Mechanical property and ballistic resistance of graphene platelets/B4C Ceramic armor prepared by spark plasma sintering

被引:48
作者
Yin, Fengbin [1 ,2 ]
Yuan, Juntang [1 ,2 ]
Chen, Mingdan [1 ,2 ]
Si, Daoxing [1 ]
Xu, Chunyu [1 ]
机构
[1] Nanjing Univ Sci & Technol, Sch Mech Engn, Nanjing 210094, Jiangsu, Peoples R China
[2] Nanjing Univ Sci & Technol, Minist Ind & Informat Technol, Collaborat Innovat Ctr High End Equipment Mfg Tec, Nanjing, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
B4C; Graphene; Mechanical property; Ballistic performance; Spark plasma sintering; BORON-CARBIDE COMPOSITES; FRACTURE-TOUGHNESS; MICROSTRUCTURE; B4C; DENSIFICATION; SI; HARDNESS; TI3SIC2; SILICON; ABILITY;
D O I
10.1016/j.ceramint.2019.08.095
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Boron carbide (B4C) ceramic toughened by graphene platelets (GPLs) was prepared by spark plasma sintering. Nonmetallic sintering aids Al2O3/Y2O3 were used to improve the sintering ability of boron carbide. Impacts of Al2O3/Y2O3 on mechanical properties and microstructure, and toughening mechanisms of graphene platelets were studied. When the content of Al2O3/Y2O3 is 5 wt%, the B4C ceramic was fully densified, and its Vickers harness and fracture toughness are 30.87 +/- 0.26 GPa and 5.76 +/- 0.37 MPa m(1/2), respectively. Fracture toughness of B4C ceramic containing 1.5 wt% GPLs is increased by 23.1% in comparison with that of B4C ceramic without GPLs, which is mainly attributed to the pining effect and packing capacity of GPLs. Ballistic resistance of the GPLs/B4C ceramic armor was experimentally studied with the method of depth of penetration test in contrast to two commercial ceramic armors (SiC, B4C). Compared to SiC and B4C, the penetration depth on the GPLs/B4C ceramic armor is the smallest, and the ballistic resistance of GPLs/B4C ceramic armor is increased by 50% and 12.5%, respectively.
引用
收藏
页码:23781 / 23787
页数:7
相关论文
共 46 条
  • [41] Effect of Ni and graphene on microstructure and toughness of titanium boride ceramic tool material prepared by spark plasma sintering
    Yin, Zengbin
    Yuan, Juntang
    Xu, Weiwei
    Chen, Mingdan
    Yan, Shiyu
    Wang, Zhenhua
    [J]. CERAMICS INTERNATIONAL, 2018, 44 (16) : 20299 - 20305
  • [42] Graphene nanosheets toughened TiB2-based ceramic tool material by spark plasma sintering
    Yin, Zengbin
    Yuan, Juntang
    Xu, Weiwei
    Liu, Kui
    Yan, Shiyu
    [J]. CERAMICS INTERNATIONAL, 2018, 44 (08) : 8977 - 8982
  • [43] Densification mechanisms and microstructural evolution during spark plasma sintering of boron carbide powders
    Zhang, Mei
    Yuan, Tiechui
    Li, Ruidi
    Xie, Siyao
    Wang, Minbo
    Weng, Qigang
    [J]. CERAMICS INTERNATIONAL, 2018, 44 (04) : 3571 - 3579
  • [44] Densification behaviour and mechanical properties of B4C-SiC intergranular/intragranular nanocomposites fabricated through spark plasma sintering assisted by mechanochemistry
    Zhang, Xiaorong
    Zhang, Zhixiao
    Wang, Weimin
    Che, Hongwei
    Zhang, Xiaoliang
    Bai, Yongmei
    Zhang, Lina
    Fu, Zhengyi
    [J]. CERAMICS INTERNATIONAL, 2017, 43 (02) : 1904 - 1910
  • [45] On the use of Ti-Si eutectic alloy as a novel sintering aid for B4C-TiB2-SiC ceramic composites
    Zhong, Zhihong
    Yang, Ankang
    Wang, Rui
    Wen, Qun
    Zhu, Zhixiong
    Wang, Guoping
    Zhang, Haibin
    [J]. CERAMICS INTERNATIONAL, 2019, 45 (09) : 12393 - 12398
  • [46] Effects of carbon and silicon on microstructure and mechanical properties of pressureless sintered B4C/TiB2 composites
    Zhu, Yu
    Cheng, Huanwu
    Wang, Yangwei
    An, Rui
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 772 : 537 - 545