Microstructural and electrical properties of CaTiO3-CaCu3Ti4O12 ceramics

被引:44
|
作者
Wang, Chih-Ming [1 ]
Lin, Shih-Yuan [2 ]
Kao, Kuo-Sheng [3 ]
Chen, Ying-Chung [2 ]
Weng, Shang-Chih [1 ]
机构
[1] Cheng Shiu Univ, Dept Elect Engn, Kaohsiung 833, Taiwan
[2] Natl Sun Yat Sen Univ, Dept Elect Engn, Kaohsiung 804, Taiwan
[3] Shu Te Univ, Dept Comp & Commun, Kaohsiung 824, Taiwan
关键词
Solid-state reactions; Ceramics; Sintering; Microstructure; Dielectric response; HIGH-DIELECTRIC-CONSTANT; BARRIER LAYER CAPACITORS; CACU3TI4O12; THIN-FILMS; STOICHIOMETRY; CU;
D O I
10.1016/j.jallcom.2009.10.216
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This study investigates the microstructure and dielectric properties of (CrO)(1-x)-(CCTO)(x) ceramics. X-ray diffraction (XRD) patterns show that the crystal phases of polycrystalline CCTO exhibit a (2 2 0) preferential orientation at the molar fraction x = 1. For (CTO)(2/3)-(CCTO)(1/3) or (CTC)(1/3)-(CCTO)(2/3) ceramics, the crystalline structures of CTO and CCTO coexist at x = 1/3 and 2/3, respectively. Surface scanning electron microscope (SEM) morphologies show that the CCTO with x = 1 sintered above 1010 degrees C exhibits liquid-phase secondary recrystallization (LPSR) regions, and these regions expand as the sintering temperature increases. Therefore, the grain size and ceramics density depends on the sintering temperature and composition. This suggests that CCTO prepared at x = 1 can be a good candidate for capacitor applications because of its high epsilon value. The dielectric properties of CCTO sintered at 1100 degrees C include a dielectric constant (epsilon) of 23,600, dielectric loss (tan delta) of 0.406 at 10 kHz, leakage current density (J) of 6.11 x 10(-6) A/cm(2) and conductivity (sigma) of 6.11 x 10(-9) Omega cm(-1) at 1 kV/cm. (C) 2009 Elsevier B.V. All rights reserved
引用
收藏
页码:423 / 430
页数:8
相关论文
共 50 条
  • [41] Influence of sintering conditions on microstructure and electrical properties of CaCu3Ti4O12 (CCTO) ceramics
    Liu, Pei
    Lai, Yuanming
    Zeng, Yiming
    Wu, Shuang
    Huang, Zihan
    Han, Jiao
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 650 : 59 - 64
  • [42] Electrodes influence on the characterization of the electrical properties of colossal permittivity CaCu3Ti4O12 ceramics
    Mao, Pu
    Lu, Gang
    Yan, Qingsong
    Annadi, Anil
    Guo, Yongguang
    Wang, Zepeng
    Liu, Zhiyong
    Xie, Bing
    Zhang, Lixue
    CERAMICS INTERNATIONAL, 2022, 48 (21) : 32156 - 32163
  • [43] Evolution of the intergranular phase during sintering of CaCu3Ti4O12 ceramics
    Romero, J. J.
    Leret, P.
    Rubio-Marcos, F.
    Quesada, A.
    Fernandez, J. F.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2010, 30 (03) : 737 - 742
  • [44] Dielectric properties of CaCu3Ti4O12 based multiphased ceramics
    Guillemet-Fritsch, S
    Lebey, T
    Boulos, M
    Durand, B
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2006, 26 (07) : 1245 - 1257
  • [45] Preparation, characterization and dielectric properties of CaCu3Ti4O12 ceramics
    Zhao, Jingchang
    Liu, Jia
    Ma, Guang
    CERAMICS INTERNATIONAL, 2012, 38 (02) : 1221 - 1225
  • [46] Dielectric and nonlinear electrical behaviors of La-doped CaCu3Ti4O12 ceramics
    Cheng, Bo
    Lin, Yuan-Hua
    Yuan, Jiancong
    Cai, Jingnan
    Nan, Ce-Wen
    Xiao, Xi
    He, Jinliang
    JOURNAL OF APPLIED PHYSICS, 2009, 106 (03)
  • [47] Microstructures and electrical responses of pure and chromium-doped CaCu3Ti4O12 ceramics
    Zheng, Qian
    Fan, Huiqing
    Long, Changbai
    JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 511 (01) : 90 - 94
  • [48] Effects of PVA organic binder on electric properties of CaCu3Ti4O12 ceramics
    Yuan, Wen-Xiang
    Li, Z. J.
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2012, 73 (04) : 599 - 603
  • [49] Calcination and sintering effects on the microstructure and dielectric properties of CaCu3Ti4O12 ceramics
    Cao, Lei
    Liu, Peng
    Zhou, Jian-Ping
    Wang, Ya-Juan
    Su, Li-Na
    Liu, Cheng
    Zhang, Huai-Wu
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2010, 11 (04): : 453 - 459
  • [50] Effect of doping ions on the structural defect and the electrical behavior of CaCu3Ti4O12 ceramics
    Xue, Renzhong
    Zhao, Gaoyang
    Chen, Jing
    Chen, Zhenping
    Liu, Dewei
    MATERIALS RESEARCH BULLETIN, 2016, 76 : 124 - 132