The Effect of Strain Rate on the Deformation Behavior of Fe-30Mn-8Al-1.0C Austenitic Low-Density Steel

被引:6
作者
Du, Jiahui [1 ]
Chen, Peng [1 ,2 ]
Guan, Xianjun [1 ]
Cai, Jiawei [1 ]
Peng, Qian [1 ]
Lin, Chuang [1 ]
Li, Xiaowu [1 ,3 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Dept Mat Phys & Chem, Shenyang 110819, Peoples R China
[2] Northeastern Univ, Key Lab Anisotropy & Texture Mat, Shenyang 110819, Peoples R China
[3] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
基金
中国国家自然科学基金;
关键词
strain rate; mechanical property; austenitic low-density steel; strain hardening; microstructure; deformation mechanism; STRENGTH-DUCTILITY MATCH; TENSILE DEFORMATION; SPINODAL DECOMPOSITION; MECHANICAL-PROPERTIES; INDUCED PLASTICITY; MN; ALLOYS; ORIGIN; TRANSFORMATION; PRECIPITATION;
D O I
10.3390/met12081374
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Automotive steels suffer different strain rates during their processing and service. In this study, the effect of strain rates on the tensile properties of fully austenitic Fe-30Mn-8Al-1.0C (wt.%) steel was investigated, and the dominant deformation mechanism was clarified. Conventional and interrupted tension tests and various microscopic characterization methods were carried out in this study. The results indicate that the yield strength increases with the increasing strain rate in the range of 10(-4)-10(-1) s(-1), and a good strength-ductility combination was achieved in the sample deformed at 10(-3) s(-1). In the process of straining at 10(-3) s(-1), microbands and deformation twins were observed. Thus, the combination of microband induced plasticity (MBIP) together with twinning induced plasticity (TWIP) leads to a continuous strain hardening behavior, and consequently to superior mechanical properties. However, adiabatic heating that leads to the increase in stacking fault energy (SFE) and inhibits the TWIP effect, as well as thermal softening jointly induces an anomalous decrease in tensile strength at the high strain rate of 10(-1) s(-1).
引用
收藏
页数:9
相关论文
共 37 条
  • [1] Orientation evolution in Hadfield steel single crystals under combined slip and twinning
    Canadinc, D.
    Sehitoglu, H.
    Maier, H. J.
    Niklasch, D.
    Chumlyakov, Y. I.
    [J]. INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2007, 44 (01) : 34 - 50
  • [2] A high specific Young's modulus steel reinforced by spheroidal kappa-carbide
    Chen, P.
    Fu, J.
    Xu, X.
    Lin, C.
    Pang, J. C.
    Li, X. W.
    Misra, R. D. K.
    Wang, G. D.
    Yi, H. L.
    [J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 87 : 54 - 59
  • [3] The origin of the brittleness of high aluminum pearlite and the method for improving ductility
    Chen, P.
    Xiong, X. C.
    Wang, G. D.
    Yi, H. L.
    [J]. SCRIPTA MATERIALIA, 2016, 124 : 42 - 46
  • [4] The κ-Carbides in Low-Density Fe-Mn-Al-C Steels: A Review on Their Structure, Precipitation and Deformation Mechanism
    Chen, Peng
    Li, Xiaowu
    Yi, Hongliang
    [J]. METALS, 2020, 10 (08) : 1 - 14
  • [5] Current state of Fe-Mn-Al-C low density steels
    Chen, Shangping
    Rana, Radhakanta
    Haldar, Arunansu
    Ray, Ranjit Kumar
    [J]. PROGRESS IN MATERIALS SCIENCE, 2017, 89 : 345 - 391
  • [6] Phase transformation of the L12 phase to kappa-carbide after spinodal decomposition and ordering in an Fe-C-Mn-Al austenitic steel
    Cheng, Wei-Chun
    Cheng, Chih-Yao
    Hsu, Chia-Wei
    Laughlin, David E.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 642 : 128 - 135
  • [7] Microstructural change in austenitic Fe-30.0wt%Mn-7.8wt%Al-1.3wt%C initiated by spinodal decomposition and its influence on mechanical properties
    Choo, WK
    Kim, JH
    Yoon, JC
    [J]. ACTA MATERIALIA, 1997, 45 (12) : 4877 - 4885
  • [8] Dependence of tensile deformation behavior of TWIP steels on stacking fault energy, temperature and strain rate
    Curtze, S.
    Kuokkala, V. -T.
    [J]. ACTA MATERIALIA, 2010, 58 (15) : 5129 - 5141
  • [9] Microstructures and mechanical properties of high-strength Fe-Mn-Al-C light-weight TRIPLEX steels
    Frommeyer, Georg
    Bruex, Udo
    [J]. STEEL RESEARCH INTERNATIONAL, 2006, 77 (9-10) : 627 - 633
  • [10] ON THE ORIGIN OF PLANAR SLIP IN FCC ALLOYS
    GEROLD, V
    KARNTHALER, HP
    [J]. ACTA METALLURGICA, 1989, 37 (08): : 2177 - 2183