Effect of different firing atmospheres on debonding strength of dental porcelain fused to commercially pure titanium

被引:0
作者
Wang, Jen-Chyan [1 ,2 ,5 ]
Fu, Po-Sung [1 ,3 ]
Lai, Pei-Ling [2 ]
Liu, Chen-Shih [1 ]
Chen, Wen-Cheng [4 ,5 ]
Hung, Chun-Cheng [1 ,2 ,5 ]
机构
[1] Kaohsiung Med Univ, Sch Dent, Coll Dent Med, 100,Shih Chuan 1st Rd, Kaohsiung 80756, Taiwan
[2] Kaohsiung Med Univ Hosp, Div Prosthodont, Dept Dent, Kaohsiung, Taiwan
[3] Kaohsiung Municipal Tatung Hosp, Dept Dent, Kaohsiung, Taiwan
[4] Feng Chia Univ, Adv Med Devices & Composites Lab, Dept Fiber & Composite Mat, Coll Engn, Taichung, Taiwan
[5] Kaohsiung Med Univ, Dent Med Devices & Mat Res Ctr, Coll Dent Med, Kaohsiung, Taiwan
关键词
bending; bonding strength; commercially pure titanium (cp Ti); noble gases; porcelain fused to metal (PFM); LOW-FUSING PORCELAIN; ALPHA-CASE FORMATION; MECHANICAL-PROPERTIES; BOND STRENGTH; ALLOY; OXIDATION; COATINGS; POROSITY; CAST; SIO2;
D O I
10.1002/kjm2.12157
中图分类号
R-3 [医学研究方法]; R3 [基础医学];
学科分类号
1001 ;
摘要
An in vitro investigation was performed to evaluate the bonding characteristics of porcelain fused to metal (PFM)/commercially pure titanium (cp Ti, grade II) in three firing atmospheres of under vacuum and using two noble gases argon (Ar) and helium (He). Three groups of porcelain veneers firing under vacuum, Ar, and He were prepared to evaluate the bonding of porcelain fused to the cold-rolled cp Ti. The bond strength of PFM durability by a three-point bending test, phases, microhardness of cp Ti after firing processes, and fractures were measured and evaluated. Results show the microhardness of cp Ti in group of porcelain firing under He atmosphere was significantly lower than that of the two other groups, which were in vacuum and Ar (P < .05). X-ray diffraction showed the He group produced in relatively small amounts of TiO2 and TiO oxides than other groups but featured relatively high quantity of airhole defects in the porcelain body leading to the lowest bond strength. The Ar group presented the highest bond strength of comparing with the groups under vacuum and using He (P < .05). Although the firing processes in He could efficiently prevent the diffusion of oxygen into Ti, the porcelain-cp Ti bond strength using Ar protective atmosphere presented the advantage to achieve clinical requirement because porcelain firing under He revealed prominent voids and defects within the body of porcelain.
引用
收藏
页码:212 / 219
页数:8
相关论文
共 50 条
[41]   The effect of ZrSiN diffusion barrier on the bonding strength of titanium porcelain [J].
Zhang, H. ;
Guo, T. W. ;
Song, Z. X. ;
Wang, X. J. ;
Xu, K. W. .
SURFACE & COATINGS TECHNOLOGY, 2007, 201 (9-11) :5637-5640
[42]   Effect of SnO coatings on the bond strength between titanium and porcelain [J].
Liu, Xiaochen ;
Guo, Litong ;
Gao, Jiqiang ;
Guo, Tianwen ;
Liu, Li ;
Li, Shibao ;
Li, Xiaona .
HIGH-PERFORMANCE CERAMICS V, PTS 1 AND 2, 2008, 368-372 :1268-+
[43]   Effect of plasma nitriding treatment on structural, tribological and electrochemical properties of commercially pure titanium [J].
Celik, Ilhan ;
Karakan, Mehmet .
PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART H-JOURNAL OF ENGINEERING IN MEDICINE, 2016, 230 (02) :145-152
[44]   Effects of different electrolytes for micro-arc oxidation on the bond strength between titanium and porcelain [J].
Yuan, Xiaohui ;
Tan, Fei ;
Xu, Haitao ;
Zhang, Shaojun ;
Qu, Fuzhen ;
Liu, Jie .
JOURNAL OF PROSTHODONTIC RESEARCH, 2017, 61 (03) :297-304
[45]   Improvements in the static/dynamic strength of porcelain fused to metal dental crowns with surface protrusions produced by selective laser melting [J].
Taftali, Merve ;
Turalioglu, Kerem ;
Yetim, A. Fatih ;
Uzun, Yakup ;
Akpinar, Salih ;
Yildiz, Fatih .
JOURNAL OF MANUFACTURING PROCESSES, 2021, 65 :112-118
[46]   Effect of Temperature on Anisotropic Behavior and Springback of Commercially Pure Titanium Foil [J].
Modanloo, Vahid .
Journal of Bio- and Tribo-Corrosion, 2024, 10 (04)
[47]   Effect of ARB Processing on Fatigue Crack Closure in Commercially Pure Titanium [J].
Kitahara, Hiromoto ;
Matsushita, Sho ;
Tsushida, Masayuki ;
Ando, Shinji .
MATERIALS TRANSACTIONS, 2013, 54 (04) :528-531
[48]   Ballistic impact behavior of commercially pure titanium with gradient nanostructure against projectiles with different nose shapes [J].
Guo, Yansong ;
Ge, Yanxin ;
Deng, Lisha ;
Wang, Chenguang ;
Zhou, Changqing ;
Gao, Tianze ;
Bataev, Ivan A. ;
Fan, Hang ;
Zhou, Qiang ;
Chen, Pengwan ;
Jia, Bin .
INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 2025, 202
[49]   Effect of electrochemical parameters on the formation of anodic films on commercially pure titanium by plasma electrolytic oxidation [J].
Quintero, D. ;
Galvis, O. ;
Calderon, J. A. ;
Castano, J. G. ;
Echeverria, F. .
SURFACE & COATINGS TECHNOLOGY, 2014, 258 :1223-1231
[50]   Improved Commercially Pure Titanium Obtained by Laser Directed Energy Deposition for Dental Prosthetic Applications [J].
Barro, Oscar ;
Arias-Gonzalez, Felipe ;
Lusquinos, Fernando ;
Comesana, Rafael ;
del Val, Jesus ;
Riveiro, Antonio ;
Badaoui, Aida ;
Gomez-Bano, Felix ;
Pou, Juan .
METALS, 2021, 11 (01) :1-15