Dynamic failure of fibre-metal laminates under impact loading - experimental observations

被引:22
作者
Li, Xin [1 ,2 ]
Yahya, Mohd Yazid [1 ]
Nia, Amin Bassiri [1 ]
Wang, Zhihua [2 ]
Lu, Guoxing [3 ]
机构
[1] Univ Teknol Malaysia, Fac Mech Engn, Ctr Composite, Johor Baharu 81310, Malaysia
[2] Taiyuan Univ Technol, Inst Appl Mech & Biomed Engn, Taiyuan, Peoples R China
[3] Swinburne Univ Technol, Fac Sci Engn & Technol, Hawthorn, Vic 3122, Australia
基金
中国国家自然科学基金;
关键词
Fibre-metal laminates; impact loading; failure mechanism; PERFORATION RESISTANCE; BEHAVIOR; INITIATION;
D O I
10.1177/0731684415616501
中图分类号
TB33 [复合材料];
学科分类号
摘要
The dynamic failure of fibre metal laminates was investigated experimentally. A projectile of hemispherical head with a diameter of 36.5mm was used to impact the fibre metal laminate panels. Three types of woven fibre fabrics (Basalt, S2-glass and Kevlar-29) were used to reinforce the aluminum sheets. Tests on these fibre metal laminate panels were conducted by using an aerodynamic gun with the impact velocity ranging from 20.6m/s to 42.8m/s. Different deformation/failure modes of fibre metal laminates were obtained by varying the impact energy. The failure mechanisms of composite layers were examined by the field emission scanning electron microscope. The results showed that before the fibre metal laminate panels were penetrated, the global deformation increased with the impact velocity. However, evident reduction of global deformation can be observed after penetration occurred. Damages of fibre metal laminate panels such as tearing of aluminum ply, fibre fracture, matrix cracks and debonding/delamination were observed around the impact region. The results indicate that basalt reinforced aluminum laminates perform well in terms of impact resistance and offer significant potential in engineering applications.
引用
收藏
页码:305 / 319
页数:15
相关论文
共 50 条
[41]   Process Variables Optimisation of Polypropylene Based Fibre-Metal Laminates Forming Using Finite Element Analysis [J].
DharMalingam, Sivakumar ;
Compston, Paul ;
Kalyanasundaram, Shankar .
SHEET METAL 2009, 2009, 410-411 :263-269
[42]   Tensile failure of fibre-metal-laminates made of titanium and carbon-fibre/epoxy laminates [J].
Sun, Jing ;
Daliri, Ali ;
Lu, Guoxing ;
Ruan, Dong ;
Lv, Yang .
MATERIALS & DESIGN, 2019, 183
[43]   Finite Element Modeling of Dynamic Failure of Composite Laminates Under Transverse Tensile Loading [J].
Liu, Tengfei .
JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2021, 21 (01) :228-240
[44]   Numerical Simulation of Bird Impact on Fibre Metal Laminates [J].
Zhu, Shuhua ;
Wang, Yuequan ;
Tong, Mingbo ;
Pan, Xiong .
POLYMERS & POLYMER COMPOSITES, 2014, 22 (02) :147-156
[45]   Low velocity impact on fibre metal laminates: A review [J].
Kakati, Sasanka ;
Chakraborty, Debabrata .
JOURNAL OF COMPOSITE MATERIALS, 2023, 57 (30) :4731-4750
[46]   THE HIGH VELOCITY IMPACT RESISTANCE OF FIBRE METAL LAMINATES [J].
Zhou, J. ;
Kaboglu, C. ;
Mohagheghian, I. ;
Guan, Z. ;
Dear, J. P. ;
Cantwell, W. J. .
ICCM 21: 21ST INTERNATIONAL CONFERENCE ON COMPOSITE MATERIALS (ICCM-21), 2017,
[47]   Failure analysis of fibre metal laminate channel section column under axial compressive pulse loading [J].
Zaczynska, Monika .
BULLETIN OF THE POLISH ACADEMY OF SCIENCES-TECHNICAL SCIENCES, 2024, 72 (05)
[48]   Large deflection dynamic response of (fiber/polymer)-metal laminates subjected to impact loading [J].
Li K. ;
Zhang J. ;
Zhang W. ;
Xia Y. ;
Li J. ;
Sha Z. ;
Qin Q. .
Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica, 2020, 37 (01) :147-154
[49]   Impact resistance and bonding capability of sandwich panels with fibre-metal laminate skins and aluminium foam core [J].
Liu, Chengjun ;
Zhang, Y. X. ;
Heslehurst, Rikard .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2014, 28 (24) :2378-2392
[50]   Mesoscale modelling of fibre reinforced concrete material under compressive impact loading [J].
Xu, Z. ;
Hao, H. ;
Li, H. N. .
CONSTRUCTION AND BUILDING MATERIALS, 2012, 26 (01) :274-288