Mechanical behavior of facial prosthetic elastomers after outdoor weathering

被引:48
作者
Eleni, P. N. [1 ]
Katsavou, I. [1 ]
Krokida, M. K. [1 ]
Polyzois, G. L. [2 ]
Gettleman, L. [3 ]
机构
[1] Natl Tech Univ Athens, Dept Chem Engn, Athens 15780, Greece
[2] Univ Athens, Div Removable Prosthodont, Sch Dent, Athens 11527, Greece
[3] Univ Louisville, Dept Diagnost Sci, Sch Dent, Louisville, KY 40292 USA
关键词
Natural weathering; Polydimethyl siloxane; Chlorinated polyethylene; Hardness; Tensile strength; MAXILLOFACIAL ELASTOMERS; PHYSICAL-PROPERTIES; THERMAL-ANALYSIS; SILICONE-RUBBER; COLOR STABILITY; UV-RADIATION; DEGRADATION; POLYMERS; POLYETHYLENE; SKIN;
D O I
10.1016/j.dental.2009.06.018
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. The degradation of maxillofacial prosthetic elastomers that occurs during physical weathering is usually responsible for the replacement of prostheses. In this study the mechanical behavior of 4 non-pigmented facial prosthetic elastomers, exposed to outdoor weathering for 1 year, was investigated. The hypothesis investigated was that irradiation time did not affect the properties measured. Methods. The samples were exposed to solar radiation for 1 year in Thessaloniki (Greece). Three different types of polydimethyl siloxane (PDMS) and chlorinated polyethylene (CPE) samples were tested in this study. Mechanical tests (compressive-tensile) were performed using a universal type testing machine. Hardness tests were evaluated using a durometer tester. Simple mathematical models were developed to correlate the measured properties with irradiation time. The stress-strain data of compression and tensile tests were modeled using parameters such as maximum stress (sigma(max)), maximum strain (epsilon(max)), elasticity parameter (E), and non-linearity parameter (p), while the mathematical model used for hardness data involves initial hardness of materials (H(0)). Results. Two of the silicone prosthetics (Elastomer 42, TechSil 25) seem to become harder and more brittle contrary to the other silicone (M 511) and chlorinated polyethylene (CPE) samples that become softer and more ductile. Duration of exposure increases these phenomena. Conclusion. The effect of irradiation time on the mechanical behavior was introduced through its effect on the models' parameters. The hypothesis was rejected since changes were observed in the model parameters. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1493 / 1502
页数:10
相关论文
共 47 条
[1]   Modification of polysiloxane polymers for biomedical applications: a review [J].
Abbasi, F ;
Mirzadeh, H ;
Katbab, AA .
POLYMER INTERNATIONAL, 2001, 50 (12) :1279-1287
[2]  
[Anonymous], D39503 ASTM
[3]  
[Anonymous], D224005 ASTM
[4]  
*ASTM, D41205 ASTM
[5]   An elastomeric material for facial prostheses: synthesis, experimental and numerical testing aspects [J].
Bellamy, K ;
Limbert, G ;
Waters, MG ;
Middleton, J .
BIOMATERIALS, 2003, 24 (27) :5061-5066
[6]  
Bellamy KE, 2005, BIO-MED MATER ENG, V15, P21
[7]   Accelerated aging and lifetime prediction: Review of non-Arrhenius behaviour due to two competing processes [J].
Celina, M ;
Gillen, KT ;
Assink, RA .
POLYMER DEGRADATION AND STABILITY, 2005, 90 (03) :395-404
[8]   Crystallization of PDMS The effect of physical and chemical crosslinks [J].
Dollase, T ;
Spiess, HW ;
Gottlieb, M ;
Yerushalmi-Rozen, R .
EUROPHYSICS LETTERS, 2002, 60 (03) :390-396
[9]   PHYSICAL-PROPERTIES OF 3 MAXILLOFACIAL MATERIALS AS A FUNCTION OF ACCELERATED AGING [J].
DOOTZ, ER ;
KORAN, A ;
CRAIG, RG .
JOURNAL OF PROSTHETIC DENTISTRY, 1994, 71 (04) :379-383
[10]   WEIBULL MODELS FOR THE STATISTICAL-ANALYSIS OF DENTAL COMPOSITE DATA - AGED IN PHYSIOLOGICAL MEDIA AND CYCLIC-FATIGUED [J].
DRUMMOND, JL ;
MIESCKE, KJ .
DENTAL MATERIALS, 1991, 7 (01) :25-29