Laser-induced oxidation-assisted micromilling of deep narrow microgroove on Inconel 718

被引:8
作者
Xin, Lianjia [1 ]
Zhang, Bin [2 ]
Zhao, Guolong [1 ]
Liu, Hanliang [2 ]
Yang, Yinfei [1 ]
Li, Liang [1 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mech & Elect Engn, Nanjing 210016, Peoples R China
[2] Beijing Spacecrafts, Beijing 100094, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Laser-induced oxidation; Inconel; 718; Deep narrow microgroove; Micromilling; TOOL WEAR; MICRO; CRACKING; ALLOY;
D O I
10.1007/s00170-021-06854-5
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
The miniaturized components of Inconel 718 superalloy are widely used in aerospace industries due to its excellent properties at elevated temperatures. In this work, an innovative hybrid processing technology named laser-induced oxidation assisted micromilling (LOMM) was proposed. A deep narrow microgroove with a depth of 1500 mu m and a width of 500 mu m was fabricated successfully by LOMM. The effects of average laser power on morphology and microstructure of the oxide layer and sub-layer were studied. In addition, milling force, surface quality of the machined microgrooves, and tool wear were investigated. Under laser irradiation with average laser power of 4.5 W, a loose and soft oxide layer, as well as a sub-layer were formed, whose thicknesses were 24 mu m and 16 mu m, respectively. The milling force during removing of the oxide layer was only around 1.2 N, which was much lower than that (3 similar to 8 N) when removing of the substrate material. Owing to the low cutting force, no obvious tool wear was observed in removing of the oxide layer. However, tool wear in terms of coating peeling and microchipping was found in micromilling of the sub-layer and substrate material. For comparison, conventional micromilling (COMM) was used to machine a deep narrow microgroove under identical milling parameters. The tool diameter was reduced by 4.4% in LOMM, while that was reduced by 22% in COMM. The tool failure forms in COMM were catastrophic nose breakage and severe coating peeling. The bottom surface roughness Sa of the deep narrow microgroove machined with LOMM was 0.21 mu m, while that machined with COMM reached 0.41 mu m. This study validated that the proposed novel hybrid process can prolong tool life, and improve surface quality and material removal rate.
引用
收藏
页码:173 / 184
页数:12
相关论文
共 31 条
[1]   Studies on wear behavior of AlTiN-coated WC tool and machined surface quality in micro endmilling of Inconel 718 [J].
Anand Krishnan, N. ;
Mathew, Jose .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2020, 110 (1-2) :291-307
[2]   Cutting performance of nano-crystalline diamond (NCD) coating in micro-milling of Ti6Al4V alloy [J].
Aslantas, K. ;
Hopa, H. E. ;
Percin, M. ;
Ucun, I. ;
Cicek, A. .
PRECISION ENGINEERING-JOURNAL OF THE INTERNATIONAL SOCIETIES FOR PRECISION ENGINEERING AND NANOTECHNOLOGY, 2016, 45 :55-66
[3]   Femtosecond laser micromachining of crystalline silicon for ablation of deep macro-sized cavities for Silicon-on-Insulator applications [J].
Bhaskar, Arun ;
Philippe, Justine ;
Braud, Flavie ;
Okada, Etienne ;
Robillard, Jean-Francois ;
Gloria, Daniel ;
Gaquiere, Christophe ;
Dubois, Emmanuel .
LASER-BASED MICRO- AND NANOPROCESSING XIII, 2019, 10906
[4]   Wear behavior of solid SiAlON milling tools during high speed milling of Inconel 718 [J].
Celik, Ali ;
Alagac, Melike Sert ;
Turan, Servet ;
Kara, Alpagut ;
Kara, Ferhat .
WEAR, 2017, 378-379 :58-67
[5]   Investigation of micro-cutting operations [J].
Chae, J ;
Park, SS ;
Freiheit, T .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2006, 46 (3-4) :313-332
[6]   A high-density, super-high-aspect-ratio microprobe array realized by high-frequency vibration assisted inverse micro w-EDM [J].
Chen, Shun-Tong ;
Yang, Shih-Wei .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2017, 250 :144-155
[7]   Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 718 [J].
Chen, Yuan ;
Zhang, Ke ;
Huang, Jian ;
Hosseini, Seyed Reza Elmi ;
Li, Zhuguo .
MATERIALS & DESIGN, 2016, 90 :586-594
[8]   Micromilling strategies: optimization issues [J].
Dimov, S ;
Pham, DT ;
Ivanov, A ;
Popov, K ;
Fansen, K .
PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2004, 218 (07) :731-736
[9]   Micromilling development and applications for microfabrication [J].
Friedrich, CR ;
Coane, PJ ;
Vasile, MJ .
MICROELECTRONIC ENGINEERING, 1997, 35 (1-4) :367-372
[10]   Alloy design and development of INCONEL718 type alloy [J].
Fu, S. H. ;
Dong, J. X. ;
Zhang, M. C. ;
Xie, X. S. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 499 (1-2) :215-220