Hydrothermal solidification of blast furnace slag by formation of tobermorite

被引:43
作者
Jing, Zhenzi
Jin, F.
Hashida, T.
Yamasaki, N.
Ishida, H.
机构
[1] Tohoku Univ, Grad Sch Environm Studies, Aoba Ku, Sendai, Miyagi 9808579, Japan
[2] Tongji Univ, Sch Environm Sci & Engn, Shanghai 200092, Peoples R China
[3] Tohoku Univ, Fracture & Reliab Res Inst, Aoba Ku, Sendai, Miyagi 9808579, Japan
关键词
Flyash; Portland Cement; Blast Furnace Slag; Calcium Silicate Hydrate; Strength Development;
D O I
10.1007/s10853-007-1726-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Blast furnace water-cooled slag (BFWS) has been solidified using a hydrothermal processing method, in which the BFWS could be solidified in an autoclave under saturated steam pressure (1.56 MPa) at 200 degrees C for 12 h by the additions of quartz or coal flyash. The tensile strength development was shown to depend on the formation of tobermorite and the packing state of the formed tobermorite in the solidified bodies. The additions of quartz or fly ash were proved to be favorable not only to the formation of tobermorite but also to the transformation of hibschite, the former improving the strength, and the latter deteriorating the strength. The excessive addition of quartz appeared to cause strength deterioration due to the fact that the residual quartz affected the formation of tobermorite in the solidified bodies.
引用
收藏
页码:8236 / 8241
页数:6
相关论文
共 13 条
[1]  
BIENIAWSKI ZT, 1978, INT J ROCK MECH MIN, V15, P99
[2]  
BRUNAUER S, 1962, AM SCI, V50, P210
[3]  
Brunauer S., 1973, Cem. Concr. Res, V3, P279, DOI 10.1016/0008-8846(73)90031-8.
[4]  
BUDNIKOV PP, 1986, J DM MENDELEEV CHEM, V13, P176
[5]  
EMILE H, 2002, ENCY SMART MAT, P1014
[6]  
Higgins DD, 1995, WORLD CEM, V6, P51
[7]  
*JAP CER IND, 2005, CERAMICS JAPAN, V40, P710
[8]   Solidification of coal fly ash using hydrothermal processing method [J].
Jing, Z ;
Matsuoka, N ;
Jin, F ;
Yamasaki, N ;
Suzuki, K ;
Hashida, T .
JOURNAL OF MATERIALS SCIENCE, 2006, 41 (05) :1579-1584
[9]   Municipal incineration bottom ash treatment using hydrothermal solidification [J].
Jing, Zhenzi ;
Matsuoka, Norihisa ;
Jin, Fangming ;
Hashida, Toshiyuki ;
Yamasaki, Nakamichi .
WASTE MANAGEMENT, 2007, 27 (02) :287-293
[10]   Hydrogarnet formation during autoclaving at 180°C in unstirred metakaolin-lime-quartz slurries [J].
Klimesch, DS ;
Ray, A .
CEMENT AND CONCRETE RESEARCH, 1998, 28 (08) :1109-1117