Features of oxidative degradation of hydroxyethyl cellulose

被引:2
作者
Chursin, V. I. [1 ]
机构
[1] Joint Stock Co, Res Inst Leather Shoe Ind, Moscow, Russia
关键词
Cellulose;
D O I
10.1134/S1070427207040271
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
The kinetics of degradation of hydroxyethyl cellulose in its oxidation with hydrogen peroxide, sodium periodate, and potassium persulfate was studied. The effect of oxidation time and oxidant concentration on the properties of the oxidation products was analyzed.
引用
收藏
页码:654 / 659
页数:6
相关论文
共 9 条
[1]  
BORISOV IM, 2002, DOKL AKAD NAUK, V383, P774
[2]  
BORISOV IM, 2003, IZV VYSSH UCHEBN ZAV, V46, P29
[3]  
FILATOV VN, 2002, BIOLOICALLY ACTIVE M, V1
[4]  
GALIASKAROVA GG, 1998, P 11 RUSS C CHEM REA, P41
[5]  
GOLOVA OP, 1955, IZV AKAD NAUK SSSR O, P899
[6]  
Ioffe BV, 1983, Refractometric methods of chemistry
[7]  
MIKHAILOV AN, 1971, COLLAGEN COVERLET FU
[8]  
STEPANENKO BN, 1978, BIOCH CHEM CARBOHYDR
[9]  
ZHBANOV RG, 1964, INFRARED SPECTRA CEL