Micro-XRD and temperature-modulated DSC investigation of nickel-titanium rotary endodontic instruments

被引:29
作者
Alapati, Satish B. [2 ]
Brantley, William A. [1 ]
Iijima, Masahiro [3 ]
Schricker, Scott R. [1 ]
Nusstein, John M. [4 ]
Li, Uei-Ming [5 ,6 ]
Svec, Timothy A. [7 ]
机构
[1] Ohio State Univ, Coll Dent, Div Restorat & Prosthet Dent, Columbus, OH 43218 USA
[2] Med Univ S Carolina, Coll Dent Med, Dept Mat Sci, Charleston, SC 29425 USA
[3] Hlth Sci Univ Hokkaido, Sch Dent, Dept Oral Growth & Dev, Div Orthodont & Dentofacial Orthoped, Ishikari, Hokkaido 06102, Japan
[4] Ohio State Univ, Coll Dent, Div Endodont, Columbus, OH 43218 USA
[5] Natl Taiwan Univ, Coll Med, Taipei 10764, Taiwan
[6] Cardinal Tien Hosp, Taipei, Taiwan
[7] Oregon Hlth & Sci Univ, Sch Dent, Dept Endodont, Portland, OR 97201 USA
关键词
Nickel-titanium; Endodontics; Rotary instrument; X-ray diffraction; Differential scanning calorimetry; Heat treatment; Phase transformation; Wrought alloys; Metallurgy; Superelasticity; X-RAY-DIFFRACTION; PHASE-TRANSFORMATIONS; ORTHODONTIC WIRES; RESISTANCE; FATIGUE; BEHAVIOR; FRACTURE; FILES; WEAR;
D O I
10.1016/j.dental.2009.04.010
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. Employ Micro-X-ray diffraction and temperature-modulated differential scanning calorimetry to investigate microstructural phases, phase transformations, and effects of heat treatment for rotary nickel-titanium instruments. Methods. Representative as-received and clinically used ProFile GT and ProTaper instruments were principally studied. Micro-XRD analyses (Cu K alpha X-rays) were performed at 25 degrees C on areas of approximately 50 mu m diameter near the tip and up to 9 mm from the tip. TMDSC analyses were performed from -80 to 100 degrees C and back to -80 degrees C on segments cut from instruments, using a linear heating and cooling rate of 2 degrees C/min, sinusoidal oscillation of 0.318 degrees C, and period of 60 s. Instruments were also heat treated 15 min in a nitrogen atmosphere at 400, 500, 600 and 850 degrees C, and analyzed. Results. At all Micro-XRD analysis regions the strongest peak occur-red near 42 degrees, indicating that instruments were mostly austenite, with perhaps some R-phase and martensite. Tip and adjacent regions had smallest peak intensities, indicative of greater work hardening, and the intensity at other sites depended on the instrument. TMDSC heating and cooling curves had single peaks for transformations between martensite and austenite. Austenite-finish (A(f)) temperatures and enthalpy changes were similar for as-received and used instruments. Heat treatments at 400, 500 and 600 degrees C raised the A(f) temperature to 45-50 degrees C, and heat treatment at 850 degrees C caused drastic changes in transformation behavior. Significance. Micro-XRD provides novel information about NiTi phases at different positions on instruments. TMDSC indicates that heat treatment might yield instruments with substantial martensite and improved clinical performance. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1221 / 1229
页数:9
相关论文
共 35 条
[1]   Vickers hardness investigation of work-hardening in used NiTi rotary instruments [J].
Alapati, Satish B. ;
Brantley, William A. ;
Nusstein, John M. ;
Daehn, Glenn S. ;
Svec, Timothy A. ;
Powers, John M. ;
Johnston, William M. ;
Guo, Wenhua .
JOURNAL OF ENDODONTICS, 2006, 32 (12) :1191-1193
[2]   SEM observations of nickel-titanium rotary endodontic instruments that fractured during clinical use [J].
Alapati, SB ;
Brantley, WA ;
Svec, TA ;
Powers, JM ;
Nusstein, JM ;
Daehn, GS .
JOURNAL OF ENDODONTICS, 2005, 31 (01) :40-43
[3]   Scanning electron microscope observations of new and used nickel-titanium rotary files [J].
Alapati, SB ;
Brantley, WA ;
Svec, TA ;
Powers, JM ;
Mitchell, JC .
JOURNAL OF ENDODONTICS, 2003, 29 (10) :667-669
[4]   Fracture resistance of electropolished rotary nickel-titanium endodontic instruments [J].
Anderson, Margot E. ;
Price, John W. H. ;
Parashos, Peter .
JOURNAL OF ENDODONTICS, 2007, 33 (10) :1212-1216
[5]   K3 endo, ProTaper, and ProFile systems: Breakage and distortion, in severely curved roots of molars [J].
Ankrum, MT ;
Hartwell, GR ;
Truitt, JE .
JOURNAL OF ENDODONTICS, 2004, 30 (04) :234-237
[6]   Temperature-modulated DSC provides new insight about transformations nickel-titanium wire [J].
Brantley, WA ;
Iijima, M ;
Grentzer, TH .
AMERICAN JOURNAL OF ORTHODONTICS AND DENTOFACIAL ORTHOPEDICS, 2003, 124 (04) :387-394
[7]   Temperature-modulated DSC study of phase transformations in nickel-titanium orthodontic wires [J].
Brantley, WA ;
Iijima, M ;
Grentzer, TH .
THERMOCHIMICA ACTA, 2002, 392 :329-337
[8]   Differential scanning calorimetric studies of nickel titanium rotary endodontic instruments [J].
Brantley, WA ;
Svec, TA ;
Iijima, M ;
Powers, JM ;
Grentzer, TH .
JOURNAL OF ENDODONTICS, 2002, 28 (08) :567-572
[9]   Differential scanning calorimetric studies of nickel-titanium rotary endodontic instruments after simulated clinical use [J].
Brantley, WA ;
Svec, TA ;
Iijima, M ;
Powers, JM ;
Grentzer, TH .
JOURNAL OF ENDODONTICS, 2002, 28 (11) :774-778
[10]  
BRANTLEY WA, 2001, ORTHODONTIC MAT SCI, P52