A Comparative Study of Laser Irradiation Versus Sandblasting in Improving the Bond Strength of Titanium Abutments

被引:5
作者
Ustun, Ozlem [1 ]
Akar, Turker [2 ]
Kirmali, Omer [1 ]
机构
[1] Akdeniz Univ, Fac Dent, Dept Prosthodont, TR-07058 Antalya, Turkey
[2] Erzincan Univ, Fac Dent, Dept Prosthodont, Erzincan, Turkey
关键词
titanium abutment; surface treatment; Er; Cr:YSGG laser; tensile bond strength; resin cement; EDS; SEM; RETAINED IMPLANT RESTORATIONS; DIFFERENT SURFACE TREATMENTS; COMPOSITE RESIN; RETENTION; CEMENT; ROUGHNESS; ZIRCONIA;
D O I
10.1089/photob.2018.4601
中图分类号
R61 [外科手术学];
学科分类号
摘要
Objective: The purpose of this study was to evaluate the effects of Er,Cr:YSGG laser irradiation with different energy powers versus sandblasting for enhancing the tensile bond strength (TBS) between titanium implant abutments (IAs) and resin cements. Background data: Clinical decementation of prosthetic restorations often occurs, particularly on short IAs. Increasing the bonding area on the IA surface can enhance the function and longevity of the superstructure. Materials and methods: Fifty dental IAs were used in solid form and randomly assigned to five groups (n=10 each) for the following different pretreatments: control group was left untreated, a laser operating at 2.78 mu m wavelength with different energy powers (1, 2, and 3 W) was used for three laser groups, and 50 mu m alumina particles were applied to the abutment surface for the sandblasting group. Fifty metal substructures that had an occlusal metal O-ring were cast and cemented to all abutments using dual-cure resin cement. Test specimens were then subjected to thermal cycling. TBS tests were performed with a universal testing machine. The specimens' surface topography and roughness were evaluated with scanning electron microscope, and energy dispersive spectroscopy (EDS) was used to measure the elemental profiles of each specimen. Data were analyzed using a one-way analysis of variance/Kruskal-Wallis test at a significance level of p<0.05. Results: Surface treatments affected the surface roughness and TBS of the IA. The sandblasting group showed the highest bond strength values (510.7760.86N) and followed by the 2 W group (279.07 +/- 37.9N). In EDS analysis, no elemental components other than titanium and oxygen were observed, except for in the sandblasting group. Conclusions: Sandblasting and 2 W laser treatment increased the surface roughness of the IA, which could contribute to the increased interfacial bond strength between the IA and resin cement.
引用
收藏
页码:465 / 472
页数:8
相关论文
共 50 条
  • [41] Surface and Mineral Changes of Primary Enamel after Laser Diode Irradiation and Application of Remineralization Agents: A Comparative In Vitro Study
    Cirdei, Mihaela-Valentina
    Margan, Madalin-Marius
    Margan, Roxana
    Ban-Cucerzan, Alexandra
    Petre, Ion
    Hulka, Iosif
    Horhat, Razvan Mihai
    Todea, Darinca Carmen
    CHILDREN-BASEL, 2024, 11 (09):
  • [42] Optimized Er: YAG Laser Irradiation Distance to Achieve the Strongest Bond Strength Between Orthodontic Brackets and Zirconia-Ceramics
    Mirhashmi, Seyyed Amir Hossein
    Akhundi, Mohammad Sadegh Ahmad
    Ganji, Saeed Mehdi Pour
    Allandadi, Mehdi
    Norouzian, Mohammad
    Chiniforush, Nasim
    JOURNAL OF LASERS IN MEDICAL SCIENCES, 2020, 11 (03) : 287 - 291
  • [43] Investigations into the use of excimer laser irradiation as a titanium alloy surface treatment in a metal to composite adhesive bond
    Molitor, P
    Young, T
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2004, 24 (02) : 127 - 134
  • [44] Effects of dentin surface treatments including Er,Cr:YSGG laser irradiation with different intensities on the push-out bond strength of the glass fiber posts to root dentin
    Kirmali, Omer
    Kustarci, Alper
    Kapdan, Alper
    Er, Kursat
    ACTA ODONTOLOGICA SCANDINAVICA, 2015, 73 (05) : 380 - 386
  • [45] Experimental Study of Bond Strength between Titanium Bar and Lime-Based Mortar
    Osofero, Adelaja Israel
    Corradi, Marco
    Borri, Antonio
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2015, 27 (06)
  • [46] Silanizing Effectiveness on the Bond Strength of Aged Bulk-Fill Composite Repaired After Sandblasting or Bur Abrasion Treatments: An in vitro Study
    Hashim, Huda
    Abd-alla, Manal Hussain
    CLINICAL COSMETIC AND INVESTIGATIONAL DENTISTRY, 2022, 14 : 265 - 273
  • [47] Effect of 830 nm Diode Laser Irradiation of Root Canal on Bond Strength of Metal and Fiber Post
    Strefezza, Claudia
    Amaral, Marcello Magri
    Quinto, Jose, Jr.
    Gouw-Soares, Sheila Cynthia
    Zamataro, Claudia Bianchi
    Zezell, Denise Maria
    PHOTOMEDICINE AND LASER SURGERY, 2018, 36 (08) : 439 - 444
  • [48] Effects of Er:YAG and Er,Cr:YSGG laser irradiation and adhesive systems on microtensile bond strength of a self-adhering composite
    Kaptan, Alper
    Oznurhan, Fatih
    LASERS IN MEDICAL SCIENCE, 2023, 38 (01)
  • [49] Comparative in vitro Study of the Tensile Bond Strength of Three Orthodontic Bonding Materials
    Martha, Krisztina
    Ogodescu, Alexandru
    Zetu, Irina
    Ogodescu, Emilia
    Gyergyay, Reka
    Pacurar, Mariana
    MATERIALE PLASTICE, 2013, 50 (03) : 208 - 211
  • [50] Comparative Study of the Effects of Key Factors on Concrete-to-Concrete Bond Strength
    Mack, V.
    Salehfard, R.
    Korayem, A. Habibnejad
    CIVIL ENGINEERING INFRASTRUCTURES JOURNAL-CEIJ, 2024, 57 (01): : 205 - 223