Utilization of pine (Pinus pinea L.) cone in manufacture of wood based composite

被引:91
作者
Ayrilmis, Nadir [1 ]
Buyuksari, Umit [1 ]
Avci, Erkan [1 ]
Koc, Enus [2 ]
机构
[1] Istanbul Univ, Fac Forestry, Dept Wood Mech & Technol, TR-34473 Istanbul, Turkey
[2] Kastamonu Integrated Wood Co, Organize Sanayi Bolgesi, Kastamonu, Turkey
关键词
Formaldehyde emission; Medium density fiberboard; Pine cone; Raw material; Wood composite; GEL TIME; PARTICLEBOARD; EXTRACTIVES; PINASTER; DENSITY; FIBER;
D O I
10.1016/j.foreco.2009.09.043
中图分类号
S7 [林业];
学科分类号
0829 ; 0907 ;
摘要
Physical and mechanical properties of medium density fiberboards (MDF) made from various mixtures of wood fibers and stone pine (Pinus pinea L) cones were evaluated using European standards. MDF panels were manufactured using standardized procedures that simulated industrial production at the laboratory. Six panel types were made from mixtures of wood fiber/cone flour, 100/0, 90/10, 80/20, 701 30, 60/40, and 50/50 percents, respectively. Addition of the cone flour into the MDF significantly reduced formaldehyde emission from the panel. In addition, the addition of 10% cone flour also improved water resistance of the MDF panels made using urea-formaldehyde (UF) resin. However, further addition of the cone flour into the panel negatively influenced their water resistance. Flexural properties and internal bond strength decreased with the increase of cone flour content in the panel. The UF resin is the main source of formaldehyde emission from the UF-bonded wood-based panels. Depending on addition of the cone flour in the panels, the formaldehyde emission values ranged from 2.6% to 55.3% lower than the panels made from 100% wood fiber. Based on the findings obtained from this study, pine cone can be used as a renewable biological formaldehyde catcher as an alternative to the traditional formaldehyde catchers for El Class MDF manufacture. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:65 / 70
页数:6
相关论文
共 35 条
  • [1] Akgul Mehmet, 2007, Pak J Biol Sci, V10, P607, DOI 10.3923/pjbs.2007.607.611
  • [2] ALBRITTON RO, 1979, FOREST PROD J, V29, P40
  • [3] [Anonymous], 1999, WOOD HDB WOOD ENG MA
  • [4] AYRILMIS N, 2009, HOLZ ALS ROH UND WER, V67, P287
  • [5] Effect of panel density on dimensional stability of medium and high density fiberboards
    Ayrilmis, Nadir
    [J]. JOURNAL OF MATERIALS SCIENCE, 2007, 42 (20) : 8551 - 8557
  • [6] Effects of Post Heat-Treatment on Surface Characteristics and Adhesive Bonding Performance of Medium Density Fiberboard
    Ayrilmis, Nadir
    Winandy, Jerrold E.
    [J]. MATERIALS AND MANUFACTURING PROCESSES, 2009, 24 (05) : 594 - 599
  • [7] Bekhta P, 2002, FOREST PROD J, V52, P72
  • [8] Incorporation of hazelnut shell and husk in MDF production
    Coepuer, Yalcin
    Gueler, Cengiz
    Tascioglu, Cihat
    Tozluoglu, Ayhan
    [J]. BIORESOURCE TECHNOLOGY, 2008, 99 (15) : 7402 - 7406
  • [9] DUNKY M, 1998, P 2 PAN PROD S LLAND
  • [10] *EUR COMM STAND, 1993, 120 EN EUR COMM STAN