Preparation, characterization and hydrolytic degradation of poly[p-dioxanone-(butylene succinate)] multiblockcopolymer

被引:23
作者
Ding, Song-Dong [1 ]
Zheng, Guang-Can [1 ]
Zeng, Jian-Bing [1 ]
Zhang, Li [1 ]
Li, Yi-Dong [1 ]
Wang, Yu-Zhong [1 ]
机构
[1] Sichuan Univ, Ctr Degradable & Flame Retardant Polymer Mat, ERCEPM MoE, Coll Chem,State Key Lab Polymer Mat Engn, Chengdu 610064, Peoples R China
关键词
Poly(p-dioxanone); Poly(butylene succinate); Poly[p-dioxanone-(butylene succinate); Hydrolytic degradation; RING-OPENING POLYMERIZATION; ENHANCED THERMAL-STABILITY; MOLECULAR-WEIGHT; POLY(BUTYLENE SUCCINATE); ENZYMATIC DEGRADATION; POLY(P-DIOXANONE); CRYSTALLIZATION; MORPHOLOGY; 1,4-DIOXAN-2-ONE; MELT;
D O I
10.1016/j.eurpolymj.2009.08.019
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A series of poly[p-dioxanone-(butylene succinate)] (PPDOBS) copolymers were prepared from p-dioxanone (PDO), 1,4-butanediol and succinate acids through a two-step process including the initial prepolymer preparation of poly(p-dioxanone)diol (PPDO-OH) and poly(butylene succinate)diol (PBS-OH) and the following copolymerization of the two kinds of prepolymers by coupling with hexamethylene diisocyanate (HDI). The molecular structures of the prepared PPDO-OH, PBS-OH and PPDOBS were characterized by hydrogen nuclear magnetic resonance spectroscopy (H-1 NMR). The crystallization of the copolymers was investigated by using differential scanning calorimetry (DSC), polarized optical microscopy (POM) and wide angle X-ray diffraction (WAXD). It has been shown that the crystallization rate and the degree of crystallization increases with the increase of the weight fraction of poly(butylene succinate) (PBS) blocks in the copolymers. In phosphate buffer solution with pH 7.4 at 37 degrees C for 18 weeks, the hydrolytic degradation behaviors of the copolymers were studied. The changes of retention weight, water absorption, pH value, and surface morphologies with the degradation time showed that the hydrolytic degradation rate of PPDOBS could be controlled by adjusting the weight fraction of poly(p-dioxanone) (PPDO) and PBS blocks in the copolymers. The changes of the thermal properties of PPDOBS during the degradation were also investigated by DSC. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3043 / 3057
页数:15
相关论文
共 44 条
  • [1] Nucleation and crystallization in double crystalline poly(p-dioxanone)-b-poly(ε-caprolactone) diblock copolymers
    Albuerne, J
    Márquez, L
    Müller, AJ
    Raquez, JM
    Degée, P
    Dubois, P
    Castelletto, V
    Hamley, IW
    [J]. MACROMOLECULES, 2003, 36 (05) : 1633 - 1644
  • [2] ANNIKAM L, 2004, POLYM DEGRAD STABIL, V83, P487
  • [3] Syntheses and physical characterization of new aliphatic triblock poly(L-lactide-b-butylene succinate-b-L-lactide)s bearing soft and hard biodegradable building blocks
    Ba, CY
    Yang, J
    Hao, QH
    Liu, XY
    Cao, A
    [J]. BIOMACROMOLECULES, 2003, 4 (06) : 1827 - 1834
  • [4] Novel amphiphilic triblock copolymer based on PPDO, PCL, and PEG: Synthesis, characterization, and aqueous dispersion
    Bahadur, K. C. Remant
    Bhattarai, Shanta Raj
    Aryal, Santosh
    Khil, Myung Seob
    Dharmaraj, N.
    Kim, Hak Yong
    [J]. COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 2007, 292 (01) : 69 - 78
  • [5] BEZWADA RS, 1995, Patent No. 5470340
  • [7] ENHANCED THERMAL STABILITY OF POLY(p-DIOXANONE) IN MELT BY ADDING AN END-CAPPING REAGENT
    Ding, S. -D.
    Bai, C. -Y.
    Liu, Z. -P.
    Wang, Y. -Z
    [J]. JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2008, 94 (01) : 89 - 95
  • [8] DING SD, 2009, J POLYM RES
  • [9] Enhanced thermal stability of poly(1,4-dioxan-2-one) in melt by adding a chelator
    Ding, Song-Dong
    Wang, Yu-Zhong
    [J]. POLYMER DEGRADATION AND STABILITY, 2006, 91 (10) : 2465 - 2470
  • [10] Doddi N, 1977, United States patent, Patent No. [US 4032 988(A1), 4032988, 4, 032, 988]