Effect of Si content on the microstructure and properties of Al-Si alloys fabricated using hot extrusion

被引:41
作者
Ma, Pan [1 ]
Jia, Yandong [2 ]
Prashanth, Konda Gokuidoss [3 ,4 ]
Yu, Zhishui [1 ]
Li, Chonggui [1 ]
Zhao, Jian [1 ]
Yang, Shanglei [1 ]
Huang, Lixin [1 ]
机构
[1] Shanghai Univ Engn Sci, Sch Mat Engn, Shanghai 201620, Peoples R China
[2] Shanghai Univ, Inst Mat, Lab Microstruct, Shanghai 200444, Peoples R China
[3] Austrian Acad Sci, Erich Schmid Inst Mat Sci, A-8700 Leoben, Austria
[4] Norwegian Univ Sci & Technol, Gjovik, Norway
基金
上海市自然科学基金; 中国国家自然科学基金; 中国博士后科学基金;
关键词
Al-Si alloy; microstructure; mechanical properties; coefficient of thermal expansion; THERMAL-EXPANSION BEHAVIOR; TENSILE PROPERTIES; MECHANICAL-PROPERTIES; MATRIX COMPOSITES; MANAGEMENT APPLICATIONS; POWDER-METALLURGY; HEAT-TREATMENT; EUTECTIC SI; SILICON; PARTICLES;
D O I
10.1557/jmr.2017.97
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al-(12, 20, 35 wt%)Si alloys were fabricated using powder metallurgy process involving hot pressing followed by hot extrusion. The effect of Si content on the microstructure [by scanning electron microscopy], the mechanical properties (hardness and tensile tests), and the thermal expansion behavior were studied in detail, respectively. Due to the friction between the Si phase and the matrix, as well as the diffusion of the Si atoms, the Si phase becomes a particulate shape after hot extrusion, and the size increases with increasing Si content. The mechanical strength increases, whereas, the elongation decreases with increasing the Si content from 12 to 35 wt%, which lead to a variation of the fracture mechanism from ductile to brittle failure. The coefficient of thermal expansion (CTE) decreases with increasing Si content as a result of restriction of Si on the Al matrix, and the measured CTE value is in good agreement with the Turner model below 573 K.
引用
收藏
页码:2210 / 2217
页数:8
相关论文
共 40 条
  • [31] Friction welding of Al-12Si parts produced by selective laser melting
    Prashanth, K. G.
    Damodaram, R.
    Scudino, S.
    Wang, Z.
    Rao, K. Prasad
    Eckert, J.
    [J]. MATERIALS & DESIGN, 2014, 57 : 632 - 637
  • [32] Microstructure and mechanical properties of Al-12Si produced by selective laser melting: Effect of heat treatment
    Prashanth, K. G.
    Scudino, S.
    Klauss, H. J.
    Surreddi, K. B.
    Loeber, L.
    Wang, Z.
    Chaubey, A. K.
    Kuehn, U.
    Eckert, J.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 590 : 153 - 160
  • [33] Characterization of 316L Steel Cellular Dodecahedron Structures Produced by Selective Laser Melting
    Prashanth, Konda Gokuldoss
    Loeber, Lukas
    Klauss, Hans-Joerg
    Kuehn, Uta
    Eckert, Juergen
    [J]. TECHNOLOGIES, 2016, 4 (04):
  • [34] Microstructural refinement of a cast hypereutectic Al-30Si alloy by friction stir processing
    Rao, A. G.
    Rao, B. R. K.
    Deshmukh, V. P.
    Shah, A. K.
    Kashyap, B. P.
    [J]. MATERIALS LETTERS, 2009, 63 (30) : 2628 - 2630
  • [35] Simultaneous enhancements of strength and toughness in an Al-12Si alloy synthesized using selective laser melting
    Suryawanshi, Jyoti
    Prashanth, K. G.
    Scudino, S.
    Eckert, J.
    Prakash, Om
    Ramamurty, U.
    [J]. ACTA MATERIALIA, 2016, 115 : 285 - 294
  • [36] A study of thermal expansion of Al-Mg alloy composites containing fly ash
    Uju, W. A.
    Oguocha, I. N. A.
    [J]. MATERIALS & DESIGN, 2012, 33 : 503 - 509
  • [37] Tensile properties of Al-12Si matrix composites reinforced with Ti-Al-based particles
    Wang, Z.
    Prashanth, K. G.
    Chaubey, A. K.
    Loeber, L.
    Schimansky, F. P.
    Pyczak, F.
    Zhang, W. W.
    Scudino, S.
    Eckert, J.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 630 : 256 - 259
  • [38] The thermal expansion behaviour of SiCp/Al-20Si composites solidified under high pressures
    Wei, Zunjie
    Ma, Pan
    Wang, Hongwei
    Zou, Chunming
    Scudino, Sergio
    Song, Kaikai
    Prashanth, Konda G.
    Jiang, Wei
    Eckert, Juergen
    [J]. MATERIALS & DESIGN, 2015, 65 : 387 - 394
  • [39] Morphologies of primary silicon in hypereutectic Al-Si alloys with melt overheating temperature and cooling rate
    Xu, C. L.
    Jiang, Q. C.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 437 (02): : 451 - 455
  • [40] Silicon dissolution and interfacial characteristics in Si/Al composites fabricated by gas pressure infiltration
    Yu, W.
    Yu, J. K.
    [J]. MATERIALS CHEMISTRY AND PHYSICS, 2013, 139 (2-3) : 783 - 788