Switching "on'' and "off'' the adhesion in stimuli-responsive elastomers
被引:40
|作者:
Kaiser, S.
[1
]
Radl, S. V.
[1
]
Manhart, J.
[1
]
Ayalur-Karunakaran, S.
[1
]
Griesser, T.
[2
,3
]
Moser, A.
[4
]
Ganser, C.
[5
]
Teichert, C.
[5
]
Kern, W.
[1
,3
]
Schloegl, S.
[1
]
机构:
[1] Polymer Competence Ctr Leoben GmbH, Roseggerstr 12, A-8700 Leoben, Austria
[2] Christian Doppler Lab Funct & Polymer Based Ink J, Otto Glockel Str 2, A-8700 Leoben, Austria
[3] Univ Leoben, Chair Chem Polymer Mat, Otto Glockel Str 2, A-8700 Leoben, Austria
[4] Univ Leoben, Chair Mat Sci & Testing Plast, Otto Glockel Str 2, A-8700 Leoben, Austria
[5] Univ Leoben, Inst Phys, Franz Josef Str 18, A-8700 Leoben, Austria
来源:
关键词:
PRESSURE-SENSITIVE ADHESIVES;
PENDANT ANTHRACENE GROUPS;
GECKO FOOT-HAIR;
9-SUBSTITUTED ANTHRACENES;
POLYMERS;
SURFACES;
SYSTEMS;
FORCE;
PHOTOCYCLOADDITION;
PHOTODIMERIZATION;
D O I:
10.1039/c8sm00284c
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
The present work aims at the preparation of dry adhesives with switchable bonding properties by using the reversible nature of the [4 pi s+4 pi s] cycloaddition of anthracenes. Photo-responsive hydrogenated carboxylated nitrile butadiene rubber with photo-responsive pendant anthracene groups is prepared by one-pot synthesis. The formation of 3D networks relies on the photodimerization of the anthracene moieties upon UV exposure (lambda > 300 nm). Controlled cleavage of the crosslink sites is achieved by either deep UV exposure (lambda = 254 nm) or thermal dissociation at 70 degrees C. The kinetics of the optical and thermal cleavage routes are compared in thin films using UV-vis spectroscopy and their influence on the reversibility of the network is detailed. Going from thin films to free standing samples the modulation of the network structure and thermo-mechanical properties over repeated crosslinking and cleavage cycles are characterized by low-field NMR spectroscopy and dynamic mechanical analysis. The applicability of the stimuli-responsive networks as adhesives with reversible bonding properties is demonstrated. The results evidence that the reversibility of the crosslinking reaction enables a controlled switching "on'' and "off'' of adhesion properties. The recovery of the adhesion force amounts to 75 and 80% for photo- and thermal dissociation, respectively. Spatial control of adhesion properties is evidenced by adhesion force mapping experiments of photo-patterned films.
引用
收藏
页码:2547 / 2559
页数:13