Corrosion of silicon nitride materials in acidic and basic solutions and under hydrothermal conditions

被引:35
作者
Herrmann, M
Schilm, J
Michael, G
Meinhardt, J
Flegler, R
机构
[1] Fraunhofer Inst Keram Technol & Sinterwerkstoffe, D-01277 Dresden, Germany
[2] Fraunhofer Inst Silikatforsch, Wurzburg, Germany
关键词
corrosion; hydrothermal corrosion; kinetics; Si3N4; CERAMICS;
D O I
10.1016/S0955-2219(02)00303-5
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Silicon nitride ceramics with different amounts and compositons of the grain boundary phases are produced by gas pressure sintering and the corrosion behaviour was analysed in acids, bases and under hydrothermal conditions. The investigation shows, that the corrosion is strongly affected by the SiO2 content in the grain boundary and the amount of the additives. The results indicate that the grains and the thin films between the grains are very stable in acids and bases but solves partially under hydrothermal conditions. The corrosion behaviour of the investigated materials with a relatively stable grain boundary phase in acids can be described by the same kinetic laws as those used to describe the corrosion of glasses. An interfacial reaction is assumed to be rate-controlling. The less stable material with Y2O3/Al2O3 additives can be described by the corrosion behaviour of oxide nitride glasses only at the beginning. For higher corrosion deaths, the formation of protective barriers consisting of a hydrated SiO2 network is assumed to occur. (C) 2003 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:585 / 594
页数:10
相关论文
共 16 条
[1]   An inhomogeneous grain boundary composition in silicon nitride ceramics as revealed by 300 kV field emission analytical electron microscopy [J].
Bando, Y ;
Mitomo, M ;
Kurashima, K .
JOURNAL OF MATERIALS SYNTHESIS AND PROCESSING, 1998, 6 (05) :359-365
[2]   A diffuse interface description of intergranular films in polycrystalline ceramics [J].
Bobeth, M ;
Clarke, DR ;
Wolfgang, P .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1999, 82 (06) :1537-1546
[3]  
HERRMAN M, 2000, HDB CERAMIC HARD MAT, P747
[4]  
HERRMANN M, 1999, BR CERAM P, V60, P455
[5]  
HERRMANN M, 1999, CFI DKG BERICHTE, V14, P130
[6]  
HERRMANN M, 24711 HE DFG PROJ
[7]   Corrosion resistance of silicon nitride ceramics [J].
Komeya, K ;
Meguro, T ;
Atago, S ;
Lin, CH ;
Abe, Y ;
Komatsu, M .
SCIENCE OF ENGINEERING CERAMICS II, 1999, 2 :235-238
[8]   Corrosion of silicon nitride in sulphuric acid aqueous solution [J].
Monteverde, F ;
Mingazzini, C ;
Giorgi, M ;
Bellosi, A .
CORROSION SCIENCE, 2001, 43 (10) :1851-1863
[9]   Mechanical degradation of silicon nitride ceramics in corrosive solutions of boiling sulphuric acid [J].
Okada, A ;
Yoshimura, M .
CORROSION OF ADVANCED CERAMICS, 1996, 113 :227-236
[10]   CHEMICAL DURABILITY OF GLASSES - THERMODYNAMIC APPROACH [J].
PAUL, A .
JOURNAL OF MATERIALS SCIENCE, 1977, 12 (11) :2246-2268