Synthesis and Characterization of Polyvinylidene-fluoride (PVDF) Nanofiber for Application as Piezoelectric Force Sensor

被引:30
作者
Saha, Shubhanwita [1 ]
Yauvana, V [2 ]
Chakraborty, Sandip [1 ]
Sanyal, Dipayan [1 ]
机构
[1] Cent Glass & Ceram Res Inst, CSIR, 96 Raja SC Mullick Rd, Kolkata 700032, India
[2] Anna Univ, Coll Engn Guindy, Chennai 600025, Tamil Nadu, India
关键词
Polyvinylidene-fluoride (PVDF); Electrospinning; Piezoelectric Force Sensor; POLY(VINYLIDENE; PHASES;
D O I
10.1016/j.matpr.2019.06.613
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present study, PVDF nanofibers containing primarily beta-phase have been synthesized by electrospinning process. For electrospinning, a number of PVDF laden precursors were prepared varying the composition of solvents (60%-80% DMF) as well as wt% of PVDF (10wt%, 12wt%, and 15 wt% PVDF). The operating parameters for electrospinning were also varied for achieving optimal size and morphology of the PVDF nanofibers. The synthesized fibers were characterized by Fourier-transform infrared spectroscopy (FTIR), field emission scanning electron microscopy (FE-SEM), X-Ray Diffraction (XRD) and differential scanning calorimetry (DSC). PVDF with the solvent ratio of 7:3 offers beads free, thin nanofibers in comparison with other compositions. The presence of crystalline beta-phase was successfully confirmed by the XRD analysis. An exothermic peak was also observed by the DSC analysis at the temperature of 70 degrees C. PVDF nanofiber based piezoelectric force sensors were constructed and their performances were tested by applying calibrated load using a universal mechanical testing (UTM) machine and observing the resulting signal in an oscilloscope. A clear correlation was observed between the peak voltage detected by the PVDF force sensor and the applied load. The study revealed the piezoelectric property for force sensing tends to maximize (maximum current -14 mu A, initial sensitivity-160 mV/kPa) around 12 wt% of PVDF due to presence of beta-gamma phase in sample. (C) 2019 Published by Elsevier Ltd.
引用
收藏
页码:1450 / 1458
页数:9
相关论文
共 14 条
  • [1] Electroactive polymer actuators and sensors
    Bar-Cohen, Yoseph
    Zhang, Qiming
    [J]. MRS BULLETIN, 2008, 33 (03) : 173 - 181
  • [2] Enhanced peripheral nerve regeneration through a poled bioresorbable poly(lactic-co-glycolic acid) guidance channel
    Bryan, David J.
    Tang, Jin Bo
    Doherty, Stephen A.
    Hile, David D.
    Trantolo, Debra J.
    Wise, Donald L.
    Summerhayes, Ian C.
    [J]. JOURNAL OF NEURAL ENGINEERING, 2004, 1 (02) : 91 - 98
  • [3] Influence of the Solvent Evaporation Rate on the Crystalline Phases of Solution-Cast Poly(Vinylidene Fluoride) Films
    Chinaglia, Dante Luis
    Gregorio, Rinaldo, Jr.
    Stefanelo, Josiani Cristina
    Pisani Altafim, Ruy Alberto
    Wirges, Werner
    Wang, Feipeng
    Gerhard, Reimund
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2010, 116 (02) : 785 - 791
  • [4] DOSHI J, 1995, J ELECTROSTAT, V35, P151, DOI 10.1016/0304-3886(95)00041-8
  • [5] Formhals A., 1934, U.S. Patents, Patent No. [1975504, US1975504A]
  • [6] GREGORIO R, 1994, J POLYM SCI POL PHYS, V32, P859, DOI 10.1002/polb.1994.090320509
  • [7] Effect of crystallization rate on the formation of the polymorphs of solution cast poly(vinylidene fluoride)
    Gregorio, Rinaldo, Jr.
    Borges, Daniel Sousa
    [J]. POLYMER, 2008, 49 (18) : 4009 - 4016
  • [8] Synthesis of biodegradable and electroactive multiblock polylactide and aniline pentamer copolymer for tissue engineering applications
    Huang, Lihong
    Zhuang, Xiuli
    Hu, Jun
    Lang, Le
    Zhang, Peibiao
    Wang, Yu
    Chen, Xuesi
    Wei, Yen
    Jing, Xiabin
    [J]. BIOMACROMOLECULES, 2008, 9 (03) : 850 - 858
  • [9] Li Mengyuan, 2013, NAT MATER, V12, P833
  • [10] Electroactive phases of poly(vinylidene fluoride): Determination, processing and applications
    Martins, P.
    Lopes, A. C.
    Lanceros-Mendez, S.
    [J]. PROGRESS IN POLYMER SCIENCE, 2014, 39 (04) : 683 - 706