Effect of Postoxidation Annealing on High Temperature Grown SiO2/4H-SiC Interfaces

被引:13
|
作者
Moon, Jeong Hyun [1 ,2 ]
Yim, Jeong Hyuk [1 ,2 ]
Seo, Han Seok [1 ,2 ]
Lee, Do Hyun [1 ,2 ]
Song, Ho Keun [1 ,2 ]
Heo, Jaeyeong [1 ,2 ]
Kim, Hyeong Joon [1 ,2 ]
Cheong, Kuan Yew [3 ]
Bahng, Wook [4 ]
Kim, Nam-Kyun [4 ]
机构
[1] Seoul Natl Univ, Coll Engn, Dept Mat Sci & Engn, Seoul 151744, South Korea
[2] Seoul Natl Univ, Interuniv Semicond Res Ctr, Seoul 151744, South Korea
[3] Univ Sains Malaysia, Sch Mat & Mineral Resources Engn, George Town 14300, Malaysia
[4] Korea Electrotechnol Res Inst, Ctr Energy Efficient Semicond, Gyungnam 641120, South Korea
关键词
annealing; capacitance; ellipsometry; MIS devices; oxidation; silicon compounds; X-ray photoelectron spectra; CRYSTAL SILICON-CARBIDE; SIC POWER DEVICES; SIC/SIO2; INTERFACE; 4H-SIC MOS; THERMAL-OXIDATION; GATE OXIDES; SIO2; NITRIDATION; QUALITY; TRAPS;
D O I
10.1149/1.3267508
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
SiO2 was grown by dry (O-2) thermal oxidation (at 1175, 1300, or 1400 degrees C) on n-type 4H-SiC substrates. The samples were prepared by subsequently exposing the grown SiO2 film on 4H-SiC to postoxidation annealing (POA) treatment using nitric oxide (NO) gas. The SiC-SiO2 interfaces were characterized by high frequency capacitance-voltage measurements, X-ray photoelectron spectroscopy (XPS), and ellipsometry. The interface trap density of the dry oxide grown at 1300 degrees C was much lower than others. At a higher grown temperature (1400 degrees C), the electrical and physical properties of the oxide were not improved compared to those oxides grown at 1175 degrees C. The XPS measurements provided evidence for the presence of intermediate oxidation states of Si oxycarbide in all samples. The areal densities of the intermediate oxidation states affected the interface trap density. The NO POA treatment significantly improved the interface trap density, the near-interface trap density, and the effective oxide charge density of the oxides grown at 1175 and 1300 degrees C. But, this improvement was not observed for the oxide grown at 1400 degrees C. The electrical properties of the metal-oxide-semiconductor devices fabricated using these oxides have also been discussed in terms of the oxide chemical compositions, which were determined by XPS and an oxide etching test.
引用
收藏
页码:H196 / H201
页数:6
相关论文
共 50 条
  • [31] Effect of Ar annealing temperature on SiO2/4H-SiC interface studied by spectroscopic ellipsometry and atomic force microscopy
    Zhong, Zhiqin
    Zhang, Guojun
    Wang, Shuya
    Dai, Liping
    MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING, 2013, 16 (06) : 2028 - 2031
  • [32] Kinetics of NO nitridation in SiO2/4H-SiC
    Feldman, L.C. (leonard.c.feldman@vanderbilt.edu), 1600, American Institute of Physics Inc. (93):
  • [33] Kinetics of NO nitridation in SiO2/4H-SiC
    McDonald, K
    Feldman, LC
    Weller, RA
    Chung, GY
    Tin, CC
    Williams, JR
    JOURNAL OF APPLIED PHYSICS, 2003, 93 (04) : 2257 - 2261
  • [34] Dielectric Properties of Thermally Grown SiO2 on 4H-SiC(0001) Substrates
    Hosoi, Takuji
    Uenishi, Yusuke
    Mitani, Shuhei
    Nakano, Yuki
    Nakamura, Takashi
    Shimura, Takayoshi
    Watanabe, Heiji
    SILICON CARBIDE AND RELATED MATERIALS 2012, 2013, 740-742 : 605 - +
  • [35] Interfacial Transition Layer in Thermally Grown SiO2 Film on 4H-SiC
    Hasunuma, Ryu
    2017 IEEE INTERNATIONAL CONFERENCE ON IC DESIGN AND TECHNOLOGY (ICICDT), 2017,
  • [36] RETRACTED: Effects of high-temperature diluted-H2 annealing on effective mobility of 4H-SiC MOSFETs with thermally-grown SiO2 (Retracted Article)
    Hirai, Hirohisa
    Kita, Koji
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2016, 55 (04)
  • [37] Extraction of the 4H-SiC/SiO2 Barrier Height Over Temperature
    Avino-Salvado, O.
    Asllani, B.
    Buttay, C.
    Raynaud, C.
    Morel, H.
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 2020, 67 (01) : 63 - 68
  • [38] Effect of postoxidation annealing on Si/SiO2 interface roughness
    Chen, XD
    Gibson, JM
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (08) : 3032 - 3038
  • [39] Effects of a post-oxidation annealing in nitrous oxide on the morphological and electrical properties of SiO2/4H-SiC interfaces
    Swanson, L. K.
    Fiorenza, P.
    Giannazzo, F.
    Alessandrino, S.
    Lorenti, S.
    Roccaforte, F.
    SILICON CARBIDE AND RELATED MATERIALS 2012, 2013, 740-742 : 715 - +
  • [40] Effects of a post-oxidation annealing in nitrous oxide on the morphological and electrical properties of SiO2/4H-SiC interfaces
    Swanson, L. K.
    Fiorenza, P.
    Giannazzo, F.
    Roccaforte, F.
    SILICON CARBIDE AND RELATED MATERIALS 2012, 2013, 740-742 : 719 - +