Effect of different firing atmospheres on debonding strength of dental porcelain fused to commercially pure titanium

被引:0
作者
Wang, Jen-Chyan [1 ,2 ,5 ]
Fu, Po-Sung [1 ,3 ]
Lai, Pei-Ling [2 ]
Liu, Chen-Shih [1 ]
Chen, Wen-Cheng [4 ,5 ]
Hung, Chun-Cheng [1 ,2 ,5 ]
机构
[1] Kaohsiung Med Univ, Sch Dent, Coll Dent Med, 100,Shih Chuan 1st Rd, Kaohsiung 80756, Taiwan
[2] Kaohsiung Med Univ Hosp, Div Prosthodont, Dept Dent, Kaohsiung, Taiwan
[3] Kaohsiung Municipal Tatung Hosp, Dept Dent, Kaohsiung, Taiwan
[4] Feng Chia Univ, Adv Med Devices & Composites Lab, Dept Fiber & Composite Mat, Coll Engn, Taichung, Taiwan
[5] Kaohsiung Med Univ, Dent Med Devices & Mat Res Ctr, Coll Dent Med, Kaohsiung, Taiwan
关键词
bending; bonding strength; commercially pure titanium (cp Ti); noble gases; porcelain fused to metal (PFM); LOW-FUSING PORCELAIN; ALPHA-CASE FORMATION; MECHANICAL-PROPERTIES; BOND STRENGTH; ALLOY; OXIDATION; COATINGS; POROSITY; CAST; SIO2;
D O I
10.1002/kjm2.12157
中图分类号
R-3 [医学研究方法]; R3 [基础医学];
学科分类号
1001 ;
摘要
An in vitro investigation was performed to evaluate the bonding characteristics of porcelain fused to metal (PFM)/commercially pure titanium (cp Ti, grade II) in three firing atmospheres of under vacuum and using two noble gases argon (Ar) and helium (He). Three groups of porcelain veneers firing under vacuum, Ar, and He were prepared to evaluate the bonding of porcelain fused to the cold-rolled cp Ti. The bond strength of PFM durability by a three-point bending test, phases, microhardness of cp Ti after firing processes, and fractures were measured and evaluated. Results show the microhardness of cp Ti in group of porcelain firing under He atmosphere was significantly lower than that of the two other groups, which were in vacuum and Ar (P < .05). X-ray diffraction showed the He group produced in relatively small amounts of TiO2 and TiO oxides than other groups but featured relatively high quantity of airhole defects in the porcelain body leading to the lowest bond strength. The Ar group presented the highest bond strength of comparing with the groups under vacuum and using He (P < .05). Although the firing processes in He could efficiently prevent the diffusion of oxygen into Ti, the porcelain-cp Ti bond strength using Ar protective atmosphere presented the advantage to achieve clinical requirement because porcelain firing under He revealed prominent voids and defects within the body of porcelain.
引用
收藏
页码:212 / 219
页数:8
相关论文
共 50 条
  • [1] Effect of silica coating on the bond strength of milled pure titanium to dental porcelain
    Ye, Jiantao
    Ye, Xiuhua
    Chang, Shaohai
    Liu, Lang
    Zhang, Yiping
    Lin, Shiyao
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2016, 124 (05) : 498 - 503
  • [2] Effects of nitrogen implantation on the bonding strength of porcelain fused to pure titanium
    Xie, Weili
    Zhong, Zhaowei
    Li, Changcheng
    Wen, Guangwu
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 2261 - +
  • [3] Effect of different production techniques on the color of porcelain-fused-to-titanium restorations
    Korkmaz, Cumhur
    HELIYON, 2024, 10 (03)
  • [4] Gold and titanium nitride coatings on cast and machined commercially pure titanium to improve titanium-porcelain adhesion
    Park, Sangwon
    Kim, Yeonmi
    Lim, Hyunpil
    Oh, Gyejeong
    Kim, Hyunseung
    Ong, Joo L.
    Lee, Kwangmin
    SURFACE & COATINGS TECHNOLOGY, 2009, 203 (20-21) : 3243 - 3249
  • [5] Effect of Different Firing Temperatures on Structural Changes in Porcelain
    Tripathi, Arvind
    Bagchi, Soumyojeet
    Singh, Juhi
    Gaurav, Vivek
    Singh, Mahendra Pal
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2018, 27 (03): : 290 - 298
  • [6] EFFECT OF A MAGNETRON-SPUTTERED ZRSIN/ZRO2 FILM ON THE BOND STRENGTH OF COMMERCIALLY PURE TITANIUM TO PORCELAIN
    Wang, Guowei
    Wang, Xiaojing
    Zhao, Yimin
    Guo, Tianwen
    JOURNAL OF PROSTHETIC DENTISTRY, 2013, 109 (05) : 313 - 318
  • [7] The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminium-vanadium alloy
    Troia, MG
    Henriques, GEP
    Nóbilo, MAA
    Mesquita, MF
    DENTAL MATERIALS, 2003, 19 (08) : 790 - 796
  • [8] Effects of silica-coating on surface topography and bond strength of porcelain fused to CAD/CAM pure titanium
    Fukuyama, Takushi
    Hamano, Naho
    Ino, Satoshi
    DENTAL MATERIALS JOURNAL, 2016, 35 (02) : 325 - 332
  • [9] Influence of Sandblasting and Chemical Etching on Titanium 99.2-Dental Porcelain Bond Strength
    Lubas, Malgorzata
    Jasinski, Jaroslaw Jan
    Zawada, Anna
    Przerada, Iwona
    MATERIALS, 2022, 15 (01)
  • [10] Interfacial characterization of porcelain veneered on the pure titanium under vacuum firing
    Lo, TN
    Lui, TS
    Chang, E
    MATERIALS TRANSACTIONS, 2004, 45 (10) : 3065 - 3070