Improving the Thermal and Mechanical Properties of Poly(l-lactide) by Forming Nanocomposites with an in Situ Ring-Opening Intermediate of Poly(l-lactide) and Polyhedral Oligomeric Silsesquioxane
被引:10
作者:
Lei, Xiu-Xiu
[1
]
Lu, Hao
[1
]
Lu, Lei
[1
]
Xu, Hai-Qing
[2
]
Zhou, Ying-Guo
[1
]
Zou, Jun
[1
]
机构:
[1] Jiangsu Univ Sci & Technol, Sch Mat Sci & Engn, Zhenjiang 212003, Jiangsu, Peoples R China
[2] Huaiyin Inst Technol, Jiangsu Prov Engn Lab Adv Mat Salt Chem Ind, Huaian 223003, Peoples R China
关键词:
poly(l-lactide) (PLLA);
ring-opening polymerization;
compatibility;
nanocomposites;
(3-amino)-propylheptaisobutyl cage silsesquioxane (AMPOSS);
STATIC MIXING REACTION;
POLY(LACTIC ACID);
CRYSTALLIZATION;
POLYMERIZATION;
NANOPARTICLES;
BEHAVIOR;
REINFORCEMENT;
SIMULATION;
COPOLYMERS;
OXIDE;
D O I:
10.3390/nano9050748
中图分类号:
O6 [化学];
学科分类号:
0703 ;
摘要:
In this study, a series of poly(l-lactide) and (3-amino)-propylheptaisobutyl cage silsesquioxane (PLLA-AMPOSS) intermediates were first fabricated using single-arm in situ solution polymerization of LLA monomers and AMPOSS nanoparticles with different contents, 0.02-1.00 mol%. Then, the PLLA-AMPOSS intermediate with 0.5 mol% AMPOSS was selected as a representative and investigated by nuclear magnetic resonance (NMR) and X-ray diffraction (XRD). Afterwards, it was added into the pure PLLA with different mass fractions. Finally, the thermal behavior, crystallization kinetics, morphological characteristics, and mechanical properties of the obtained PLLA/PLLA-AMPOSS nanocomposites were carefully measured and investigated by differential scanning calorimetry (DSC), polarizing microscopy (POM), scanning electron microscopy (SEM), and tensile test. After comparing the PLLA-AMPOSS intermediate and PLLA/AMPOSS blend, the results show that the ring-open polymerization of PLLA-AMPOSS intermediate was successful. The results also show that the existence of PLLA-AMPOSS has a strong influence on the crystallization behavior of PLLA/PLLA-AMPOSS composites, which can be attributed to the heterogeneous nucleation effect of PLLA-AMPOSS. In addition, it was also found from the tensile test results that the addition of the PLLA-AMPOSS nanofiller improved the tensile strength and strain at break of PLLA/PLLA-AMPOSS nanocomposites. All of these results indicate the good nucleating effect of PLLA-AMPOSS and that the AMPOSS disperses well in the PLLA/PLLA-AMPOSS nanocomposites. A conclusion can be drawn that the selective nucleating agent and the combined method of in situ ring-opening polymerization and physical blending are feasible and effective.