Corrosion behaviour of mechanically polished AA7075-T6 aluminium alloy

被引:55
作者
Liu, Y. [1 ]
Laurino, A. [2 ]
Hashimoto, T. [1 ]
Zhou, X. [1 ]
Skeldon, P. [1 ]
Thompson, G. E. [1 ]
Scamans, G. M. [3 ]
Blanc, C. [2 ]
Rainforth, W. M. [4 ]
Frolish, M. F. [4 ]
机构
[1] Univ Manchester, Ctr Corros & Protect, Sch Mat, Manchester M60 1QD, Lancs, England
[2] CNRS, CIRIMAT, ENSIACET, UMR 5085, F-31077 Toulouse, France
[3] Innoval Technol, Beaumont Close, Banbury OX16 1TQ, Oxon, England
[4] Univ Sheffield, Dept Mat Engn, Sheffield S1 3JD, S Yorkshire, England
基金
英国工程与自然科学研究理事会;
关键词
AA7075 aluminium alloy; corrosion; near-surface deformed layer; grain boundary; FILIFORM CORROSION; 1ST BREAKDOWN; SHEET;
D O I
10.1002/sia.3136
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the present study, the effects of mechanical polishing on the microstructure and corrosion behaviour of AA7075 aluminium alloy are investigated. It was found that a nano-grained, near-surface deformed layer, up to 400 nm thickness, is developed due to significant surface shear stress during mechanically polishing. Within the near-surface deformed layer, the alloying elements have been redistributed and the microstructure of the alloy is modified; in particular, the normal MgZn2 particles for T6 are absent. However, segregation bands, approximately 10-nm thick, containing mainly zinc, are found at the grain boundaries within the near-surface deformed layer. The presence of such segregation bands promoted localised corrosion along the grain boundaries within the near-surface deformed layer due to microgalvanic action. During anodic polarisation of mechanically polished alloy in sodium chloride solution, two breakdown potentials were observed at -750 mV and -700 mV, respectively. The first breakdown potential is associated with an increased electrochemical activity of the near-surface deformed layer, and the second breakdown potential is associated with typical pitting of the bulk alloy. Copyright (C) 2009 John Wiley & Sons, Ltd.
引用
收藏
页码:185 / 188
页数:4
相关论文
共 10 条
[1]   Formation and evolution of a subsurface layer in a metalworking process [J].
Fishkis, M ;
Lin, JC .
WEAR, 1997, 206 (1-2) :156-170
[2]  
Humphreys FJ, 2017, Recrystallization and Related Annealing Phenomena, Vthird
[3]   Surface morphological changes of aluminium alloys in alkaline solution: effect of second phase material [J].
Koroleva, EV ;
Thompson, GE ;
Hollrigl, G ;
Bloeck, M .
CORROSION SCIENCE, 1999, 41 (08) :1475-1495
[4]   Filiform corrosion of aluminium sheet. I. Corrosion behaviour of painted material [J].
Leth-Olsen, H ;
Nisancioglu, K .
CORROSION SCIENCE, 1998, 40 (07) :1179-1194
[5]   Precipitation in an AA6111 aluminium alloy and cosmetic corrosion [J].
Liu, Y. ;
Zhou, X. ;
Thompson, G. E. ;
Hashimoto, T. ;
Scamans, G. M. ;
Afseth, A. .
ACTA MATERIALIA, 2007, 55 (01) :353-360
[6]  
Plassart G., 2000, P 2 INT C AL SURF SC, P29
[7]  
Scamans G.M., 2000, P 2 INT C AL SURF SC, P9
[8]   On the first breakdown in AA7075-T6 [J].
Zhao, Zhijun ;
Frankel, G. S. .
CORROSION SCIENCE, 2007, 49 (07) :3064-3088
[9]   The effect of temper on the first breakdown in AA7075 [J].
Zhao, Zhijun ;
Frankel, G. S. .
CORROSION SCIENCE, 2007, 49 (07) :3089-3111
[10]   The influence of surface treatment on filiform corrosion resistance of painted aluminium alloy sheet [J].
Zhou, X ;
Thompson, GE ;
Scamans, GM .
CORROSION SCIENCE, 2003, 45 (08) :1767-1777