Sorption and desorption of silver ions by bentonite clays

被引:11
作者
Constantino, Leonel Vinicius [1 ]
Quirino, Juliana Nunes [1 ]
Monteiro, Alessandra Maffei [1 ]
Abrao, Taufik [2 ]
Parreira, Paulo Sergio [3 ]
Urbano, Alexandre
Santos, Maria Josefa [1 ]
机构
[1] Univ Estadual Londrina, Dept Quim, Rod Celso Garcia Cid PR445, BR-86051990 Londrina, Parana, Brazil
[2] State Univ Londrina UEL, Dept Elect Engn DEEL, Rod Celso Garcia Cid PR445 S-N,Campus Univ, BR-86057970 Londrina, PR, Brazil
[3] Univ Estadual Londrina, Dept Fis, Rod Celso Garcia Cid PR445, BR-86051990 Londrina, Parana, Brazil
关键词
Montmorillonite; Sorption; Desorption; Environment; Silver; MODIFIED CHITOSAN; AQUEOUS-SOLUTIONS; ADSORPTION; REMOVAL; TOXICITY; EQUILIBRIUM; COPPER; CU;
D O I
10.1007/s11356-017-8394-x
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Anthropogenic activities have increased the concentration of metal species in the environment. The toxicity of silver ions to aquatic and terrestrial organisms has required monitoring by analytical methods, besides actions to promote its control as pollutant. Sorption and desorption processes are directly related to the mobility and availability of metal ions in the environment. In this context, clay minerals can be used for pre-concentration, removal and recovery of silver ions from aqueous solution. Herein, two bentonite clays (BaVC-1 and SWy-2) were characterised and applied to investigate the sorption and desorption of silver ions. Isotherms were fitted to the dual-mode Langmuir-Freundlich model to qualify and quantify sorption sites and evaluate the mobilisation process. The maximum sorption capacity was 743 and 849 meq kg(-1) for BaVC-1 and SWy-2, respectively. Hysteresis index (HI) and mobilisation factor (MF) suggest that the desorption of silver ions in BaVC-1 is about four times more conducive compared to that in SWy-2, although both materials have demonstrated a great potential for Ag+ pre-concentration from aqueous solutions.
引用
收藏
页码:11349 / 11359
页数:11
相关论文
共 49 条
[1]   Removal of divalent manganese from aqueous solution using glycine modified chitosan resin [J].
Al-Wakeel, Khaled Z. ;
Abd El Monem, H. ;
Khalil, Mostafa M. H. .
JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2015, 3 (01) :179-186
[2]  
[Anonymous], 2004, Soil and Water Chemistry: An Integrative Approach
[3]  
ATSDR, 2015, PUBL HLTH STAT SILV
[4]   Preparation, characterization and catalytic activity of titania pillared montmorillonite clays [J].
Binitha, N. N. ;
Sugunan, S. .
MICROPOROUS AND MESOPOROUS MATERIALS, 2006, 93 (1-3) :82-89
[5]   Characterization of Cu-complexes in smectite with different layer charge location: Chemical, thermal and EXAFS studies [J].
Brigatti, MF ;
Colonna, S ;
Malferrari, D ;
Medici, L .
GEOCHIMICA ET COSMOCHIMICA ACTA, 2004, 68 (04) :781-788
[6]   ACUTE TOXICITY OF PRIORITY POLLUTANTS TO BLUEGILL (LEPOMIS-MACROCHIRUS) [J].
BUCCAFUSCO, RJ ;
ELLS, SJ ;
LEBLANC, GA .
BULLETIN OF ENVIRONMENTAL CONTAMINATION AND TOXICOLOGY, 1981, 26 (04) :446-452
[7]   Characterization of the cation-exchanged bentonites by XRPD, ATR, DTA/TG analyses and BET measurement [J].
Caglar, B. ;
Afsin, B. ;
Tabak, A. ;
Eren, E. .
CHEMICAL ENGINEERING JOURNAL, 2009, 149 (1-3) :242-248
[8]  
Carlson L, 2004, BENTONITE MINERALO 2
[9]   Removal of cadmium, zinc, manganese and chromium cations from aqueous solution by a clay mineral [J].
da Fonseca, Maria G. ;
de Oliveira, Michelle M. ;
Arakaki, Luiza N. H. .
JOURNAL OF HAZARDOUS MATERIALS, 2006, 137 (01) :288-292
[10]  