Decomposition Kinetics of Ferrite in Isothermally Aged SAF 2507-Type Duplex Stainless Steel

被引:24
作者
Berecz, Tibor [1 ]
Fazakas, Eva [2 ]
Meszaros, Istvan [1 ]
Sajo, Istvan [3 ]
机构
[1] Budapest Univ Technol & Econ, Dept Mat Sci & Engn, H-1111 Budapest, Hungary
[2] Bay Zoltan Nonprofit Ltd Appl Res, Inst Mat Sci & Technol, H-1116 Budapest, Hungary
[3] Univ Pecs, Janos Szentagothai Res Ctr, H-7624 Pecs, Hungary
关键词
differential thermal analysis; duplex stainless steel; electron backscatter diffraction; energy-dispersive x-ray spectroscopy; magnetic investigation method; sigma phase; x-ray diffraction; SIGMA-PHASE FORMATION; TREATMENT TEMPERATURE; PRECIPITATION; TRANSFORMATION; DIFFUSION; CD3MN;
D O I
10.1007/s11665-015-1793-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Decomposition of the ferritic phase is studied in isothermally aged SAF 2507 superduplex stainless steel (SDSS) by means of different examination methods. The ferritic phase (delta) undergoes an eutectoid transformation into secondary austenite (gamma (2)) and sigma-phase between 650 and 1000 A degrees C. Samples were treated at 900 A degrees C because the incubation time of this transformation is the shortest at this temperature. In order to follow the microstructural changes, x-ray diffraction analysis (XRD), automated electron backscatter diffraction (EBSD), applied magnetic investigation [vibrating sample magnetometer (VSM)], micro-hardness tests, and differential thermal analysis (DTA) were used. The results of XRD and EBSD methods for phase quantification showed nearly the same amounts for all three phases. The results of applied magnetic investigation for the fraction of ferritic phase were also in good agreement with the corresponding results of XRD and EBSD methods. Decomposition of ferrite is similarly well-traceable on EBSD phase maps where the coherent ferritic areas gradually broke into pieces with increasing time of heat treatment. According to the EBSD measurements the sigma-phase grains appeared and started to grow after 2 min aging time in the ferritic-austenitic matrix, usually on the boundaries of ferritic and austenitic grains. After 15 min treating time, the microstructure consisted of mainly sigma- and austenitic (primary and secondary) phases with negligible amount of ferrite. Chemical composition of the sigma-phase was measured by energy-dispersive x-ray spectroscopy (EDS) at different aging times. Activation energies of sigma-phase precipitation and alpha'-phase formation were determined by the Kissinger plot, through DTA measurements; they are 243 and 261 kJ/mol, respectively. Using the results of phase quantifications, the Johnson-Mehl-Avrami equation was fitted.
引用
收藏
页码:4777 / 4788
页数:12
相关论文
共 37 条
[1]   Effect of ageing on phase evolution and mechanical properties of a high tungsten super-duplex stainless steel [J].
Akisanya, Alfred R. ;
Obi, Udoka ;
Renton, Neill C. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 535 :281-289
[2]   CALCULATION OF AVRAMI PARAMETERS FOR HETEROGENEOUS SOLID-STATE REACTIONS USING A MODIFICATION OF KISSINGER METHOD [J].
AUGIS, JA ;
BENNETT, JE .
JOURNAL OF THERMAL ANALYSIS, 1978, 13 (02) :283-292
[3]   Granulation, Phase Change, and Microstructure - Kinetics of Phase Change. III [J].
Avrami, M .
JOURNAL OF CHEMICAL PHYSICS, 1941, 9 (02) :177-184
[4]   Kinetics of phase change I - General theory [J].
Avrami, M .
JOURNAL OF CHEMICAL PHYSICS, 1939, 7 (12) :1103-1112
[5]  
Avrami M., 1940, J CHEM PHYS, V8, P212, DOI [10.1063/1.1750631, DOI 10.1063/1.1750631]
[6]   Effect of solution treatment temperature on the precipitation kinetic of σ-phase in 2205 duplex stainless steel welds [J].
Badji, R. ;
Bouabdallah, M. ;
Bacroix, B. ;
Kahloun, C. ;
Bettahar, K. ;
Kherrouba, N. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 496 (1-2) :447-454
[7]   Phase transformation and mechanical behavior in annealed 2205 duplex stainless steel welds [J].
Badji, Riad ;
Bouabdallah, Mabrouk ;
Bacroix, Brigitte ;
Kahloun, Charlie ;
Belkessa, Brahim ;
Maza, Halim .
MATERIALS CHARACTERIZATION, 2008, 59 (04) :447-453
[8]   On the activation energy of the σ-phase formation in a pure and Ti-doped Fe-Cr alloy [J].
Blachowski, A ;
Dubiel, SM ;
Zukrowski, J .
INTERMETALLICS, 2001, 9 (06) :493-498
[9]   SOLUTE DIFFUSION IN ALPHA-IRON AND GAMMA-IRON [J].
BOWEN, AW ;
LEAK, GM .
METALLURGICAL TRANSACTIONS, 1970, 1 (06) :1695-&
[10]  
BOWEN AW, 1970, METALL TRANS, V1, P2767