Effect of organic and inorganic compounds on dissolution kinetics of chalcopyrite in hydrogen peroxide- Hydrochloric acid system

被引:13
作者
Abdelraheem, Mohamed Taha Osman [1 ]
Agacayak, Tevfik [2 ]
机构
[1] Omdurman Islamic Univ, Dept Min Engn, Khartoum, Sudan
[2] Konya Tech Univ, Dept Min Engn, Konya, Turkey
关键词
Activation energy; Chalcopyrite; Hydrogen peroxide; Hydrochloric acid; Leaching; Diffusion control; PART I; COPPER; CONCENTRATE; EXTRACTION; SULFIDE; MEDIA;
D O I
10.1016/j.jscs.2022.101478
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The addition of 2-Propanol as an organic substance and NaCl as an inorganic com-pound in hydrochloric acid with hydrogen peroxide as a strong leaching agent of chalcopyrite was investigated. The effects of the leaching parameters on copper extraction, such as stirring speed, H2O2 concentration, temperature, HCl concentration and solid/liquid ratio were studied. The max-imum final copper extraction of 54.55% was obtained with 600 rpm stirring speed, 1.5 M H2O2, 0.5 M HCl, 600 rpm, 50 C, 240 min of the reaction and particle size of -106 +75 mm. Further experiments were performed when the solid-to-liquid ratio (S/L), stirring speed, temperature, HCl,H2O2 and leaching time were kept constant to examine the influence of NaCl and 2-Propanol concentrations in the range of 0-0.5 M and 0-3 M, respectively. The results showed that the copper extraction was increased up to 58.11% with addition of NaCl. While copper extraction yield reached 94.25% in case of addition of 2-propanol with the optimum parameters(0.5 M HCl,50 C, 1.5 M H2O2, 600 rpm, particle size -106 +75 lm, solid liquid ratio 2g/L, 3 M 2-propanol). The chalcopyrite leaching in hydrogen peroxide- hydrochloric acid system was found to be described by the interface transfer and diffusion across the product layer with activation energy of 77.14 kJ/mol. Addition of 2-propanol suggested that the reaction was under product layer diffusion control and decreased the activation energy of chalcopyrite leaching to 67.98 kJ/mol. Crown Copyright (c) 2022 Published by Elsevier B.V. on behalf of King Saud University.
引用
收藏
页数:9
相关论文
共 24 条
[1]   LEACHING OF CHALCOPYRITE CONCENTRATE IN HYDROGEN PEROXIDE SOLUTION [J].
Agacayak, Tevfik ;
Aras, Ali ;
Aydogan, Salih ;
Erdemoglu, Murat .
PHYSICOCHEMICAL PROBLEMS OF MINERAL PROCESSING, 2014, 50 (02) :657-666
[2]   Leaching of pyrite with hydrogen peroxide in sulphuric acid [J].
Antonijevic, MM ;
Dimitrijevic, M ;
Jankovic, Z .
HYDROMETALLURGY, 1997, 46 (1-2) :71-83
[3]   Chalcopyrite Leaching with Hydrogen Peroxide in Formic Acid Medium [J].
Arslanoglu, Hasan ;
Yaras, Ali .
TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2020, 73 (03) :785-792
[4]  
Baba AFA., 2009, J. Miner. Mater. Charact. Eng., V8, P787
[5]   Dissolution kinetics of malachite in ammonia/ammonium carbonate leaching [J].
Bingöl, D ;
Canbazoglu, M ;
Aydogan, S .
HYDROMETALLURGY, 2005, 76 (1-2) :55-62
[6]   Leaching of chalcopyrite with ferric ion.: Part I:: General aspects [J].
Cordoba, E. M. ;
Munoz, J. A. ;
Blazquez, M. L. ;
Gonzalez, F. ;
Ballester, A. .
HYDROMETALLURGY, 2008, 93 (3-4) :81-87
[7]  
DALTON RF, 1991, JOM-J MIN MET MAT S, V43, P51
[8]  
Dickinson CF, 1999, THERMOCHIM ACTA, V341, P89
[9]  
Dixon DG, 2008, CAN METALL QUART, V47, P327, DOI 10.1179/000844308794408317
[10]   PASSIVATION OF CHALCOPYRITE DURING OXIDATIVE LEACHING IN SULFATE MEDIA [J].
HACKL, RP ;
DREISINGER, DB ;
PETERS, E ;
KING, JA .
HYDROMETALLURGY, 1995, 39 (1-3) :25-48