The effects of grinding on the structure of a low-defect kaolinite

被引:0
|
作者
Reynolds, RC [1 ]
Bish, DL
机构
[1] Dartmouth Coll, Hanover, NH 03755 USA
[2] Los Alamos Natl Lab, Los Alamos, NM 87545 USA
关键词
D O I
暂无
中图分类号
P3 [地球物理学]; P59 [地球化学];
学科分类号
0708 ; 070902 ;
摘要
Numerous studies have demonstrated the presence of at least two distinct kaolinites in individual kaolinite samples, one a low-defect material and the other a moderate- to high-defect material. Other studies have shown that some kaolinites contain the lowest-defect material in the coarsest size fractions whereas others contain the lowest-defect kaolinite in the finest fractions. In an attempt to clarify possible mechanisms for producing such kaolinite samples, we have used powder X-ray diffraction to study the effects of mechanical grinding on the nature of layer stacking in the >40 mum fraction of the American Petroleum Institute kaolinite standard no. 9 from Mesa Alta, New Mexico. This material is relatively rich in a low-defect kaolinite. Hand grinding for 10 min plus grinding under acetone for up to an additional 34 min in an automatic agate grinder produced significant changes in its diffraction pattern. However, further dry grinding in a ball mill for 10 min produced material that was almost totally disordered, based on measures such as the Hinkley index. The diffraction patterns of the wet-ground materials showed evidence of increasing disorder that could be modeled best as a physical mixture of low- and high-defect material, consistent with a physical mixture of the original ordered phase with varying amounts of a highly disordered material. Disorder in the high-defect kaolinite is caused by the interstratification of normal kaolinite layers with their enantiomorphs. Contrary to expectations, grinding of kaolinite does not produce a progressive increase in disorder for all of the crystallites present in a sample. Instead, grinding apparently creates increased amounts of a disordered kaolinite that coexist with relatively unaffected material. There is no evidence for the occurrence of an intermediate disordered phase. Contrary to previous reports, disorder caused by physical stress does not include random layer displacements of +/-b/3.
引用
收藏
页码:1626 / 1630
页数:5
相关论文
共 50 条
  • [1] Deintercalation of Hydrazine-Intercalated Low-Defect Kaolinite
    Ray L. Frost
    J. Theo Kloprogge
    Janos Kristof
    Erzsebet Horvath
    Clays and Clay Minerals, 1999, 47 : 732 - 741
  • [2] Deintercalation of hydrazine-intercalated low-defect kaolinite
    Ctr. Instrumental and Devmtl. Chem., Queensland University of Technology, 2 George Street, Brisbane, QLD Q 4001, Australia
    不详
    不详
    Clays Clay Min., 6 (732-741):
  • [3] Deintercalation of hydrazine-intercalated low-defect kaolinite
    Frost, RL
    Kloprogge, JT
    Kristof, J
    Horvath, E
    CLAYS AND CLAY MINERALS, 1999, 47 (06) : 732 - 741
  • [4] PREPARATION, STRUCTURE, AND PROPERTIES OF LOW-DEFECT POLYACETYLENE
    KOBRVANSKII, VM
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA A & SERIYA B, 1994, 36 (05): : B881 - B894
  • [5] High- and low-defect kaolinite for brick making: Comparisons of technological properties, phase evolution and microstructure
    Wang, Sen
    Gainey, Lloyd
    Mackinnon, Ian D. R.
    Xi, Yunfei
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 366
  • [6] Spectra on the influence of grinding to kaolinite structure
    Hao, QL
    Yang, XJ
    Wang, Y
    Lu, L
    Wang, X
    SPECTROSCOPY AND SPECTRAL ANALYSIS, 2000, 20 (03) : 302 - 304
  • [7] Antibacterial and Low-Defect Graphene Ink Coatings
    Dimitrieva, S. E.
    Baskakov, S. A.
    Baskakova, Yu. V.
    NANOBIOTECHNOLOGY REPORTS, 2024, 19 (01) : 78 - 88
  • [8] Spectra on the influence of grinding to kaolinite structure
    Hao, Qingli
    Yang, Xujie
    Wang, Ying
    Lu, Lude
    Wang, Xin
    Guang Pu Xue Yu Guang Pu Fen Xi/Spectroscopy and Spectral Analysis, 2000, 20 (03): : 302 - 304
  • [9] REACTIVE EVAPORATION OF LOW-DEFECT DENSITY HAFNIA
    CHOW, R
    FALABELLA, S
    LOOMIS, GE
    RAINER, F
    STOLZ, CJ
    KOZLOWSKI, MR
    APPLIED OPTICS, 1993, 32 (28): : 5567 - 5574
  • [10] A NEW TECHNIQUE FOR CHARACTERIZING LOW-DEFECT SIMOX
    FECHNER, PS
    GARDNER, GR
    LIU, ST
    MATERIALS LETTERS, 1990, 9 (12) : 508 - 510