Nanomechanical and Fluorescence Characterizations of Weathered PV Module Encapsulation

被引:3
|
作者
Kim, Jae Hyun [1 ]
Lyu, Yadong [1 ]
Fairbrother, Andrew [1 ]
Miller, David C. [2 ]
Kempe, Michael D. [2 ]
Koehl, Michael [3 ]
Gu, Xiaohong [1 ]
机构
[1] NIST, Engn Lab, Gaithersburg, MD 20899 USA
[2] Natl Renewable Energy Lab, Photovolta Res, Golden, CO 80401 USA
[3] Inst Solar Energy Syst ISE, D-79110 Freiburg, Germany
来源
IEEE JOURNAL OF PHOTOVOLTAICS | 2021年 / 11卷 / 03期
关键词
Glass; Degradation; Additives; Temperature measurement; Silicon compounds; Silicon; Radiation effects; Accelerated aging; characterization; encapsulation; fluorescence; modulus; photovoltaic; SOLAR-CELLS; DEGRADATION; PERFORMANCE; OXIDATION; EVA;
D O I
10.1109/JPHOTOV.2021.3053657
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Nanoindentation and fluorescence spectroscopy provide spatially resolved mechanical and chemical characterization for degradation of poly (ethylene-co-vinyl acetate) (EVA) encapsulants aged under accelerated weathering and in field deployed photovoltaic (PV) modules. For the accelerated weathering tests, two different EVA formulations in the glass/EVA/glass-laminated coupons were exposed to ultraviolet (UV) light for 180 days at three different temperatures (40, 60, and 80 degrees C) and UV intensities (0.4, 2.2, and 2.9 W/m(2)/nm at 340 nm). The fluorescence spectra and moduli were uniform through the cross section of both EVA formulations at the lowest temperature and UV intensity; however, under the highest temperature and UV intensity, the UV irradiated sides showed lower moduli and higher fluorescence compared to the opposite sides. For EVA obtained from PV modules deployed 27 years in Sacramento, CA, USA, changes in fluorescence intensity across the thickness were relatively greater than changes in modulus. On the other hand, for EVA obtained from the same type of module stored in the shed for 27 years, no fluorescence was observed, and a uniform modulus was seen through the EVA layer, but with substantially higher values than those obtained from the field-deployed modules. The different extent of changes between laboratory and field exposures suggests the importance of considering effects of temperature and UV intensity for designing a reliable accelerated testing. This study uniquely demonstrates the capability of microscale characterization using nanoindentation and fluorescence microscopy to monitor mechanical and chemical degradation of EVA encapsulants in PV modules.
引用
收藏
页码:725 / 730
页数:6
相关论文
共 50 条
  • [1] Image Analysis of PV Module Electroluminescence
    Lai, T.
    Ramirez, C.
    Potter, B. G., Jr.
    Simmons-Potter, K.
    RELIABILITY OF PHOTOVOLTAIC CELLS, MODULES, COMPONENTS, AND SYSTEMS X, 2017, 10370
  • [2] Influence of Lamination Conditions of EVA Encapsulation on Photovoltaic Module Durability
    Wu, Dan
    Wessel, Patrick
    Zhu, Jiang
    Montiel-Chicharro, Daniel
    Betts, Thomas R.
    Mordvinkin, Anton
    Gottschalg, Ralph
    MATERIALS, 2023, 16 (21)
  • [3] The impact on the performance of a PV module as a result of the encapsulant fluorescence induced by weathering
    Hamzavy, Babak T.
    2018 IEEE 7TH WORLD CONFERENCE ON PHOTOVOLTAIC ENERGY CONVERSION (WCPEC) (A JOINT CONFERENCE OF 45TH IEEE PVSC, 28TH PVSEC & 34TH EU PVSEC), 2018, : 3251 - 3256
  • [4] Encapsulation of PV Modules Using Ethylene Vinyl Acetate Copolymer as the Encapsulant
    Jiang, Shan
    Wang, Kemin
    Zhang, Hongwen
    Ding, Yonghong
    Yu, Qiang
    MACROMOLECULAR REACTION ENGINEERING, 2015, 9 (05) : 522 - 529
  • [5] Quantification of PV Module Discoloration using Visual Image Analysis
    Chattopadhyay, Shashwata
    Solanki, Chetan Singh
    Kottantharayil, Anil
    Narasimhan, K. L.
    Vasi, Juzer
    Tatapudi, Sai
    TamizhMani, Govindasamy
    2017 IEEE 44TH PHOTOVOLTAIC SPECIALIST CONFERENCE (PVSC), 2017, : 1850 - 1854
  • [6] A Novel Hot Spot Mitigation Circuit for Improved Reliability of PV Module
    Ghosh, Santosh
    Yadav, Vinod K.
    Mukherjee, Vivekananda
    IEEE TRANSACTIONS ON DEVICE AND MATERIALS RELIABILITY, 2020, 20 (01) : 191 - 198
  • [7] Optimal Model Selection For PV Module Modeling
    Mahammed, I. Hadj
    Bakelli, Y.
    Oudjana, S. Hamid
    Arab, A. Hadj
    Berrah, S.
    2012 24TH INTERNATIONAL CONFERENCE ON MICROELECTRONICS (ICM), 2012,
  • [8] UV LED ageing of polymers for PV cell encapsulation
    Pinochet, Nicolas
    Pirot-Berson, Lucie
    Couderc, Romain
    Therias, Sandrine
    NPJ MATERIALS DEGRADATION, 2024, 8 (01)
  • [9] Impact of hailstorm on the performance of PV module: a review
    Gupta, Vinay
    Sharma, Madhu
    Pachauri, Rupendra
    Babu, K. N. Dinesh
    ENERGY SOURCES PART A-RECOVERY UTILIZATION AND ENVIRONMENTAL EFFECTS, 2022, 44 (01) : 1923 - 1944
  • [10] In-Field Energy Performance of Solar PV Module Made of UMG Silicon
    Roberto Guerra, Moises
    de la Parra Laita, Inigo
    Garcia Solano, Miguel
    Pascual, Julio
    IEEE JOURNAL OF PHOTOVOLTAICS, 2022, 12 (05): : 1109 - 1115