The effect of powder pre-treatment on the mechanical and thermoelectric properties of spark plasma sintered N-type bismuth telluride

被引:5
|
作者
Abdelnabi, Ahmed A. [1 ]
Lakhian, Vickram [1 ]
McDermid, Joseph R. [2 ]
Cotton, James S. [1 ]
机构
[1] McMaster Univ, Dept Mech Engn, Hamilton, ON, Canada
[2] McMaster Univ, Dept Mat Sci & Engn, Hamilton, ON, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Thermoelectric materials; Mechanical properties; Uniaxial tensile strength; (Bi-0.95 Sb-0.05)(2)(Se-0.05 Te-0.95)(3); Powder pre-treatment; Spark plasma sintering (SPS); THERMAL-STRESS ANALYSIS; ELECTRICAL-PROPERTIES; BI2TE3; PERFORMANCE; GENERATOR; ALLOYS;
D O I
10.1016/j.jallcom.2021.159782
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effect of N-type (Bi-0.95 Sb-0.05)(2)(Se-0.05 Te-0.95)(3) powder pre-treatments, including annealing and powder oxide reduction, was determined in terms of both the mechanical and thermoelectric properties for bodies fabricated using spark plasma sintering (SPS). The uniaxial tensile strength was measured and the figure of merit "ZT" was calculated both parallel and perpendicular to the sintering pressure direction. The powder oxide reduction pre-treatment was carried out using 5% H-2 center dot 95% Ar (vol%) in an in-house built mechanically agitated fluidized bed reduction facility at 380 degrees C for 24 h, while annealing was carried out at the same temperature and holding time using high purity Ar. Both pre-treatments were compared to the as manufactured baseline powder sample that was dried under vacuum for 24 h. It was determined that the oxide content decreased from 0.362 to 0.143 wt% after H-2 reduction, while it decreased to 0.341 wt% after annealing. The increase in the mechanical properties was found to be mainly due to the annealing pretreatment, which resulted in an increased relative density of the sintered samples from 97.0% to 98.0%. The annealing pre-treatment increased the characteristic uniaxial tensile strength from 30.4 to 34.1 MPa in the parallel direction and from 30.8 to 38.0 MPa in the perpendicular direction. The increase in the ZT is attributed to the increase in the Seebeck coefficient, which is in turn due to a decrease in the carrier concentration, as was found by examining the literature. The ZT(max) (150 degrees C) increased from 0.54 to 0.63 versus the dried powder in both the parallel and perpendicular directions due to powder oxide reduction and 0.58 and 0.62 in the parallel and the perpendicular directions, respectively, due to annealing versus the dried powder. (c) 2021 Elsevier B.V. All rights reserved.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] High performance n-type bismuth telluride with highly stable thermoelectric figure of merit
    Yamashita, O
    Tomiyoshi, S
    JOURNAL OF APPLIED PHYSICS, 2004, 95 (11) : 6277 - 6283
  • [42] Thermoelectric properties of p-type bismuth telluride material fabricated by plasma sintering of metal powder mixture
    Tokiai, T
    Uesugi, T
    Etoh, Y
    Tamura, S
    Yoneyama, Y
    Koumoto, K
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1996, 104 (09) : 837 - 843
  • [43] N-Type Bismuth Telluride Nanocomposite Materials Optimization for Thermoelectric Generators in Wearable Applications
    Nozariasbmarz, Amin
    Krasinski, Jerzy S.
    Vashaee, Daryoosh
    MATERIALS, 2019, 12 (09)
  • [44] Thermoelectric properties of n-type bismuth telluride based alloys prepared by hot pressing and zone melting method
    Ha, HP
    Kim, TH
    Hyun, DB
    Yoon, EP
    PROCEEDINGS OF THE FOURTH INTERNATIONAL CONFERENCE ON MATERIALS ENGINEERING FOR RESOURCES, VOL 1, 2001, : 238 - 239
  • [45] Thermoelectric properties of n-type nanocrystalline bismuth-telluride-based thin films deposited by flash evaporation
    Takashiri, M.
    Takiishi, M.
    Tanaka, S.
    Miyazaki, K.
    Tsukamoto, H.
    JOURNAL OF APPLIED PHYSICS, 2007, 101 (07)
  • [46] Mechanical properties and microstructure of spark plasma sintered nanostructured p-type SiGe thermoelectric alloys
    Bathula, Sivaiah
    Jayasimhadri, M.
    Dhar, Ajay
    MATERIALS & DESIGN, 2015, 87 : 414 - 420
  • [47] Enhanced thermoelectric properties of bismuth telluride bulk achieved by telluride-spilling during the spark plasma sintering process
    Ge, Zhen-Hua
    Ji, Yi-Hong
    Qiu, Yang
    Chong, Xiaoyu
    Feng, Jing
    He, Jiaqing
    SCRIPTA MATERIALIA, 2018, 143 : 90 - 93
  • [48] Effect of Heat Treatment on the Thermoelectric Properties of Bismuth-Antimony-Telluride Prepared by Mechanical Deformation and Mechanical Alloying
    Lee, Deuk-Hee
    Lee, Jae-Uk
    Jung, Sung-Jin
    Baek, Seung-Hyub
    Kim, Ju-Heon
    Kim, Dong-Ik
    Hyun, Dow-Bin
    Kim, Jin-Sang
    JOURNAL OF ELECTRONIC MATERIALS, 2014, 43 (06) : 2255 - 2261
  • [49] Control of p-type and n-type thermoelectric properties of bismuth telluride thin films by combinatorial sputter coating technology
    Goto, Masahiro
    Sasaki, Michiko
    Xu, Yibin
    Zhan, Tianzhuo
    Isoda, Yukihiro
    Shinohara, Yoshikazu
    APPLIED SURFACE SCIENCE, 2017, 407 : 405 - 411
  • [50] Study on microstructure and mechanical properties of spark plasma sintered Alumix 431 powder
    Garbiec, D.
    Siwak, P.
    POWDER METALLURGY, 2016, 59 (04) : 242 - 248