Analysis of internal corrosion of supercritical CO2 pipeline

被引:17
作者
Tang, Sen [1 ,2 ]
Zhu, Chengyuan [1 ,2 ]
Cui, Gan [1 ,2 ]
Xing, Xiao [1 ,2 ]
Mu, Jie [1 ,2 ]
Li, Zili [1 ,2 ]
机构
[1] China Univ Petr East China, Coll Pipeline & Civil Engn, Qingdao 266580, Peoples R China
[2] Shandong Key Lab Oil & Gas Storage & Transportat, Qingdao 266580, Peoples R China
基金
中国国家自然科学基金;
关键词
anticorrosive; CCS; corrosion; impurity; material; X65; CARBON-STEEL; LOW-ALLOY STEEL; WATER-CONTENT; ELECTROCHEMICAL CORROSION; TRANSPORT PIPELINES; LOCALIZED CORROSION; DIOXIDE CORROSION; STAINLESS-STEEL; MILD-STEEL; X70; STEEL;
D O I
10.1515/corrrev-2020-0041
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Carbon capture and storage (CCS) technology is considered to be one of the key technologies to reduce CO2 emissions. This paper reviews the industry corrosion accidents of CCS transportation system, in which the pipeline corrosion risk is analyzed, and the pipeline corrosion theory is summarized. Also, the effect of impurities on gas phase properties is discussed. We analyze the corrosion mechanism of multicomponent impurities on metals in a supercritical CO2 environment from the aspects of corrosion rate and corrosion products. We also describe the mechanism of pitting and stress corrosion of metals in a supercritical CO2 environment. Besides, the formation mechanism of FeCO3 protective layer and the research status of corrosion resistant alloys in supercritical CO2 are reviewed and analyzed. Finally, a series of shortcomings and prospects of the current research are put forward.
引用
收藏
页码:219 / 241
页数:23
相关论文
共 54 条
[1]   Update of DNV recommended practice RP-J202 with focus on CO2 Corrosion with Impurities [J].
Brown, Jock ;
Graver, Brit ;
Gulbrandsen, Egil ;
Dugstad, Arne ;
Morland, Bjorn .
12TH INTERNATIONAL CONFERENCE ON GREENHOUSE GAS CONTROL TECHNOLOGIES, GHGT-12, 2014, 63 :2432-2441
[2]   Corrosion of austenitic alloys in high temperature supercritical carbon dioxide [J].
Cao, G. ;
Firouzdor, V. ;
Sridharan, K. ;
Anderson, M. ;
Allen, T. R. .
CORROSION SCIENCE, 2012, 60 :246-255
[3]   Effect of chromium on the pitting resistance of oil tube steel in a carbon dioxide corrosion system [J].
Chen, CF ;
Lu, MX ;
Sun, DB ;
Zhang, ZH ;
Chang, W .
CORROSION, 2005, 61 (06) :594-601
[4]   Determining the corrosive potential of CO2 transport pipeline in high pCO2-water environments [J].
Choi, Yoon-Seok ;
Nesic, Srdjan .
INTERNATIONAL JOURNAL OF GREENHOUSE GAS CONTROL, 2011, 5 (04) :788-797
[5]   Effect of Impurities on the Corrosion Behavior of CO2 Transmission Pipeline Steel in Supercritical CO2-Water Environments [J].
Choi, Yoon-Seok ;
Nesic, Srdjan ;
Young, David .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2010, 44 (23) :9233-9238
[6]   Microstructure dependence of stress corrosion cracking initiation in X-65 pipeline steel exposed to a near-neutral pH soil environment [J].
Chu, R ;
Chen, W ;
Wang, SH ;
King, F ;
Jack, TR ;
Fessler, RR .
CORROSION, 2004, 60 (03) :275-283
[7]   Corrosion of pipelines used for CO2 transport in CCS: Is it a real problem? [J].
Cole, Ivan S. ;
Corrigan, Penny ;
Sim, Samson ;
Birbilis, Nick .
INTERNATIONAL JOURNAL OF GREENHOUSE GAS CONTROL, 2011, 5 (04) :749-756
[8]   A comprehensive review of metal corrosion in a supercritical CO2 environment [J].
Cui, Gan ;
Yang, Ziqing ;
Liu, Jianguo ;
Li, Zili .
INTERNATIONAL JOURNAL OF GREENHOUSE GAS CONTROL, 2019, 90
[9]   Study on corrosion properties of pipelines in simulated produced water saturated with supercritical CO2 [J].
Cui, ZD ;
Wu, SL ;
Zhu, SL ;
Yang, XJ .
APPLIED SURFACE SCIENCE, 2006, 252 (06) :2368-2374
[10]   PREPARATION AND DECOMPOSITION OF AMMONIOJAROSITE AT ELEVATED-TEMPERATURES IN H2O-(NH4)(2)SO4-H2SO4 MEDIA [J].
DAS, GK ;
ANAND, S ;
ACHARYA, S ;
DAS, RP .
HYDROMETALLURGY, 1995, 38 (03) :263-276