Microstructure and electrochemical corrosion behavior of selective laser melted Ti-6Al-4V alloy in simulated artificial saliva

被引:28
作者
Ju, Jiang [1 ,2 ]
Li, Jing-jing [1 ,2 ]
Jiang, Min [1 ]
Li, Meng-ya [3 ]
Yang, Li-xiang [1 ]
Wang, Kai-ming [4 ]
Yang, Chao [1 ,2 ]
Kang, Mao-dong [1 ,2 ]
Wang, Jun [1 ,2 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Inst Solidificat Sci & Technol, Shanghai 200240, Peoples R China
[2] Shanghai Jiao Tong Univ, Shanghai Key Lab Adv High Temp Mat & Precis Formi, Shanghai 200240, Peoples R China
[3] Beijing Inst Technol, Sch Aerosp Engn, Beijing 100081, Peoples R China
[4] Tsinghua Univ, Dept Mech Engn, State Key Lab Tribol, Beijing 100084, Peoples R China
基金
中国博士后科学基金; 国家重点研发计划; 中国国家自然科学基金;
关键词
Ti-6Al-4V alloy; selective laser melting; microstructure; electrochemical corrosion behavior;
D O I
10.1016/S1003-6326(20)65485-1
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Ti-6Al-4V alloy was fabricated via selective laser melting (SLM) to improve its corrosion resistance for implant. The microstructure and electrochemical corrosion behavior were investigated using scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM), electrochemical test and contact angle test. It can be found that the as-selective laser melted (as-SLMed) Ti-6Al-4V alloys show beta columnar microstructure in building direction and nearly circular checkerboard microstructure in scanning direction, while the wrought and wrought+HT samples exhibit equiaxed microstructure. The as-SLMed Ti-6Al-4V alloy exhibits better corrosion resistance than the wrought and wrought+HT samples due to hydrophobicity, high grain boundary density and uniform distribution of alloying elements in simulated artificial saliva at 37 degrees C.
引用
收藏
页码:167 / 177
页数:11
相关论文
共 50 条
  • [21] Microstructure change and corrosion resistance of selective laser melted Ti-6Al-4V alloy subjected to pneumatic shot peening and ultrasonic shot peening
    Zhang, Qi
    Xu, Shuo
    Wang, Jie
    Zhang, Xianjie
    Wang, Junbiao
    Si, Chaorun
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2022, 10 (01)
  • [22] Corrosion Behavior of Selective Laser Melted Ti-6Al-4V in 0.1 mol/L NaOH Solution
    Huang, Lei
    Zheng, Shunli
    Qin, Yue
    Han, Jianyang
    Qiao, Yanxin
    Chen, Jian
    COATINGS, 2023, 13 (01)
  • [23] Effect of crystallographic orientation on mechanical anisotropy of selective laser melted Ti-6Al-4V alloy
    Yang, Jingjing
    Yu, Hanchen
    Wang, Zemin
    Zeng, Xiaoyan
    MATERIALS CHARACTERIZATION, 2017, 127 : 137 - 145
  • [24] Effects of electropulsing on the microstructure and microhardness of a selective laser melted Ti6Al4V alloy
    Gao, J. B.
    Ben, D. D.
    Yang, H. J.
    Meng, L. X.
    Ji, H. B.
    Lian, D. L.
    Chen, J.
    Yi, J. L.
    Wang, L.
    Li, P.
    Zhang, Z. F.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 875
  • [25] On the Texture Formation of Selective Laser Melted Ti-6Al-4V
    Simonelli, Marco
    Tse, Yau Yau
    Tuck, Chris
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (06): : 2863 - 2872
  • [26] Dynamic evolution of oxide film on selective laser melted Ti-6Al-4V alloy
    Zhang, Yifei
    Li, Jianzhong
    Xu, Haoyuan
    Feng, Limin
    Zhang, Tao
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 849
  • [27] Differences in electrochemical corrosion behaviours between selective laser melted and wrought Ti6Al4V alloys in acid fluoride-containing artificial saliva
    Guan, Lei
    Yang, Xiangyu
    Li, Yu
    Shi, Changliang
    Yan, Dejun
    Huang, Jiayong
    Zhang, Lai-Chang
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2021, 51 (11) : 1619 - 1633
  • [28] Temperature sensitivity of mechanical properties and microstructure during moderate temperature deformation of selective laser melted Ti-6Al-4V alloy
    Song, Jingwen
    Han, Yuanfei
    Fang, Minhan
    Hu, Fuguo
    Ke, Linda
    Li, Ying
    Lei, Liming
    Lu, Weijie
    MATERIALS CHARACTERIZATION, 2020, 165
  • [29] Influence of substructures on the selective laser melted Ti-6Al-4V alloy as a function of laser re-melting
    Karimi, J.
    Xie, M. S.
    Wang, Z.
    Prashanth, K. G.
    JOURNAL OF MANUFACTURING PROCESSES, 2021, 68 : 1387 - 1394
  • [30] Comparison on mechanical anisotropies of selective laser melted Ti-6Al-4V alloy and 304 stainless steel
    Yu, Hanchen
    Yang, Jingjing
    Yin, Jie
    Wang, Zemin
    Zeng, Xiaoyan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 695 : 92 - 100