Inorganic electrolyte additives to suppress the degradation of graphite anodes by dissolved Mn(II) for lithium-ion batteries

被引:101
作者
Komaba, S [1 ]
Kaplan, B
Ohtsuka, T
Kataoka, Y
Kumagai, N
Groult, H
机构
[1] Iwate Univ, Dept Chem Engn, Morioka, Iwate 0208551, Japan
[2] Univ Paris 06, CNRS, UMR 7612, LI2C Lab, F-75252 Paris 05, France
关键词
lithium-ion battery; graphite; LiMn2O4; Mn dissolution; additive; SEI;
D O I
10.1016/S0378-7753(03)00224-6
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
It is well known that when the carbon/LiMn2O4-based cathode battery was operated at elevated temperatures, the severe capacity loss occurred in following cycles. As we recently described, the capacity loss is mainly due to the degradation on the carbon anode side caused by the deposition of manganese at the carbon followed by the irreversible decomposition at the graphite/deposited Mn/electrolyte interface. It was found that inorganic additives in electrolyte, such as LiI, LiBr, and NH4I effectively suppressed the degradation of graphite anode to improve the battery performance. In case of LiI and LiBr, the irreversible reaction at the Mn/electrolyte interface was suppressed by specific adsorption of iodide or bromide anions on the metallic Mn surface. Further, the reduction of Mn(II) would be suppressed by adding NH4I into electrolyte which could be due to the formation of a stable amine complex of Mn(II). (C) 2003 Elsevier Science B.V All rights reserved.
引用
收藏
页码:378 / 382
页数:5
相关论文
共 21 条
  • [1] Materials' effects on the elevated and room temperature performance of C/LiMn2O4 Li-ion batteries
    Amatucci, GG
    Schmutz, CN
    Blyr, A
    Sigala, C
    Gozdz, AS
    Larcher, D
    Tarascon, JM
    [J]. JOURNAL OF POWER SOURCES, 1997, 69 (1-2) : 11 - 25
  • [2] BIOENSAN P, 2000, P 10 INT M LITH BATT
  • [3] Mechanism for limited 55°C storage performance of Li1.05Mn1.95O4 electrodes
    Du Pasquier, A
    Blyr, A
    Courjal, P
    Larcher, D
    Amatucci, G
    Gérand, B
    Tarascon, JM
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (02) : 428 - 436
  • [4] IN-SITU SCANNING VIBRATING ELECTRODE TECHNIQUE FOR THE CHARACTERIZATION OF INTERFACE BETWEEN LITHIUM ELECTRODE AND ELECTROLYTES CONTAINING ADDITIVES
    ISHIKAWA, M
    YOSHITAKE, S
    MORITA, M
    MATSUDA, Y
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1994, 141 (12) : L159 - L161
  • [5] Electrochemical control of a Li metal anode interface: improvement of Li cyclability by inorganic additives compatible with electrolytes
    Ishikawa, M
    Machino, S
    Morita, M
    [J]. JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1999, 473 (1-2) : 279 - 284
  • [6] Electrolyte effects on spinel dissolution and cathodic capacity losses in 4 v Li/LixMn2O4 rechargeable cells
    Jang, DH
    Oh, SM
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (10) : 3342 - 3348
  • [7] Influence of manganese(II), cobalt(II), and nickel(II) additives in electrolyte on performance of graphite anode for lithium-ion batteries
    Komaba, S
    Kumagai, N
    Kataoka, Y
    [J]. ELECTROCHIMICA ACTA, 2002, 47 (08) : 1229 - 1239
  • [8] Manganese dissolution from lithium doped Li-Mn-O spinel cathode materials into electrolyte solution
    Komaba, S
    Kumagai, N
    Sasaki, T
    Miki, Y
    [J]. ELECTROCHEMISTRY, 2001, 69 (10) : 784 - 787
  • [9] Electrochemical behavior of graphite electrode for lithium ion batteries in Mn and Co additive electrolytes
    Kumagai, N
    Komaba, S
    Kataoka, Y
    Koyanagi, M
    [J]. CHEMISTRY LETTERS, 2000, (10) : 1154 - 1155
  • [10] Enhanced structural stability and cyclability of Al-doped LiMn2O4 spinel synthesized by the emulsion drying method
    Myung, ST
    Komaba, S
    Kumagai, N
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (05) : A482 - A489