Investigation of Mg, K, Cu, Zn doped S53P4 bioactive glass in vitro studies; bioactivity and biodegradability features

被引:0
|
作者
Cevlik, Cem Batuhan [1 ]
Ozarslan, Ali Can [1 ]
Lkizler, Burcu Karakuzu [1 ]
Elalmis, Yeliz Basaran [1 ]
Yucel, Sevil [1 ]
机构
[1] Yildiz Tech Univ, Dept Bioengn, Fac Chem & Met Engn, Istanbul, Turkey
关键词
Bioactive glass; doped; melt-quenching method; various forms; simulated body fluid; SUBSTITUTES; SCAFFOLDS;
D O I
暂无
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
In this study, it was aimed to produce by melt-quenching method non-additive (SiO2-Na2O-P2O5-CaO) and ion additive (SiO2-Na2O-P2O5-CaO-MgO-ZnO-K2O-CuO) bioactive glasses (different forms; powder and granule). In vitro bioactivity and biodegradability properties of bioactive glasses in different forms (granule and powder) were examined with Simulated Body Fluid (SBF) and Tris-HCI analyses. Chemical bonds structures and surface morphology analysis of bioactive glasses (both additive and non-additive) were performed with FT-IR and SEM-EDS analysis before and after SBF immersion. SBF studies showed that both S53P4 bioactive glasses had similar bioactivity. As a results of Tris-HCI studies, in vitro biodegradability of bioactive glasses in powder forms are better than bioactive glasses in granule forms because of rapid raise of its pH value in Tris-HCI. However, ion additive S53P4 powder bioactive glass had more stable degradation behavior in comparison with non-additive S53P4 powder bioactive glass.
引用
收藏
页码:1131 / 1136
页数:6
相关论文
共 50 条
  • [1] Phase composition and in vitro bioactivity of porous implants made of bioactive glass S53P4
    Fagerlund, S.
    Massera, J.
    Moritz, N.
    Hupa, L.
    Hupa, M.
    ACTA BIOMATERIALIA, 2012, 8 (06) : 2331 - 2339
  • [2] In vitro dissolution of bioactive glass S53P4 microspheres
    Sinitsyna, Polina
    Karlstrom, Oskar
    Hupa, Leena
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2022, 105 (03) : 1658 - 1670
  • [3] In vitro antibiofilm activity of bioactive glass S53P4
    Drago, Lorenzo
    Vassena, Christian
    Fenu, Simone
    De Vecchi, Elena
    Signori, Valentina
    De Francesco, Raffaele
    Romano, Carlo Luca
    FUTURE MICROBIOLOGY, 2014, 9 (05) : 593 - 601
  • [4] In vitro model for frontal sinus obliteration with bioactive glass S53P4
    Peltola, MJ
    Suonpää, JTK
    Andersson, ÖH
    Määttänen, HS
    Aitasalo, KMJ
    Yli-Urpo, A
    Laippala, PJ
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 2000, 53 (02): : 161 - 166
  • [5] S53P4 Bioactive Glass - an Alternative Treatment of Bone Defects
    Trambitas, Cristian
    Pop, Tudor Sorin
    Miron, Alina Dia Trambitas
    Dorobantu, Dorin Constantin
    Brinzaniuc, Klara
    REVISTA DE CHIMIE, 2017, 68 (02): : 387 - 389
  • [6] Influence of SrO substitution for CaO on the properties of bioactive glass S53P4
    Jonathan Massera
    Leena Hupa
    Journal of Materials Science: Materials in Medicine, 2014, 25 : 657 - 668
  • [7] Mastoid obliteration with S53P4 bioactive glass in cholesteatoma surgery
    Mestdagh, Pieter D. de Veij
    Colnot, David R.
    Borggreven, Pepijn A.
    Orelio, Claudia C.
    Quak, Jasper J.
    ACTA OTO-LARYNGOLOGICA, 2017, 137 (07) : 690 - 694
  • [8] Clinical applications of Bioactive glass S53P4 in bone infections: a systematic review
    Bigoni, M.
    Turati, M.
    Zanchi, N.
    Lombardo, A. S.
    Graci, J.
    Omeljaniuk, R. J.
    Zatti, G.
    Gaddi, D.
    EUROPEAN REVIEW FOR MEDICAL AND PHARMACOLOGICAL SCIENCES, 2019, 23 : 240 - 251
  • [9] Impact of substituting K2O for Na2O on physico-chemical properties and in vitro bioactivity of bioactive glass S53P4
    Sinitsyna, Polina
    Engblom, Markus
    Hupa, Leena
    OPEN CERAMICS, 2023, 16
  • [10] Preparation and characterization of fluorapatite-bioactive glass S53P4 nanocomposite
    Manafi, Sahebali
    Mirjalili, Fatemeh
    Hajisafari, Mahmood
    Orand, Faranak
    JOURNAL OF NANOANALYSIS, 2019, 6 (03): : 145 - 156