Thermodynamic evaluation of hypereutectic Al-Si (A390) alloy with addition of Mg

被引:62
作者
Hekmat-Ardakan, Alireza [1 ]
Ajersch, Frank [1 ]
机构
[1] Ecole Polytech, Dep Genie Chim, Montreal, PQ H3C 3A7, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Thermodynamic; Factsage Aluminum alloys; Eutectic solidification; Magnesium; WEAR BEHAVIOR; SLIDING WEAR; COMPOSITE; CU;
D O I
10.1016/j.actamat.2010.02.017
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper presents the thermodynamic evaluation of A390 hypereutectic Al-Si alloy (Al-17% Si-4.5% Cu-0.5% Mg) and alloys up to 10% Mg, using the Factsage (R) software. Two critical compositions were detected at 4.2% and 7.2% Mg where the temperatures of the liquidus, the start of the binary and of the ternary eutectic reaction are changed. These critical compositions show differences in the formation of Mg,Si intermetallic particles during the solidification interval. For compositions up to 4.2% Mg, the Mg2Si intermetallic phase first appears in the ternary eutectic zone. With Mg contents between 4.2% and 7.2%, Mg2Si particle appears in both the binary and ternary eutectic reactions. Above 7.2% Mg, it solidifies as a primary phase and also during the binary and ternary reactions. The calculated liquid fraction vs. temperature curves also showed a decrease of the eutectic formation temperature (knee point temperature) with the addition of Mg content up to 4.2% Mg. This temperature becomes almost constant up to 10% Mg. The calculation of eutectic formation temperature shows a good agreement with differential scanning calorimetry (DSC) tests. (C) 2010 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:3422 / 3428
页数:7
相关论文
共 16 条
[11]  
Mondolfo L.F., 1978, MANGANESE ALUMINUM A
[12]   Effects of modification during conventional and semi-solid metal processing of A356 Al-Si alloy [J].
Nafisi, S ;
Ghomashchi, R .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 415 (1-2) :273-285
[13]   Dry sliding wear behavior of Mg2Si/Al composites against automobile friction material [J].
Qin, Q. D. ;
Zhao, Y. G. ;
Zhou, W. .
WEAR, 2008, 264 (7-8) :654-661
[14]   A comparison of the sliding wear behavior of a hypereutectic Al-Si alloy prepared by spray-deposition and conventional casting methods [J].
Wang, F ;
Ma, YJ ;
Zhang, ZY ;
Cui, XH ;
Jin, YS .
WEAR, 2004, 256 (3-4) :342-345
[15]   Microstructural development of Al-15wt.%Mg2Si in situ composite with mischmetal addition [J].
Zhang, J ;
Fan, Z ;
Wang, YQ ;
Zhou, BL .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 281 (1-2) :104-112
[16]   In situ Mg2Si/Al-Si composite modified by K2TiF6 [J].
Zhao, YG ;
Qin, QD ;
Zhao, YQ ;
Liang, YH ;
Jiang, QC .
MATERIALS LETTERS, 2004, 58 (16) :2192-2194