Enhanced Kinetic Stability of Pure and Y-Doped Tetragonal ZrO2

被引:35
作者
Kogler, Michaela [1 ]
Koeck, Eva-Maria [1 ]
Vanicek, Stefan [2 ]
Schmidmair, Daniela [3 ]
Goetsch, Thomas [1 ]
Stoeger-Pollach, Michael [4 ]
Hejny, Clivia [3 ]
Kloetzer, Bernhard [1 ]
Penner, Simon [1 ]
机构
[1] Univ Innsbruck, Inst Phys Chem, A-6020 Innsbruck, Austria
[2] Univ Innsbruck, Inst Inorgan & Theoret Chem, A-6020 Innsbruck, Austria
[3] Univ Innsbruck, Inst Mineral & Petrog, A-6020 Innsbruck, Austria
[4] Vienna Univ Technol, Univ Serv Ctr Transmiss Electron Microscopy USTEM, A-1040 Vienna, Austria
关键词
MONOCLINIC PHASE-TRANSFORMATION; THERMAL-DECOMPOSITION; ZIRCONIUM ALKOXIDES; CUBIC PHASE; CRYSTALLIZATION; SURFACE; FILMS; METASTABILITY; CALCINATION; TRANSITION;
D O I
10.1021/ic502623t
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
The kinetic stability of pure and yttrium-doped tetragonal zirconia (ZrO2) polymorphs prepared via a pathway involving decomposition of pure zirconium and zirconium + yttrium isopropoxide is reported. Following this preparation routine, high surface area, pure, and structurally stable polymorphic modifications of pure and Y-doped tetragonal zirconia are obtained in a fast and reproducible way. Combined analytical high-resolution in situ transmission electron microscopy, high-temperature X-ray diffraction, and chemical and thermogravimetric analyses reveals that the thermal stability of the pure tetragonal ZrO2 structure is very much dominated by kinetic effects. Tetragonal ZrO2 crystallizes at 400 degrees C from an amorphous ZrO2 precursor state and persists in the further substantial transformation into the thermodynamically more stable monoclinic modification at higher temperatures at fast heating rates. Lower heating rates favor the formation of an increasing amount of monoclinic phase in the product mixture, especially in the temperature region near 600 degrees C and during/after recooling. If the heat treatment is restricted to 400 degrees C even under moist conditions, the tetragonal phase is permanently stable, regardless of the heating or cooling rate and, as such, can be used as pure catalyst support. In contrast, the corresponding Y-doped tetragonal ZrO2 phase retains its structure independent of the heating or cooling rate or reaction environment. Pure tetragonal ZrO2 can now be obtained in a structurally stable form, allowing its structural, chemical, or catalytic characterization without in-parallel triggering of unwanted phase transformations, at least if the annealing or reaction temperature is restricted to T = 400 degrees C.
引用
收藏
页码:13247 / 13257
页数:11
相关论文
共 53 条
[11]  
DAVIS BH, 1984, J AM CERAM SOC, V67, pC168
[12]   Stabilization of tetragonal ZrO2 in ZrO2-SiO2 binary oxides [J].
del Monte, F ;
Larsen, W ;
Mackenzie, JD .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (03) :628-634
[13]   STRUCTURAL DISORDER AND PHASE-TRANSITIONS IN ZRO2-Y2O3 SYSTEM [J].
FEINBERG, A ;
PERRY, CH .
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1981, 42 (06) :513-518
[14]  
Garnweitner G., 2007, NANOTECHNOLOGIES LIF
[15]   OCCURRENCE OF METASTABLE TETRAGONAL ZIRCONIA AS A CRYSTALLITE SIZE EFFECT [J].
GARVIE, RC .
JOURNAL OF PHYSICAL CHEMISTRY, 1965, 69 (04) :1238-&
[16]   Nanocrystalline zirconia-yttria system - a Raman study [J].
Ghosh, A ;
Suri, AK ;
Pandey, M ;
Thomas, S ;
Mohan, TRR ;
Rao, BT .
MATERIALS LETTERS, 2006, 60 (9-10) :1170-1173
[17]   Surface Science Studies on the Zirconia-Based Model Catalysts [J].
Han, Yong ;
Zhu, Junfa .
TOPICS IN CATALYSIS, 2013, 56 (15-17) :1525-1541
[18]  
Herd W., 1989, LANGMUIR, V5, P96
[19]   NOVEL SYNTHETIC METHOD FOR THE CATALYTIC USE OF THERMALLY STABLE ZIRCONIA - THERMAL-DECOMPOSITION OF ZIRCONIUM ALKOXIDES IN ORGANIC MEDIA [J].
INOUE, M ;
KOMINAMI, H ;
INUI, T .
APPLIED CATALYSIS A-GENERAL, 1993, 97 (02) :L25-L30
[20]  
INOUE M, 1995, APPL CATAL A-GEN, V121, pL1, DOI 10.1016/0926-860X(94)00226-6