.5 wt.% NaCl solution primarily consisted of Mg(OH)(2) and Mg-2(OH)(3)Cl center dot 4H(2)O. The results of hydrogen evolution, weight loss and potentiodynamic polarization tests showed that the AZ63 magnesium alloy samples had better corrosion resistance in natural seawater than in 3.5 wt.% NaCl aqueous solution.
引用
收藏
页码:8084 / 8093
页数:10
相关论文
共 50 条
[31]   Effect of Cr addition on corrosion behavior of cupronickel alloy in 3.5 wt% NaCl solution [J].
Li, Shifang ;
Fang, Mei ;
Xiao, Zhu ;
Meng, Xiangpeng ;
Lei, Qian ;
Jia, Yanlin .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 22 :2222-2238
[32]   Corrosion Behavior of Cu-Ni-Fe-Mn-Cr Alloy in 3.5 wt% NaCl Solution [J].
Li, Shifang ;
Xiao, Zhu ;
Fang, Mei ;
Xie, Haofeng ;
Peng, Lijun .
CORROSION, 2024, 80 (09) :889-898
[33]   The impact of homogenization treatment on microstructure microhardness and corrosion behavior of wrought AZ80 magnesium alloys in 3.5 wt% NaCl solution [J].
Naik, Gajanan M. ;
Gote, Gopal D. ;
Narendranath, S. ;
Kumar, S. S. Satheesh .
MATERIALS RESEARCH EXPRESS, 2018, 5 (08)
[34]   Investigation of electrochemical corrosion behavior in a 3.5 wt.% NaCl solution of boronized dual-phase steel [J].
Kayali, Yusuf ;
Anaturk, Bilal .
MATERIALS & DESIGN, 2013, 46 :776-783
[35]   In-Situ Raman Characterization of Initial Corrosion Behavior of Copper in Neutral 3.5% (wt.) NaCl Solution [J].
Liu, Ming ;
Li, Jun .
MATERIALS, 2019, 12 (13)
[36]   Corrosion behaviors of Cr2AlC/α-Al2O3 composites in 3.5 wt. % NaCl aqueous solution [J].
Zhang, Zerong ;
Qian, Yuhai ;
Xu, Jingjun ;
Zuo, Jun ;
Li, Meishuan .
CERAMICS INTERNATIONAL, 2020, 46 (08) :11846-11853
[37]   Study of the corrosion behavior and the corrosion films formed on the surfaces of Mg-xSn alloys in 3.5 wt.% NaCl solution [J].
Wang, Jingfeng ;
Li, Yang ;
Huang, Song ;
Zhou, Xiaoen .
APPLIED SURFACE SCIENCE, 2014, 317 :1143-1150
[38]   Electrochemical behavior of Mg-Al-Zn-In alloy as anode materials in 3.5 wt.% NaCl solution [J].
Li, Jiarun ;
Zhang, Binbin ;
Wei, Qinyi ;
Wang, Ning ;
Hou, Baorong .
ELECTROCHIMICA ACTA, 2017, 238 :156-167
[39]   Corrosion-Wear Mechanism of (AlTiV)100-xCrx Lightweight High-Entropy Alloy in the 3.5 wt.% NaCl Solution [J].
Huang, Jiakai ;
Zhang, Peng ;
Yang, Junjie ;
Li, Wei ;
Wang, Qiwei ;
Li, Jie .
MATERIALS, 2025, 18 (11)
[40]   Electrochemical behaviour of dental amalgam in natural, artificial saliva and in 0.90 wt.% NaCl solution [J].
Chowdhury, Nivedita Dutta ;
Ghosh, K. S. .
CORROSION SCIENCE, 2018, 133 :217-230