Mechanical properties of cast A356 alloy, solidified at cooling rates enhanced by phase transition of a cooling medium

被引:38
作者
Zhang, L. Y. [1 ]
Zhou, B. D.
Zhan, Z. J.
Jia, Y. Z.
Shan, S. F.
Zhang, B. Q.
Wang, W. K.
机构
[1] Yanshan Univ, Sch Mat Sci & Engn, Qinhuangdao 066004, Peoples R China
[2] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[3] Yanshan Univ, R&D Ctr Adv Mat, Qinhuangdao 066004, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2007年 / 448卷 / 1-2期
关键词
phase transition cooling; A356 casting alloy; mechanical properties; solidification microstructure; solid solubility;
D O I
10.1016/j.msea.2006.10.025
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Phase transition cooling (PTC), using the absorbed latent heat during the melting of phase transition cooling medium to cool and solidify alloys in the process of casting, is a new fast cooling technology. Specimens of A356 casting aluminum alloy were prepared by this method. For comparison. specimens made by water-cooling copper mould (WCCM) were prepared too. The mechanical properties of A356 alloy made by PTC and WCCM were measured by microhardness and tensile strength testing methods. Microstructures of A356 alloy were investigated by scanning electron microscopy (SEM), differential scanning calorimetry (DSC) and X-rays diffraction (XRD). The results show that both microhardness and ultimate tensile strength (UTS) of A356 alloy made by PTC method are much higher than those made by WCCM method. This can be attributed to the refined microstructure and the extended solubility of silicon in alpha-Al. The solubility of silicon in a-Al was 2.7 at.% in specimens solidified in phase transition cooling medium and 2.4 at.% in specimens solidified in water-cooling copper mould. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:361 / 365
页数:5
相关论文
共 14 条
[1]  
BENDJIK A, 1980, J MATER SCI, V28, P2803
[2]   A study of high-temperature precipitation in Al-Mg-Si alloys with an excess of silicon [J].
Eskin, DG ;
Massardier, V ;
Merle, P .
JOURNAL OF MATERIALS SCIENCE, 1999, 34 (04) :811-820
[3]   Analysis of variability in tensile ductility of a semi-solid metal cast A356 Al-alloy [J].
Gokhale, AM ;
Patel, GR .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 392 (1-2) :184-190
[4]   Effect of power ultrasound on solidification of aluminum A356 alloy [J].
Jian, X ;
Xu, H ;
Meek, TT ;
Han, Q .
MATERIALS LETTERS, 2005, 59 (2-3) :190-193
[5]   Electromagnetic stirring and Sr modification in A356 alloy [J].
Jung, BI ;
Jung, CH ;
Han, TK ;
Kim, YH .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 111 (1-3) :69-73
[6]   Microstructure of Al-Si-Mg alloy processed by rotary-die equal channel angular pressing [J].
Kim, JC ;
Nishida, Y ;
Arima, H ;
Ando, T .
MATERIALS LETTERS, 2003, 57 (11) :1689-1695
[7]   Microstructures and mechanical properties of 6061 aluminum alloy processed by accumulative roll-bonding [J].
Lee, SH ;
Saito, Y ;
Sakai, T ;
Utsunomiya, H .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 325 (1-2) :228-235
[8]   Age-hardening behavior of cast Al-Si base alloy [J].
Li, RX ;
Li, RD ;
Zhao, YH ;
He, LZ ;
Li, CX ;
Guan, HR ;
Hu, ZQ .
MATERIALS LETTERS, 2004, 58 (15) :2096-2101
[9]   Correlation between mechanical properties and amount of dendritic α-Al phase in as-cast near-eutectic Al-11.6% Si alloys modified with strontium [J].
Liao, HC ;
Sun, Y ;
Sun, GX .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 335 (1-2) :62-66
[10]   CRYSTAL SYSTEM OF ROD-SHAPED PRECIPITATES IN AN AL-1.0MASS-PERCENT-MG2SI-0.4MASS-PERCENT SI ALLOY [J].
MATSUDA, K ;
TADA, S ;
IKENO, S ;
SATO, T ;
KAMIO, A .
SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (08) :1175-1180