Development of A1-5Cu/B4C composites with low coefficient of thermal expansion for automotive application

被引:50
作者
Pozdniakov, A. V. [1 ]
Lotfy, A. [1 ]
Qadir, A. [1 ]
Shalaby, E. [1 ]
Khomutov, M. G. [1 ]
Churyumov, A. Yu. [1 ]
Zolotorevskiy, V. S. [1 ]
机构
[1] NUST, MISiS, Leninskiy Ave 4, Moscow 119049, Russia
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2017年 / 688卷
关键词
Aluminum matrix composites; Squeeze casting; Electron microscopy; Coefficient of thermal expansion; X-ray diffraction; Mechanical properties; Castability; METAL-MATRIX COMPOSITES; SI PISTON ALLOY; MECHANICAL-PROPERTIES; CASTING TECHNIQUES; VOLUME FRACTION; PARTICLE-SIZE; MICROSTRUCTURE; BEHAVIOR; FRACTURE;
D O I
10.1016/j.msea.2017.01.075
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The purpose of this research is to provide a competitive alternative to aluminum silicon alloys used in automotive applications. This alternate was created by developing composites of A1-5%Cu alloy reinforced with B4C particulates with a low coefficient of thermal expansion. Stir casting was used to produce Al-5%Cu alloys containing 2%, 5%, and 7 %wt. B4C particulates were subsequently added using the squeeze casting process. The squeeze casting technique decreased the porosity of the final composites. The composites exhibited a fairly uniform particle distribution throughout the alloy matrix. The microstructure and the XRD results of the composites indicated that a significant reaction had occurred at the interface between the particles and the matrix. Increasing the aging temperature from 200 to 250 degrees C decreased the hardness values of the matrix and the composites and decreased the time required to reach the peak. The coefficient of thermal expansion (GTE) for both the stir and squeezed cast samples decreased as the percentage of reinforcements increased and increased as the temperature range increased. Increasing the concentration of B4C increased YS and decreased the plasticity during compression test at both room and elevated temperatures. The Al-5%Cu-7%B4C composite has a significant higher tensile properties than A336 (AlSil2CuMgNi) at 260 degrees C. Special mould made of 20Cr13 steel was constructed to evaluate castability. The Al-5%Cu-7%B4C composite completely repeats shape of the mould during squeeze casting process without hot cracking.
引用
收藏
页码:1 / 8
页数:8
相关论文
共 28 条
[1]   Dry sliding wear behaviour of hypereutectic Al-Si piston alloys containing iron-rich intermetallics [J].
Abouei, V. ;
Shabestari, S. G. ;
Saghafian, H. .
MATERIALS CHARACTERIZATION, 2010, 61 (11) :1089-1096
[2]  
[Anonymous], 1989, REG REC AL ASS ALL D
[3]  
[Anonymous], 2010, ASM HDB PROP SEL NON, V2
[4]  
[Anonymous], 2010, ASM HDB CAST V 2, V2
[5]  
Bonnet G., 2009, Packaging, Transport, Storage & Security of Radioactive Material, V20, P98, DOI 10.1179/174651009X416880
[6]   Effect of volume fraction and size of B4C particles on production and microstructure properties of B4C reinforced aluminium alloy composites [J].
Canakci, A. ;
Arslan, F. ;
Varol, T. .
MATERIALS SCIENCE AND TECHNOLOGY, 2013, 29 (08) :954-960
[7]   Thermal expansion anisotropy in extruded SiC particle reinforced 2080 aluminum alloy matrix composites [J].
Chawla, N. ;
Deng, X. ;
Schnell, D. R. M. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 426 (1-2) :314-322
[8]   The design, microstructure and tensile properties of B4C particulate reinforced 6061Al neutron absorber composites [J].
Chen, H. S. ;
Wang, W. X. ;
Li, Y. L. ;
Zhang, P. ;
Nie, H. H. ;
Wu, Q. C. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 632 :23-29
[9]  
Chen N, 2008, J MATER PROCESS TECH, V209, P1471
[10]   The effect of internal stress on the thermal expansion coefficient of Al/SiCp composite [J].
Chen, Na ;
Zhang, Hongxiang ;
Mu, Guohong ;
Gu, Mingyuan .
JOURNAL OF COMPOSITE MATERIALS, 2007, 41 (22) :2691-2699