Electrochemical study on hot corrosion of Si-modified aluminide coated In-738LC in Na2SO4-20 wt.% NaCl melt at 750°C

被引:70
|
作者
Shirvani, K [1 ]
Saremi, M
Nishikata, A
Tsuru, T
机构
[1] Univ Tehran, Fac Engn, Dept Met & Mat Engn, Tehran, Iran
[2] Tokyo Inst Technol, Grad Sch Engn, Dept Met & Ceram Sci, Meguro Ku, Tokyo 1528552, Japan
关键词
hot corrosion; molten salt;
D O I
10.1016/S0010-938X(02)00127-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion performance of the slurry Si-modified alummide coating on the nickel base superalloy In-738LC exposed to low temperature hot corrosion condition has been investigated in Na2SO4-20 wt.% NaCl melt at 750 degreesC by combined use of the anodic polarization and characterization techniques. The coated specimen showed a passive behavior up to -0.460 V vs. Ag/AgCl (0.1 mol fraction) reference electrode, followed by a rapid increase in anodic current due to localized attack in the higher potential region. In the passive region, the anodic dissolution of constituents of the coating occurred through the passive film, probably SiO2, at slow rate of 20-30 mutA/cm(2). The passive current for the Si-modified coating was two orders of magnitude smaller than that for bare In-738LC, which is known as Cr2O3 former in this melt. This indicates that the SiO2 film is chemically more stable than Cr2O3 film under this condition. However, pitting-like corrosion commenced around -0.460 V and proceeded at the high rate of 100 mA/cm(2) in the higher potential region than +0.400 V. The corrosion products formed on the coating polarized in different anodic potentials were characterized by SEM, EDS and XRD. It was found from the characterization that oxidation was dominant attack mode and no considerable sulfidation occurred at 750 degreesC. The SiO2 oxide was not characterized in the passive region because the thickness of the passive film was extremely thin, but was detected as the primary oxide in the localized corrosion region, where the selective oxidation of Al was observed by further progress of the corrosion attack front into the inner layer of coating. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1011 / 1021
页数:11
相关论文
共 28 条
  • [1] Hot corrosion behavior of aluminized and Si-modified aluminized coated IN-738LC produced by a novel hot-dip process
    Targhi, Vahid Tavakoli
    Omidvar, Hamid
    Sharifianjazi, Fariborz
    Pakseresht, Amirhossein
    SURFACES AND INTERFACES, 2020, 21
  • [2] Hot corrosion behaviour of a Ni plus CrAlYSiN composite coating in Na2SO4-25 wt.% NaCl melt
    Zhu, Lijuan
    Zhu, Shenglong
    Wang, Fuhui
    APPLIED SURFACE SCIENCE, 2013, 268 : 103 - 110
  • [3] Electrochemical impedance study of corrosion of B-1900 alloy in the presence of a solid Na2SO4 and a liquid 25 wt.% NaCl-75 wt.% Na2SO4 film at 800 °C in air
    Zeng, CL
    Zhang, T
    ELECTROCHIMICA ACTA, 2004, 49 (9-10) : 1429 - 1433
  • [4] Hot Corrosion Behavior of Si-Y-Co-Modified Aluminide Coating Exposed to NaCl + Na2SO4 Salt at 1173 K
    Liu, Zongjie
    Zhou, Chungen
    OXIDATION OF METALS, 2016, 85 (1-2): : 205 - 217
  • [5] Hot Corrosion Behavior of Si–Y–Co-Modified Aluminide Coating Exposed to NaCl + Na2SO4 Salt at 1173 K
    Zongjie Liu
    Chungen Zhou
    Oxidation of Metals, 2016, 85 : 205 - 217
  • [6] Hot corrosion of YSZ/Al2O3 dispersed NiCrAlY plasma-sprayed coatings in Na2SO4-10 wt.% NaCl melt
    Sreedhar, Gosipathala
    Raja, V. S.
    CORROSION SCIENCE, 2010, 52 (08) : 2592 - 2602
  • [7] Synergistic effect of element modification and preoxidation on hot corrosion behaviour of the nanocrystalline coating under molten salt of 75 wt.% Na2 SO4+25 wt.% NaCl at 900 °C
    Yang, Xiaowen
    Yang, Lanlan
    Lu, Yiliang
    Wang, Jinlong
    Yang, Shasha
    Chen, Zehao
    Zhang, Qiang
    Chen, Minghui
    Qiao, Yanxin
    Wang, Fuhui
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 235 : 53 - 69
  • [8] Hot corrosion and electrochemical behavior of NiCrAlY, NiCoCrAlY and NiCoCrAlYTa coatings in molten NaCl-Na2SO4 at 800°C
    Wang, Jiahao
    Li, Dangguo
    Shao, Tianmin
    SURFACE & COATINGS TECHNOLOGY, 2022, 440
  • [9] Role of iridium in hot corrosion resistance of pt-ir modified aluminide coatings with Na2SO4-NaCl salt at 1173 K
    Wu, Ying-Na
    Yamaguchi, Akihiro
    Murakami, Hideyuki
    Kuroda, Seiji
    MATERIALS TRANSACTIONS, 2006, 47 (08) : 1918 - 1921
  • [10] Hot corrosion behavior and near-surface microstructure of a "low-temperature high-activity Cr-aluminide" coating on inconel 738LC exposed to Na2SO4, Na2SO4 + V2O5 and Na2SO4 + V2O5 + NaCl at 900 °C
    Doolabi, M. Salehi
    Ghasemi, B.
    Sadrnezhaad, S. K.
    Habibollahzadeh, A.
    Jafarzadeh, K.
    CORROSION SCIENCE, 2017, 128 : 42 - 53