共 22 条
- [1] BEARDMORE P, 1996, T TMS AIME, V236, P102
- [2] FLEMINGS MC, 1974, SOLIDIFICATION PROCE, P303
- [3] FREDRIKSSON H, 1991, SCAND J METALL, V20, P43
- [4] GHOSH S, 1964, AFS T, V40, P721
- [5] GSEHNEIDNER KA, 1964, SOLID STATE PHYS, V16, P275
- [6] JACKSON KA, 1958, LIQUID METALS SOLIDI, P17
- [7] LOWATA T, 1994, IMONO, V66, P803
- [8] Effect of solidification cooling rate on the morphology and number per unit volume of primary Mg2Si particles in a hypereutectic Al-Mg-Si alloy [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (05): : 1368 - 1372
- [9] Chip and built-up edge formation in the machining of in situ Al4C3-Al composite [J]. MATERIALS & DESIGN, 2003, 24 (03): : 215 - 221