Mold growth on nonceramic insulators and its impact on electrical performance

被引:42
作者
Gorur, RS [1 ]
Montesinos, J
Roberson, R
Burnham, J
Hill, R
机构
[1] Arizona State Univ, Tempe, AZ 85287 USA
[2] Florida Power & Light Co, Juno Beach, FL 33408 USA
[3] MacLean Power Syst, Franklin Pk, IL 60131 USA
关键词
clean fog flashover tests; FTIR analysis; hydrophobicity; mold growth; nonceramic insulators; surface resistance;
D O I
10.1109/TPWRD.2003.809681
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
This paper describes the identification of a common mold (i.e., fungus) growing on nonceramic insulators (NCIs) in service, and analyzes its impact on the electrical performance. The insulators evaluated were line posts removed from a 138-kV transmission line serving the interior (away from the coast) regions in Florida. The insulators had housings made from different types of silicone rubber (SR) and ethylene propylene rubber (EPR) polymer families. Electrical tests performed include surface resistance measurements and determination of contamination withstand capability (CWC) using the clean-fog procedure. Changes in the CWC were correlated to material changes by using micro-Fourier transform infrared (FTIR) analysis and surface resistance measurements. It was concluded that the mold growth is dependent on material formulation and outdoor environment. On SR insulators that exhibited mold growth, there was a reduction in the CWC when compared to the same insulator without the mold; however, even the reduced level of CWC was superior to that obtained on similarly rated EPR and porcelain insulators without any visible mold growth. Lastly, simple methods to remove the mold from the insulators are listed.
引用
收藏
页码:559 / 563
页数:5
相关论文
共 8 条
[1]   Electrical performance of non-ceramic insulators in artificial contamination tests - Role of resting time [J].
delaO, A ;
Gorur, RS ;
Burnham, JT .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 1996, 3 (06) :827-835
[2]   AC CLEAN FOG TESTS ON NON-CERAMIC INSULATING MATERIALS AND A COMPARISON WITH PORCELAIN [J].
DELAO, A ;
GORUR, RS ;
CHANG, J .
IEEE TRANSACTIONS ON POWER DELIVERY, 1994, 9 (04) :2000-2008
[3]   Field and laboratory aging of polymeric distribution cable terminations: Part 1 - Field aging [J].
Gorur, RS ;
Bernstein, BS .
IEEE TRANSACTIONS ON POWER DELIVERY, 1998, 13 (02) :316-322
[4]  
HEATHERINGTON W, 1997, P S MOD INS TECHN, P243
[5]   MECHANISM OF HVDC WALL BUSHING FLASHOVER IN NONUNIFORM RAIN [J].
SCHNEIDER, HM ;
LUX, AE .
IEEE TRANSACTIONS ON POWER DELIVERY, 1991, 6 (01) :448-455
[6]  
*STRI, 1992, 921 STRI
[7]  
1995, IEEE GUIDE CLEANING
[8]  
1975, ARTIFICIAL POLLUTION